# US 2013/0283603 A1 · Method of manufacturing positive electrode active material for lithium ion battery

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2013/0283603 A1
- Document ID: US20130283603A1
- Status: Published application
- Kind: A1
- Application number: 13/923,428
- Filed: 2013-06-21
- Published: 2013-10-31
- Earliest claimed: 2011-08-29
- Assignees: Semiconductor Energy Laboratory Co., Ltd.
- Applicants: Semiconductor Energy Laboratory Co., Ltd.
- Inventors: Takuya MIWA; Kuniharu Nomoto; Nobuhiro Inoue
- Web page: https://patentgrep.com/patent/US20130283603A1

## CPC

- H01G 9/042: characterised by the material (H01G11/22 takes precedence)
- H01M 4/5825: {Oxygenated metallic salts or polyanionic structures, e.g. borates, phosphates, silicates, olivines}
- H01M 4/625: {Carbon or graphite}
- H01M 10/058: Construction or manufacture
- B82Y 30/00: Nanotechnology for materials or surface science, e.g. nanocomposites
- H01M 4/622: {being polymers}
- Y02E 60/10: Energy storage using batteries
- Y02P 70/50: Manufacturing or production processes characterised by the final manufactured product
- Y10T 29/49115: including coating or impregnating
- H01G: CAPACITORS; CAPACITORS, RECTIFIERS, DETECTORS, SWITCHING DEVICES, LIGHT-SENSITIVE OR TEMPERATURE-SENSITIVE DEVICES OF THE ELECTROLYTIC TYPE (selection of specified materials as dielectric H01B3/00; capacitors having potential barriers H10D1/62, H10K10/10)
- H01M: PROCESSES OR MEANS, e.g. BATTERIES, FOR THE DIRECT CONVERSION OF CHEMICAL ENERGY INTO ELECTRICAL ENERGY
- B82Y: SPECIFIC USES OR APPLICATIONS OF NANOSTRUCTURES; MEASUREMENT OR ANALYSIS OF NANOSTRUCTURES; MANUFACTURE OR TREATMENT OF NANOSTRUCTURES
- Y02E: REDUCTION OF GREENHOUSE GAS [GHG] EMISSIONS, RELATED TO ENERGY GENERATION, TRANSMISSION OR DISTRIBUTION
- Y02P: CLIMATE CHANGE MITIGATION TECHNOLOGIES IN THE PRODUCTION OR PROCESSING OF GOODS
- Y10T: TECHNICAL SUBJECTS COVERED BY FORMER US CLASSIFICATION

## Abstract

At least one of an aqueous solution A containing lithium, an aqueous solution B containing iron, manganese, cobalt, or nickel, and an aqueous solution C containing a phosphoric acid includes graphene oxide. The aqueous solution A is dripped into the aqueous solution C, so that a mixed solution E including a precipitate D is prepared. The mixed solution E is dripped into the aqueous solution B, so that a mixed solution G including a precipitate F is prepared. The mixed solution G is subjected to heat treatment in a pressurized atmosphere, so that a mixed solution H is prepared, and the mixed solution H is then filtered. Thus, particles of a compound containing lithium and oxygen which have a small size are obtained.

## Claims

### Claim 1

(canceled)

### Claim 2

A method of manufacturing a positive electrode, comprising the steps of:
preparing a first mixed solution by mixing a first aqueous solution comprising lithium into a second aqueous solution comprising a phosphoric acid;
preparing a second mixed solution by putting the first mixed solution into a third aqueous solution;
obtaining a particle containing lithium and oxygen from the second mixed solution;
wherein at least one of the first aqueous solution, the second aqueous solution, and the third aqueous solution comprises graphene oxide, and
wherein the third aqueous solution comprises any one of iron, manganese, cobalt, and nickel.

### Claim 3

A method of manufacturing a positive electrode, comprising the steps of:
preparing a first mixed solution by mixing a first aqueous solution comprising lithium into a second aqueous solution comprising a phosphoric acid;
preparing a second mixed solution by putting the first mixed solution into a third aqueous solution;
obtaining an active material comprising a particle from the second mixed solution;
preparing a slurry comprising the active material;
obtaining a positive electrode active material layer from the slurry; and
providing a positive electrode current collector with the positive electrode active material layer,
wherein at least one of the first aqueous solution, the second aqueous solution, and the third aqueous solution comprises graphene oxide, and
wherein the third aqueous solution comprises any one of manganese, cobalt, and nickel.

### Claim 4 (depends on 2)

The method of manufacturing a positive electrode according to claim 2,
wherein the particle is a particle of lithium iron phosphate.

### Claim 5 (depends on 3)

The method of manufacturing a positive electrode according to claim 3, wherein the particle is a particle of lithium iron phosphate.

### Claim 6

A method of manufacturing a positive electrode, comprising the steps of:
preparing a first mixed solution by mixing a first aqueous solution comprising lithium into a second aqueous solution comprising a phosphoric acid;
preparing a second mixed solution by putting the first mixed solution into a third aqueous solution;
obtaining an active material comprising a particle from the second mixed solution;
preparing a slurry comprising the active material;
obtaining a positive electrode active material layer from the slurry, the positive electrode active material layer comprising graphene oxide and particles of lithium iron phosphate; and
providing a positive electrode current collector with the positive electrode active material layer,
wherein at least one of the first aqueous solution, the second aqueous solution, and the third aqueous solution comprises graphene oxide, and
wherein the third aqueous solution comprises iron.

### Claim 7 (depends on 2)

The method of manufacturing a positive electrode according to claim 2, wherein the particle has a size of 30 nm to 250 nm.

### Claim 8 (depends on 3)

The method of manufacturing a positive electrode according to claim 3, wherein the particle has a size of 30 nm to 250 nm.

### Claim 9 (depends on 6)

The method of manufacturing a positive electrode according to claim 6, wherein the particle has a size of 30 nm to 250 nm.

### Claim 10 (depends on 2)

A method of manufacturing a power storage device, comprising:
preparing a slurry comprising the particle according to claim 2;
obtaining a positive electrode active material layer from the slurry; and
providing a positive electrode current collector with the positive electrode active material layer,
forming a negative electrode by providing a negative electrode current collector with a negative electrode active material layer; and
providing a separator between the positive electrode and the negative electrode in a housing filled with an electrolyte solution,
wherein an electrode is connected to each of the positive electrode current collector and the negative electrode current collector.

### Claim 11 (depends on 3)

A method of manufacturing a power storage device, comprising:
forming the positive electrode according to claim 3;
forming a negative electrode by providing a negative electrode current collector with a negative electrode active material layer; and
providing a separator between the positive electrode and the negative electrode in a housing filled with an electrolyte solution,
wherein an electrode is connected to each of the positive electrode current collector and the negative electrode current collector.

### Claim 12 (depends on 6)

A method of manufacturing a power storage device, comprising:
forming the positive electrode according to claim 6;
forming a negative electrode by providing a negative electrode current collector with a negative electrode active material layer; and
providing a separator between the positive electrode and the negative electrode in a housing filled with an electrolyte solution,
wherein an electrode is connected to each of the positive electrode current collector and the negative electrode current collector.

### Claim 13 (depends on 10)

The method of manufacturing a power storage device, according to claim 10,
wherein a material in the negative electrode active material layer comprises a negative electrode active material with a plurality of whiskers and a conductive layer covering the negative electrode active material with the plurality of whiskers.

### Claim 14 (depends on 11)

The method of manufacturing a power storage device, according to claim 11,
wherein a material in the negative electrode active material layer comprises a negative electrode active material with a plurality of whiskers and a conductive layer covering the negative electrode active material with the plurality of whiskers.

### Claim 15 (depends on 12)

The method of manufacturing a power storage device, according to claim 12,
wherein a material in the negative electrode active material layer comprises a negative electrode active material with a plurality of whiskers and a conductive layer covering the negative electrode active material with the plurality of whiskers.