# US 2013/0283704 A1 · Method for producing polishing liquid composition

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2013/0283704 A1
- Document ID: US20130283704A1
- Status: Published application
- Kind: A1
- Application number: 13/996,976
- Filed: 2011-12-21
- Published: 2013-10-31
- Earliest claimed: 2010-12-24
- Assignees: Kao Corporation
- Inventors: Yasuhiro Yoneda; Kanji Sato
- Web page: https://patentgrep.com/patent/US20130283704A1

## CPC

- C09G 1/02: containing abrasives or grinding agents {(abrasives as such C09K3/14; polishing of semi-conductors H10P52/40)}
- C09K 3/1463: {Aqueous liquid suspensions}
- G11B 5/8404: {manufacturing base layers}
- C09G: POLISHING COMPOSITIONS (French polish C09F11/00); SKI WAXES
- C09K: MATERIALS FOR MISCELLANEOUS APPLICATIONS, NOT PROVIDED FOR ELSEWHERE
- G11B: INFORMATION STORAGE BASED ON RELATIVE MOVEMENT BETWEEN RECORD CARRIER AND TRANSDUCER (recording measured values in a way that does not require playback through a transducer G01D9/00; recording or playback apparatus using mechanically marked tape, e.g. punched paper tape, or using unit records, e.g. punched or magnetically marked cards G06K; transferring data from one type of record carrier to another G06K1/18; circuits for coupling output of reproducer to radio receiver H04B1/20; gramophone pick-ups or like acoustic electromechanical transducers or circuits therefor H04R)

## Abstract

Provided is a method for producing a polishing composition capable of reducing scratches and particles of an object to be polished, after polishing. It is a method for producing a polishing composition including a step of filtering with a filtration filter a silica particle dispersion containing colloidal silica whose primary particles have an average particle diameter in a range of 1 to 100 nm, wherein the filtration filter includes diatomite cationized by use of a polyvalent amine compound having 9 to 200 cationic groups in the molecule.

## Claims

### Claim 1

A method for producing a polishing composition, the method comprising a step of filtering with a filtration filter a silica particle dispersion containing colloidal silica whose primary particles have an average particle diameter in a range of 1 to 100 nm,
wherein the filtration filter comprises diatomite cationized by use of a polyvalent amine compound having 9 to 200 cationic groups in the molecule.

### Claim 2 (depends on 1)

The method for producing a polishing composition according to claim 1, wherein the polyvalent amine compound is polyalkyleneimine.

### Claim 3 (depends on 1)

The method for producing a polishing composition according to claim 1, wherein the polyvalent amine compound has a number average molecular weight in a range of 400 to 9000.

### Claim 4 (depends on 1)

The method for producing a polishing composition according to claim 1, wherein an average pore diameter of the diatomite obtained by a mercury intrusion method is 0.1 to 3.5 μm.

### Claim 5 (depends on 1)

The method for producing a polishing composition according to claim 1, wherein an integrated pore volume of not larger than 0.15 μm of the diatomite obtained by a nitrogen adsorption method is not less than 0.3 mL/g.

### Claim 6 (depends on 1)

The method for producing a polishing composition according to claim 1, wherein the diatomite has a BET specific surface area of not less than 4.0 m2/g.

### Claim 7 (depends on 1)

The method for producing a polishing composition according to claim 1, comprising a step of producing a filtration filter comprising the cationized diatomite.

### Claim at position 8

8-9. (canceled)

### Claim 10 (depends on 1)

The method for producing a polishing composition according to claim 1, wherein in the cationization treatment, the ratio in the amount of the polyvalent amine compound in use to the diatomite (weight ratio) is 1/500 to 1/1 as (‘weight of polyvalent amine compound’/‘weight of diatomite’).

### Claim 11 (depends on 1)

The method for producing a polishing composition according to claim 1, wherein a content of the cationized diatomite in the filtration filter is not less than 0.001 g/cm2 and not more than 1 g/cm2.

### Claim 12 (depends on 1)

The method for producing a polishing composition according to claim 1, wherein a content of the colloidal silica in the silica particle dispersion is 1 to 50 wt %.

### Claim 13 (depends on 1)

The method for producing a polishing composition according to claim 1, wherein the number of the cationic groups in the polyvalent amine compound is not less than 20 and not more than 100.

### Claim 14 (depends on 1)

The method for producing a polishing composition according to claim 1, wherein the polyalkyleneimine is polyethyleneimine, polypropyleneimine, or polybutadieneimine.

### Claim 15 (depends on 1)

The method for producing a polishing composition according to claim 1, wherein the pH of the silica particle dispersion is 9 to 11.

### Claim 16 (depends on 1)

The method for producing a polishing composition according to claim 1, wherein in the filtration treatment, a depth filter and/or a pleats filter is used further in combination with the filtration filter.