# US 2013/0283858 A1 · Titania-doped quartz glass and making method

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2013/0283858 A1
- Document ID: US20130283858A1
- Status: Published application
- Kind: A1
- Application number: 13/920,628
- Filed: 2013-06-18
- Published: 2013-10-31
- Earliest claimed: 2009-12-25
- Assignees: Shin-Etsu Chemical Co., Ltd.
- Inventors: Shigeru Maida; Hisatoshi Otsuka; Tetsuji Ueda; Masanobu Ezaki
- Web page: https://patentgrep.com/patent/US20130283858A1

## CPC

- G03F 7/2008: {characterised by the reflectors, diffusers, light or heat filtering means or anti-reflective means used}
- B82Y 10/00: Nanotechnology for information processing, storage or transmission, e.g. quantum computing or single electron logic
- B82Y 40/00: Manufacture or treatment of nanostructures
- C03B 19/1423: {Reactant deposition burners}
- C03B 19/1453: {Thermal after-treatment of the shaped article, e.g. dehydrating, consolidating, sintering}
- C03C 3/06: with more than 90% silica by weight, e.g. quartz {(C03C3/045 takes precedence)}
- G03F 1/24: Reflection masks; Preparation thereof
- C03B 2201/21: doped with molecular hydrogen
- C03B 2201/23: doped with hydroxyl groups
- C03B 2201/42: doped with titanium
- C03B 2207/06: Concentric circular ports
- C03B 2207/12: Nozzle or orifice plates
- C03B 2207/36: Fuel or oxidant details, e.g. flow rate, flow rate ratio, fuel additives
- C03C 2201/06: Doped silica-based glasses
- G03F: PHOTOMECHANICAL PRODUCTION OF TEXTURED OR PATTERNED SURFACES, e.g. FOR PRINTING, FOR PROCESSING OF SEMICONDUCTOR DEVICES; MATERIALS THEREFOR; ORIGINALS THEREFOR; APPARATUS SPECIALLY ADAPTED THEREFOR; (phototypographic composing devices B41B; photosensitive materials or processes for photographic purposes G03C; electrophotography, sensitive layers or processes therefor G03G)
- B82Y: SPECIFIC USES OR APPLICATIONS OF NANOSTRUCTURES; MEASUREMENT OR ANALYSIS OF NANOSTRUCTURES; MANUFACTURE OR TREATMENT OF NANOSTRUCTURES
- C03B: MANUFACTURE, SHAPING, OR SUPPLEMENTARY PROCESSES
- C03C: CHEMICAL COMPOSITION OF GLASSES, GLAZES OR VITREOUS ENAMELS; SURFACE TREATMENT OF GLASS; SURFACE TREATMENT OF FIBRES OR FILAMENTS MADE FROM GLASS, MINERALS OR SLAGS; JOINING GLASS TO GLASS OR OTHER MATERIALS

## Abstract

Methods for selecting titania-doped quartz glass which experiences a reduction in OH group concentration of less than or equal to 100 ppm upon heat treatment at 900° C. for 100 hours as suitable material for the EUV lithography member.

## Claims

### Claim 1

A method of selecting a titania-doped quartz glass having a reduction in OH group concentration of less than or equal to 100 ppm, comprising
measuring a sample of a titania-doped quartz glass ingot to be selected for OH group concentration,
heat-treating the sample at 900° C. for 100 hours,
measuring the heat-treated sample for OH group concentration, and
computing a reduction of OH group concentration to evaluate the sample whether the reduction of OH group concentration is less than or equal to 100 ppm or not,
wherein said titania-doped quartz glass ingot being prepared by a method comprising the steps of
subjecting a silicon-providing reactant gas and a titanium-providing reactant gas to oxidation or flame hydrolysis with the aid of a combustible gas and a combustion-supporting gas, to thereby form synthetic silica-titania fine particles,
depositing the silica-titania fine particles on a rotating target, and
concurrently melting and vitrifying the deposited particles into titania-doped quartz glass.

### Claim 2 (depends on 1)

The method of claim 1 wherein the titania-doped quartz glass to be selected further has a difference between maximum and minimum reductions of OH group concentration over the glass upon the 900° C./100-hour heat treatment of less than or equal to 50 ppm.

### Claim 3 (depends on 1)

The method of claim 1 wherein the titania-doped quartz glass to be selected further has an OH group concentration of 300 ppm to 950 ppm after the 900° C./100-hour heat treatment.

### Claim 4 (depends on 1)

The method of claim 1 wherein the titania-doped quartz glass to be selected further has an OH group concentration gradient of less than or equal to 100 ppm/cm after the 900° C./100-hour heat treatment.

### Claim 5 (depends on 1)

The method of claim 1 wherein the method of preparing the titania-doped quartz glass ingot further comprises
a step of feeding oxygen gas as the combustion-supporting gas through a central tube of a burner in admixture with the silicon-providing reactant gas and the titanium-providing reactant gas in a molar ratio of oxygen gas to the sum of the silicon-providing reactant gas and the titanium-providing reactant gas of at least 5, and/or
a step of injecting hydrogen gas as the combustible gas through one or more hydrogen gas feed tubes of the burner at a linear velocity of less than or equal to 100 m/sec.

### Claim 6 (depends on 1)

The method of claim 1 wherein in the method of preparing the titania-doped quartz glass ingot, flow rates of the combustible gas, the combustion-supporting gas, the silicon-providing reactant gas and the titanium-providing reactant gas are controlled so that respective variations of the flow rates may fall within ±1%,
temperatures of cooling air introduced into a quartz glass manufacturing furnace from outside, exhaust gas from the furnace, and ambient air surrounding the furnace are controlled so that respective variations of the temperatures may fall within ±2.5° C., and
the rotating target is rotated at a rotational speed of at least 5 rpm when the silica-titania fine particles are deposited on the rotating target.

### Claim 7

A method of preparing a titania-doped quartz glass, comprising steps of
subjecting a silicon-providing reactant gas and a titanium-providing reactant gas to oxidation or flame hydrolysis with aid of a combustible gas and a combustion-supporting gas, to thereby form synthetic silica-titania fine particles,
depositing the silica-titania fine particles on a rotating target, and
concurrently melting and vitrifying the deposited particles into titania-doped quartz glass,
the method further comprising
a step of feeding oxygen gas as the combustion-supporting gas through a central tube of a burner in admixture with the silicon-providing reactant gas and the titanium-providing reactant gas in a molar ratio of oxygen gas to a sum of the silicon-providing reactant gas and the titanium-providing reactant gas of at least 5, and
a step of injecting hydrogen gas as the combustible gas through one or more hydrogen gas feed tubes of a burner at a linear velocity of less than or equal to 100 m/sec.

### Claim 8

A method for preparing a titania-doped quartz glass, comprising steps of
subjecting a silicon-providing reactant gas and a titanium-providing reactant gas to oxidation or flame hydrolysis with aid of a combustible gas and a combustion-supporting gas, to thereby form synthetic silica-titania fine particles,
depositing the silica-titania fine particles on a rotating target, and
concurrently melting and vitrifying the deposited particles into titania-doped quartz glass,
the method further comprising
a step of injecting hydrogen gas as the combustible gas through one or more hydrogen gas feed tubes of a burner at a linear velocity of less than or equal to 100 m/sec.

### Claim 9 (depends on 7)

The method of claim 7 wherein
flow rates of the combustible gas, the combustion-supporting gas, the silicon-providing reactant gas and the titanium-providing reactant gas are controlled so that respective variations of the flow rates fall within ±1%,
temperatures of cooling air introduced from the outside of a quartz glass manufacturing furnace thereinto, exhaust gas from the furnace, and ambient air surrounding the furnace are controlled so that respective variations of the temperatures fall within ±2.5° C., and
the rotating target is rotated at a rotational speed of at least 5 rpm when the silica-titania fine particles are deposited on the rotating target.

### Claim 10 (depends on 8)

The method of claim 8 wherein
flow rates of the combustible gas, the combustion-supporting gas, the silicon-providing reactant gas and the titanium-providing reactant gas are controlled so that respective variations of the flow rates fall within ±1%,
temperatures of cooling air introduced from the outside of a quartz glass manufacturing furnace thereinto, exhaust gas from the furnace, and ambient air surrounding the furnace are controlled so that respective variations of the temperatures fall within ±2.5° C., and
the rotating target is rotated at a rotational speed of at least 5 rpm when the silica-titania fine particles are deposited on the rotating target.

### Claim 11 (depends on 7)

The method of claim 7, further comprises annealing and shaping the ingot formed by melting and vitrifying the deposited particles.

### Claim 12 (depends on 11)

The method of claim 11, further comprises forming a slice from the ingot and polishing the slice to form a lithographic member or a mirror element.

### Claim 13 (depends on 8)

The method of claim 8, further comprises annealing and shaping the ingot formed by melting and vitrifying the deposited particles.

### Claim 14 (depends on 13)

The method of claim 13 which comprises forming a slice from the ingot and polishing the slice to form a lithographic member or mirror element.