# US 2013/0283602 A1 · Method of forming a solid state cathode for high energy density secondary batteries

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2013/0283602 A1
- Document ID: US20130283602A1
- Status: Published application
- Kind: A1
- Application number: 13/986,253
- Filed: 2013-04-16
- Published: 2013-10-31
- Earliest claimed: 2010-12-01
- Assignees: QuantumScape Corporation
- Inventors: Isaiah O. Oladeji
- Web page: https://patentgrep.com/patent/US20130283602A1

## CPC

- H01M 10/058: Construction or manufacture
- H01M 4/0404: {by coating on electrode collectors}
- H01M 4/0419: {involving spraying}
- H01M 4/0435: {Rolling or calendering}
- H01M 4/0471: {involving thermal treatment, e.g. firing, sintering, backing particulate active material, thermal decomposition, pyrolysis}
- H01M 4/049: {Manufacturing of an active layer by chemical means}
- H01M 4/1391: of electrodes based on mixed oxides or hydroxides, or on mixtures of oxides or hydroxides, e.g. LiCoOx
- H01M 10/0525: Rocking-chair batteries, i.e. batteries with lithium insertion or intercalation in both electrodes; Lithium-ion batteries
- H01M 10/054: Accumulators with insertion or intercalation of metals other than lithium, e.g. with magnesium or aluminium
- H01M 10/26: Selection of materials as electrolytes
- H01M 10/28: Construction or manufacture
- H01M 4/625: {Carbon or graphite}
- H01M 10/052: Li-accumulators
- H01M 10/0562: Solid materials
- H01M 10/0566: Liquid materials
- Y02E 60/10: Energy storage using batteries
- Y02P 70/50: Manufacturing or production processes characterised by the final manufactured product
- Y10T 29/49108: Electric battery cell making
- Y10T 29/49115: including coating or impregnating
- H01M: PROCESSES OR MEANS, e.g. BATTERIES, FOR THE DIRECT CONVERSION OF CHEMICAL ENERGY INTO ELECTRICAL ENERGY
- Y02E: REDUCTION OF GREENHOUSE GAS [GHG] EMISSIONS, RELATED TO ENERGY GENERATION, TRANSMISSION OR DISTRIBUTION
- Y02P: CLIMATE CHANGE MITIGATION TECHNOLOGIES IN THE PRODUCTION OR PROCESSING OF GOODS
- Y10T: TECHNICAL SUBJECTS COVERED BY FORMER US CLASSIFICATION

## Abstract

A method for making a solid state cathode comprises the following steps: forming an alkali-free first solution comprising at least one transition metal and at least two ligands; spraying this solution onto a substrate that is heated to about 100 to 400° C. to form a first solid film containing the transition metal(s) on the substrate; forming a second solution comprising at least one alkali metal, at least one transition metal, and at least two ligands; spraying the second solution onto the first solid film on the substrate that is heated to about 100 to 400° C. to form a second solid film containing the alkali metal and at least one transition metal; and, heating to about 300 to 1000° C. in a selected atmosphere to react the first and second films to form a homogeneous cathode film. The cathode may be incorporated into a lithium or sodium ion battery.

## Claims

### Claim 1

A method of forming a Li ion battery comprising the steps of:
a) forming a generally planar metallic cathode current collector;
b) forming a substantially alkali-free first solution comprising at least one transition metal and at least two ligands;
c) spraying said first solution onto said current collector while maintaining said current collector at a temperature between about 100 and 400° C. to form a first solid film containing said transition metal on said current collector;
d) forming a second solution comprising at least one alkali metal, at least one transition metal, and at least two ligands;
e) spraying said second solution onto said first solid film on said substrate while maintaining said substrate at a temperature between about 100 and 400° C. to form a second solid film containing said alkali metal and at least one transition metal; and,
f) heating to a temperature between about 300 and 1000° C. in a selected atmosphere to react said first and second films to form a homogeneous cathode film;
g) depositing a solid state electrolyte on said cathode film;
h) depositing a Li metal anode on said solid electrolyte; and,
i) providing a generally planar metallic anode current collector in contact with said Li metal anode.

### Claim 2 (depends on 1)

The method of claim 1 wherein said first solution comprises:
at least one transition metal selected from the group consisting of: Mn, Co, Ni, Al, Fe, and Sn; and,
at least two ligands selected from the group consisting of: urea, acetic acid, citric acid, hydrochloric acid, sulfuric acid, nitric acid, lithium citrate, sodium citrate, triethanolamine, ethylenediamine, ammonia, nitrilotriacetic acid, phosphoric acid, and acetonitrile.

### Claim 3 (depends on 1)

The method of claim 1 wherein said second solution comprises:
an alkali metal selected from the group consisting of: Li and Na;
at least one transition metal selected from the group consisting of: Mn, Co, Ni, Al, Fe, and Sn; and,
at least two ligands selected from the group consisting of: urea, acetic acid, citric acid, hydrochloric acid, sulfuric acid, nitric acid, lithium citrate, sodium citrate, triethanolamine, ethylenediamine, ammonia, nitrilotriacetic acid, and acetonitrile.

### Claim 4 (depends on 1)

The method of claim 1 wherein said solid state electrolyte comprises LIPON deposited on said cathode film by sputtering, and said anode current collector comprises TiN/Cu.

### Claim 5 (depends on 1)

The method of claim 1 wherein said homogeneous cathode film comprises a compound selected from the group consisting of:
LiMn2-xM1xO4 where M1 is selected from the group consisting of Al, Sn, Zn, and Fe, and 0≦x≦0.05;
LiCo1-xM2xO2 where M2 is selected from the group consisting of Ni and Al, and 0≦x≦0.5;
LiNi1-xM3xO2 where M3 is selected from the group consisting of Co and Al, and 0≦x≦0.5;
LiMnxNiyCozAltO2 where x+y+z+t=1, and 0≦(x, y, z, and t)≦1;
LiM4PO4 where M4 is selected from the group consisting of Fe, Co, Ni, and Mn;
NaMn2-xM5xO4 where M5 is selected from the group consisting of Al, Sn, Zn, and Fe, and 0≦x≦0.05;
NaCo1-xM6xO2 where M6 is selected from the group consisting of Ni and Al, and 0≦x≦0.5;
NaNi1-xM7xO2 where M7 is selected from the group consisting of Co and Al, and 0≦x≦0.5;
NaMnxNiyCozAltO2 where x+y+z+t=1, and 0≦(x, y, z, and t)≦1; and,
NaM8PO4 where M8 is selected from the group consisting of Fe, Co, Ni, and Mn.

### Claim 6 (depends on 1)

The method of claim 1 further comprising the step of calendaring to increase the density of said deposited films prior to heating step (f).

### Claim 7 (depends on 6)

The method of claim 6 wherein said calendaring comprises applying a mechanical pressure of at least 2000 psi.

### Claim 8

A method of forming a Li ion battery comprising the steps of:
a) forming a generally planar metallic cathode current collector;
b) forming a substantially alkali-free first solution comprising at least one transition metal and at least two ligands;
c) spraying said first solution onto said current collector while maintaining said current collector at a temperature between about 100 and 400° C. to form a first solid film containing said transition metal on said current collector;
d) forming a second solution comprising at least one alkali metal, at least one transition metal, and at least two ligands;
e) spraying said second solution onto said first solid film on said substrate while maintaining said substrate at a temperature between about 100 and 400° C. to form a second solid film containing said alkali metal and at least one transition metal; and,
f) heating to a temperature between about 300 and 1000° C. in a selected atmosphere to react said first and second films to form a homogeneous cathode film;
g) disposing a polymeric separator on said cathode film;
h) disposing an anode material on the opposite side of said separator from said cathode film to form a cell;
i) placing said cell in a container with leads attached to said anode and said cathode;
j) filling said container with a Li ion conductive liquid electrolyte; and,
k) sealing said container.

### Claim 9 (depends on 8)

The method of claim 8 wherein said first solution comprises:
at least one transition metal selected from the group consisting of: Mn, Co, Ni, Al, Fe, and Sn; and,
at least two ligands selected from the group consisting of: urea, acetic acid, citric acid, hydrochloric acid, sulfuric acid, nitric acid, lithium citrate, sodium citrate, triethanolamine, ethylenediamine, ammonia, nitrilotriacetic acid, phosphoric acid, and acetonitrile.

### Claim 10 (depends on 8)

The method of claim 8 wherein said second solution comprises:
an alkali metal selected from the group consisting of: Li and Na;
at least one transition metal selected from the group consisting of: Mn, Co, Ni, Al, Fe, and Sn; and,
at least two ligands selected from the group consisting of: urea, acetic acid, citric acid, hydrochloric acid, sulfuric acid, nitric acid, lithium citrate, sodium citrate, triethanolamine, ethylenediamine, ammonia, nitrilotriacetic acid, and acetonitrile.

### Claim 11 (depends on 8)

The method of claim 8 wherein said liquid electrolyte comprises LiPF6.

### Claim 12 (depends on 8)

The method of claim 8 wherein said homogeneous cathode film comprises a compound selected from the group consisting of:
LiMn2-xM1xO4 where M1 is selected from the group consisting of Al, Sn, Zn, and Fe, and 0≦x≦0.05;
LiCo1-xM2xO2 where M2 is selected from the group consisting of Ni and Al, and 0≦x≦0.5;
LiNi1-xM3xO2 where M3 is selected from the group consisting of Co and Al, and 0≦x≦0.5;
LiMnxNiyCozAltO2 where x+y+z+t=1, and 0≦(x, y, z, and t)≦1;
LiM4PO4 where M4 is selected from the group consisting of Fe, Co, Ni, and Mn;
NaMn2-xM5xO4 where M5 is selected from the group consisting of Al, Sn, Zn, and Fe, and 0≦x≦0.05;
NaCo1-xM6xO2 where M6 is selected from the group consisting of Ni and Al, and 0≦x≦0.5;
NaNi1-xM7xO2 where M7 is selected from the group consisting of Co and Al, and 0≦x≦0.5;
NaMnxNiyCozAltO2 where x+y+z+t=1, and 0≦(x, y, z, and t)≦1; and,
NaM8PO4 where M8 is selected from the group consisting of Fe, Co, Ni, and Mn.

### Claim 13 (depends on 8)

The method of claim 8 further comprising the step of mechanical calendaring at a pressure of at least 2000 psi to increase the density of said deposited films prior to heating step (f).