# US 2013/0281586 A1 · Graft copolymer, production method therefor, resin composition, and molded article

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2013/0281586 A1
- Document ID: US20130281586A1
- Status: Published application
- Kind: A1
- Application number: 13/977,300
- Filed: 2011-12-27
- Published: 2013-10-24
- Earliest claimed: 2010-12-28
- Assignees: Mitsubishi Rayon Co., Ltd.
- Inventors: Hiroaki Otonari; Takashi Miura; Toshihiro Kasai
- Web page: https://patentgrep.com/patent/US20130281586A1

## CPC

- C08G 77/442: containing vinyl polymer sequences
- C08F 283/12: on to polysiloxanes
- C08F 283/124: {on to polysiloxanes having carbon-to-carbon double bonds}
- C08L 51/085: {on to polysiloxanes}
- C08L 69/00: Compositions of polycarbonates; Compositions of derivatives of polycarbonates
- C08L 2201/02: Flame or fire retardant/resistant
- C08G: MACROMOLECULAR COMPOUNDS OBTAINED OTHERWISE THAN BY REACTIONS ONLY INVOLVING UNSATURATED CARBON-TO-CARBON BONDS
- C08F: MACROMOLECULAR COMPOUNDS OBTAINED BY REACTIONS ONLY INVOLVING CARBON-TO-CARBON UNSATURATED BONDS
- C08L: COMPOSITIONS OF MACROMOLECULAR COMPOUNDS (compositions based on polymerisable monomers C08F, C08G; artificial filaments or fibres D01F; textile treating compositions D06)

## Abstract

Disclosed are a method of producing a graft copolymer, comprising polymerizing a vinyl monomer (B) containing a polyfunctional vinyl monomer (b1) in the presence of a polyorganosiloxane rubber (A) comprising more than 20% by mass of a toluene-insoluble matter, wherein a mass percentage of the polyfunctional vinyl monomer (b1) is 11 to 19% by mass based on 100% by mass of a total amount of the polyorganosiloxane rubber (A) and the vinyl monomer (B); a graft copolymer obtained by the method; a resin composition being prepared by blending the graft copolymer with a resin and having high impact resistance and heat resistance and sufficient flame retardancy; and a molded article obtained by molding the resin composition.

## Claims

### Claim 1

A method of producing a graft copolymer, comprising polymerizing a vinyl monomer (B) containing a polyfunctional vinyl monomer (b1) in the presence of a polyorganosiloxane rubber (A) comprising more than 20% by mass of a toluene-insoluble matter,
wherein a mass percentage of the polyfunctional vinyl monomer (b1) is 11 to 19% by mass based on 100% by mass of a total amount of the polyorganosiloxane rubber (A) and the vinyl monomer (B).

### Claim 2 (depends on 1)

The method of producing a graft copolymer according to claim 1, wherein the polyfunctional vinyl monomer (b1) is allyl methacrylate.

### Claim 3 (depends on 1)

The method of producing a graft copolymer according to claim 1, wherein the mass percentage of the polyfunctional vinyl monomer (b1) is 13 to 17% by mass based on 100% by mass of the total amount of the polyorganosiloxane rubber (A) and the vinyl monomer (B).

### Claim 4 (depends on 1)

A graft copolymer obtained by the production method according to claim 1.

### Claim 5 (depends on 4)

A resin composition comprising 100 parts by mass of a resin and 0.5 to 20 parts by mass of the graft copolymer according to claim 4.

### Claim 6 (depends on 5)

The resin composition according to claim 5, wherein the resin is polycarbonate.

### Claim 7 (depends on 5)

A molded article obtained by molding the resin composition according to claim 5.

### Claim 8 (depends on 7)

The molded article according to claim 7, wherein the molded article is a casing for home appliances.

### Claim 9

A graft copolymer, wherein when 5 parts by mass of the graft copolymer is blended with 100 parts by mass of a polycarbonate having a viscosity average molecular weight of 22000, 0.3 parts by mass of a phenol antioxidant represented by the following formula (1), 0.3 parts by mass of a phosphorus antioxidant represented by the following formula (2), and 0.5 parts by mass of a polytetrafluoroethylene having a mass average molecular weight of 8000000 to 15000000,
(1) Charpy impact strength at −30° C. is 20 kJ/m2 or more, and
(2) a total burning time of a molded article having a thickness of 1.6 mm in a UL94V test is 40 s or less:

### Claim 10 (depends on 9)

The graft copolymer according to claim 9, wherein
(3) a deflection temperature under load at a load of 1.8 MPa is 118° C. or more.

### Claim 11 (depends on 9)

A resin composition comprising 100 parts by mass of a resin and 0.5 to 20 parts by mass of the graft copolymer according to claim 9.

### Claim 12 (depends on 11)

The resin composition according to claim 11, wherein the resin is polycarbonate.

### Claim 13 (depends on 11)

A molded article obtained by molding the resin composition according to claim 11.

### Claim 14 (depends on 13)

The molded article according to claim 13, wherein the molded article is a casing for home appliances.