# US 2013/0283706 A1 · Polycrystalline diamond

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2013/0283706 A1
- Document ID: US20130283706A1
- Status: Published application
- Kind: A1
- Application number: 13/921,684
- Filed: 2013-06-19
- Published: 2013-10-31
- Earliest claimed: 2009-06-02
- Inventors: Kaveshini Naidoo; Thembinkosi Shabalala
- Web page: https://patentgrep.com/patent/US20130283706A1

## CPC

- B24D 18/00: Manufacture of grinding tools {or other grinding devices}, e.g. wheels, not otherwise provided for
- B24D 99/005: {Segments of abrasive wheels}
- C22C 26/00: Alloys containing diamond {or cubic or wurtzitic boron nitride, fullerenes or carbon nanotubes}
- E21B 10/36: Percussion drill bits ({with helical conveying portion E21B10/445;} characterised by wear resisting parts E21B10/46)
- E21B 10/46: characterised by wear resisting parts, e.g. diamond inserts
- E21B 10/567: with preformed cutting elements mounted on a distinct support, e.g. polycrystalline inserts
- Y10T 428/249961: With gradual property change within a component
- Y10T 428/268: Monolayer with structurally defined element
- B24D: TOOLS FOR GRINDING, BUFFING OR SHARPENING (abrading-bodies specially designed for tumbling apparatus, e.g. abrading-balls B24B31/14; honing tools B24B33/08; lapping tools B24B37/11)
- C22C: ALLOYS (treatment of alloys C21D, C22F)
- E21B: EARTH OR ROCK DRILLING; OBTAINING OIL, GAS, WATER, SOLUBLE OR MELTABLE MATERIALS OR A SLURRY OF MINERALS FROM WELLS
- Y10T: TECHNICAL SUBJECTS COVERED BY FORMER US CLASSIFICATION

## Abstract

A polycrystalline diamond (PCD) material 10 comprising at least 88 volume percent and at most 99 volume percent diamond grains 12, the mean diamond grain contiguity being greater than 60.5 percent. The PCD material 10 is particularly but not exclusively for use in boring into the earth.

## Claims

### Claim at position 1

1-15. (canceled)

### Claim 16

A method of making PCD material, the method including subjecting an aggregated mass of diamond grains to a pressure treatment at a pressure of greater than 6.0 GPa in the presence of a metallic catalyst material for diamond at a temperature sufficiently high for the catalyst material to melt, and sintering the diamond grains to form PCD material; the diamond grains having the size distribution characteristic that at least 50 percent of the grains have average equivalent circle diameter (ECD) size greater than 5 microns, and at least 20 percent of the grains have average ECD size in the range from 10 to 15 microns.

### Claim 17 (depends on 16)

A method as claimed in claim 16, including subjecting the PCD material to a further pressure treatment at a pressure of at least about 2 GPa.

### Claim 18 (depends on 16)

A method as claimed in claim 16, including removing metallic catalyst material for diamond from interstices between the diamond grains of the PCD material.

### Claim 19 (depends on 16)

A method as claimed in claim 16, including subjecting the PCD material to a heat treatment at a temperature of at least about 500 degrees centigrade for at least about 5 minutes.

### Claim 20 (depends on 16)

A method as claimed in claim 16, including introducing an additive material into the aggregated mass, the additive material containing at least one element selected from V, Ti, Mo, Zr, W, Ta, Hf, Si, Sn or Al.

### Claim at position 7

21-27. (canceled)