# US 2013/0281625 A1 · Methods and Apparatus for Forming Blends of Polyolefin and Resin Modifier

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2013/0281625 A1
- Document ID: US20130281625A1
- Status: Published application
- Kind: A1
- Application number: 13/822,656
- Filed: 2011-08-19
- Published: 2013-10-24
- Earliest claimed: 2010-10-15
- Assignees: ExxonMobile Chemicals Patents Inc.
- Inventors: Jay K. Keung; Yann Devorest; Chia Yung Cheng
- Web page: https://patentgrep.com/patent/US20130281625A1

## CPC

- B29C 48/255: Flow control means, e.g. valves (flow dividers B29C48/695)
- B29C 48/08: flexible, e.g. films
- B29C 48/2886: {of fillers or of fibrous materials, e.g. short-fibre reinforcements}
- B29C 48/29: in liquid form
- B29C 48/385: using two or more serially arranged screws in separate barrels
- B29C 48/397: {using a single screw}
- B29C 48/40: using two or more parallel screws {or at least two parallel non-intermeshing screws}, e.g. twin screw extruders
- B29C 48/53: having a varying channel depth, e.g. varying the diameter of the longitudinal screw trunk
- B29C 48/565: having projections other than the thread, e.g. pins
- B29C 48/793: upstream of the plasticising zone, e.g. heating in the hopper
- B29C 48/832: {Heating}
- B29C 48/91: Heating, e.g. for cross linking
- B29C 48/92: Measuring, controlling or regulating
- C08L 23/12: Polypropene
- B29C 48/022: {characterised by the choice of material}
- B29C 48/365: using pumps, e.g. piston pumps
- B29C 48/387: {using a screw extruder and a gear pump}
- B29C 48/395: using screws surrounded by a cooperating barrel, e.g. single screw extruders
- B29C 48/66: Barrier threads, i.e. comprising primary and secondary threads whereby the secondary thread provides clearance to the barrel for material movement
- B29C 48/767: {through a degassing opening of a barrel}
- B29C 48/83: {Heating or cooling the cylinders}
- B29C 2791/001: Shaping in several steps
- B29C 2948/92704: Temperature
- B29C 2948/92895: Barrel or housing
- B29K 2105/0005: {containing compounding ingredients (releasing, lubricating or separating agents B29C33/56, fibers B29K2105/08, B29K2105/12; fillers B29K2105/16, recycled material B29K2105/26)}
- B29K 2105/06: containing reinforcements, fillers or inserts
- B29K 2105/16: Fillers
- B29K 2995/0053: bi-axially
- B29L 2007/008: {Wide strips, e.g. films, webs}
- B29C: SHAPING OR JOINING OF PLASTICS; SHAPING OF MATERIAL IN A PLASTIC STATE, NOT OTHERWISE PROVIDED FOR; AFTER-TREATMENT OF THE SHAPED PRODUCTS, e.g. REPAIRING (making preforms B29B11/00; making laminated products by combining previously unconnected layers which become one product whose layers will remain together B32B37/00 - B32B41/00)
- C08L: COMPOSITIONS OF MACROMOLECULAR COMPOUNDS (compositions based on polymerisable monomers C08F, C08G; artificial filaments or fibres D01F; textile treating compositions D06)
- B29K: INDEXING SCHEME ASSOCIATED WITH SUBCLASSES B29B, B29C OR B29D, RELATING TO MOULDING MATERIALS OR TO MATERIALS FOR {MOULDS, } REINFORCEMENTS, FILLERS OR PREFORMED PARTS, e.g. INSERTS
- B29L: INDEXING SCHEME ASSOCIATED WITH SUBCLASS B29C, RELATING TO PARTICULAR ARTICLES

## Abstract

A process for preparing a blend of thermoplastic polymer and resin modifier within a single-screw extruder, wherein the resin modifier is a hydrocarbon resin.

## Claims

### Claim 1

A process for preparing a blend of thermoplastic polymer and resin modifier, the process comprising the steps of:
(i) charging neat thermoplastic polymer to a single-screw extruder;
(ii) charging neat resin modifier to the extruder;
(iii) conveying the polyolefin and resin modifier through a feed section of the extruder to form a blend, where the feed section has an average channel depth;
(iv) conveying the blend through a compression section of the extruder to thereby form a molten blend;
(v) mixing the molten blend after said step of conveying the blend through the compression section to thereby impart positive pressure on the molten blend in a downstream direction;
(vi) conveying the molten blend through a metering section, where the metering section has an average channel depth; and
(vii) extruding the molten blend, wherein the blend or molten blend is subjected to a compression ratio that is at least 1.2, where the compression ratio is the ratio of the feed section average channel depth to the metering section average channel depth.

### Claim 2 (depends on 1)

The process of claim 1, where the blend includes a thermoplastic polymer to resin modifier weight ratio of 95:5 to 5:95.

### Claim 3 (depends on 1)

The process of claim 1, where said step of extruding includes forming a film.

### Claim 4 (depends on 1)

The process of claim 1, where said step of charging neat thermoplastic polymer includes charging thermoplastic polymer pellets comprising at least 95 wt % of the thermoplastic polymer, and where said step of charging neat resin modifier includes charging resin pellets comprising at least 95 wt % of the resin modifier.

### Claim 5 (depends on 1)

The process of claim 1, where the thermoplastic polymer is a polyolefin selected from the group consisting of polypropylene and polyethylene.

### Claim 6 (depends on 1)

The process of claim 1, where the resin modifier is an amorphous hydrocarbon resin.

### Claim 7 (depends on 1)

The process of claim 1, where said step of charging thermoplastic polymer and said step of charging resin modifier includes gravimetrically feeding the thermoplastic polymer and resin modifier to the extruder.

### Claim 8 (depends on 1)

The process of claim 1, where the feed section has a length ≧5 L/D.

### Claim 9 (depends on 1)

The process of claim 1, where the feed section has a length ≧8 L/D.

### Claim 10 (depends on 1)

The process of claim 1, where the feed section includes a channel characterized by a feed depth ratio of from 0.150 to about 0.300, and where said step of conveying the thermoplastic polymer and resin modifier through a feed section of the extruder includes conveying the blend through the channel.

### Claim 11 (depends on 1)

The process of claim 1, where said step of conveying the thermoplastic polymer and resin modifier through a feed section of the extruder includes subjecting the blend to a temperature of at least 200° F. (93.3° C.).

### Claim 12 (depends on 1)

The process of claim 1, where said step of conveying the blend through a compression section of the extruder includes subjecting the blend to a temperature of at least 300° F. (149° C.).

### Claim 13 (depends on 1)

The process of claim 1, where said step of conveying the molten blend through a metering section of the extruder includes subjecting the blend to a temperature of at least 350° F. (177° C.).

### Claim 14 (depends on 1)

The process of claim 1, where the compression section includes a first channel having a depth that increases from an upstream point to a downstream point and a second channel having a depth that decreases from the upstream point to the downstream point.

### Claim 15 (depends on 1)

The process of claim 1, where the metering section has a length ≧4 L/D.

### Claim 16 (depends on 1)

The process of claim 1, where the metering section includes a channel characterized by a metering depth ratio of from 0.01 to about 0.250, and where said step of conveying the thermoplastic polymer and resin modifier through the metering section of the extruder includes conveying the blend through the channel.

### Claim 17 (depends on 1)

The process of claim 1, where the compression ratio is at least 1.5.

### Claim 18 (depends on 1)

The process of claim 1, wherein the resin modifier is selected from the group consisting of petroleum resins, polyterpene resins, coal resins, rosins, and mixtures thereof.

### Claim 19 (depends on 1)

The process of claim 1, wherein the resin modifier is selected from the group consisting of cycloaliphatic hydrocarbon resins, hydrogenated cycloaliphatic resins, and aromatic modified cycloaliphatic hydrocarbon resins or mixtures thereof.

### Claim 20 (depends on 1)

The process of claim 1, wherein the resin modifier comprises a polypentadiene resin.

### Claim 21

A process for preparing a blend of thermoplastic polymer and resin modifier, the process comprising the steps of:
(i) charging neat polyolefin to a single-screw extruder;
(ii) charging neat resin modifier to the extruder wherein the resin modifier is selected from the group consisting of hydrogenated cycloaliphatic resins, and aromatic modified cycloaliphatic hydrocarbon resins or mixtures thereof;
(iii) conveying the polyolefin and resin modifier through a feed section of the extruder to form a blend, where the feed section has a feed depth;
(iv) conveying the blend through a compression section of the extruder to thereby form a molten blend;
(v) mixing the molten blend after said step of conveying the blend through the compression section to thereby impart positive pressure on the molten blend in a downstream direction;
(vi) conveying the molten blend through a metering section, where the metering section has a metering depth; and
(vii) extruding the molten blend, where during at least one of said step of conveying through a feed section, said step of conveying through a compression section, and said step of conveying through a metering section, the blend or molten blend is subjected to a pressure imparted a compression ratio that is at least 1.2, where the compression ratio is the ratio of the feed depth to the metering depth.

### Claim 22

A process for preparing a blend of thermoplastic polymer and resin modifier, the process comprising the steps of:
(i) charging neat thermoplastic polymer to a single-screw extruder;
(ii) charging neat resin modifier to the extruder wherein the resin modifier comprises a polycyclopentadiene resin;
(iii) conveying the thermoplastic polymer and resin modifier through a feed section of the extruder to form a blend, where the feed section has a feed depth;
(iv) conveying the blend through a compression section of the extruder to thereby form a molten blend;
(v) mixing the molten blend after said step of conveying the blend through the compression section to thereby impart positive pressure on the molten blend in a downstream direction;
(vi) conveying the molten blend through a metering section, where the metering section has metering depth; and
(vii) extruding the molten blend, where during at least one of said step of conveying through a feed section, said step of conveying through a compression section, and said step of conveying through a metering section, the blend or molten blend is subjected to a pressure imparted a compression ratio that is at least 1.2, where the compression ratio is the ratio of the feed depth to the metering depth.