# US 2013/0281582 A1 · Polylactide-graft-lignin blends and copolymers

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2013/0281582 A1
- Document ID: US20130281582A1
- Status: Published application
- Kind: A1
- Application number: 13/850,447
- Filed: 2013-03-26
- Published: 2013-10-24
- Earliest claimed: 2012-03-26
- Inventors: John R. Dorgan; Michael Paul Eyser; Clay Perbix
- Web page: https://patentgrep.com/patent/US20130281582A1

## CPC

- C08G 63/00: Macromolecular compounds obtained by reactions forming a carboxylic ester link in the main chain of the macromolecule (polyester-amides C08G69/44; polyester-imides C08G73/16)
- C08G 63/912: {derived from hydroxycarboxylic acids}
- C08H 6/00: {Macromolecular compounds derived from lignin, e.g. tannins, humic acids}
- C08L 67/04: Polyesters derived from hydroxycarboxylic acids, e.g. lactones (C08L67/06 takes precedence)
- C08L 97/005: {Lignin}
- C08G: MACROMOLECULAR COMPOUNDS OBTAINED OTHERWISE THAN BY REACTIONS ONLY INVOLVING UNSATURATED CARBON-TO-CARBON BONDS
- C08H: DERIVATIVES OF NATURAL MACROMOLECULAR COMPOUNDS (polysaccharides C08B; natural rubber C08C; natural resins or their derivatives C09F; bituminous materials C10)
- C08L: COMPOSITIONS OF MACROMOLECULAR COMPOUNDS (compositions based on polymerisable monomers C08F, C08G; artificial filaments or fibres D01F; textile treating compositions D06)

## Abstract

The present invention is directed to a PLA-graft-lignin polymers and copolymers and methods of making the same. As the lignocellulosic biorefining industry emerges as a viable fuels technology, the availability of the assortment of lignins will also expand. The use of lignins as a copolymer is one area where lignin may be utilized.

## Claims

### Claim 1

A method to produce a polylactide-graft-lignin blend, the method comprising:
butyrate a lignin to produce a butyrated lignin;
heating a polylactic acid to a temperature between about 160° C. to about 190° C.; and
mixing the heated polylactic acid with the butyrated lignin to produce a polylactide-graft-lignin blend.

### Claim 2 (depends on 1)

The method of claim 1, further comprising cooling the polylactide-graft-lignin blend.

### Claim 3 (depends on 1)

The method of claim 1, further comprising adding a stabilizer solution to the heated polylactic acid before mixing the heated polylactic acid with the butyrated lignin.

### Claim 4 (depends on 1)

The method of claim 1, wherein the lignin is between about 0.5 wt. % to about 40 wt. %.

### Claim 5 (depends on 1)

The method of claim 1, wherein the method for butyration of a lignin comprising:
drying the lignins;
mixing the lignin in butyric acid for between about 96 hours to about 264 hours to produce a butyrated lignin;
isolating the butyrated lignin; and
washing the butyrated lignin.

### Claim 6 (depends on 5)

The method of claim 5, wherein the lignins are dried at between about 100° C. and about 150° C.

### Claim 7 (depends on 5)

The method of claim 5, wherein the lignins are dried at about 125° C.

### Claim 8 (depends on 6)

The method of claim 6, wherein the lignins are dried for between about 12 hours to about 48 hours.

### Claim 9 (depends on 6)

The method of claim 6, wherein the lignins are dried for about 24 hours.

### Claim 10 (depends on 5)

The method of claim 5, wherein the lignins are reacted in the butyric acid at between about 30° C. and about 75° C. under vigorous agitation.

### Claim 11 (depends on 5)

The method of claim 5, wherein the lignin is reacted in the butyric acid at about 50° C. under vigorous agitation.

### Claim 12 (depends on 5)

The method of claim 5, wherein the lignin is selected from the group consisting of alkali lignin and organosolv lignin.

### Claim 13 (depends on 5)

The method of claim 5, wherein the lignin is reacted in the butyric acid and purged with an inert gas, wherein the inert gas is selected from the group consisting of nitrogen, argon, and helium.

### Claim 14

A method to produce a polylactide-graft-lignin copolymer, the method comprising:
drying a lignin to produce a dried lignin;
purging the dried lignin to produce a purged dried lignin;
adding a solvent to the purged dried lignin to produce a suspension;
adding purged lactide to the suspension to produce a lactide-suspension;
adding a catalyst to the lactide-suspension to produce a mixture; and
polymerizing the mixture to produce the polylactide-graft-lignin copolymer.

### Claim 15 (depends on 14)

The method of claim 14, further comprising adding chloroform to the polylactide-graft-lignin copolymer to produce a chloroform-polylactide-graft-lignin copolymer.

### Claim 16 (depends on 15)

The method of claim 15, further comprising adding poly(acrylic acid) to the chloroform-polylactide-graft-lignin copolymer.

### Claim 17 (depends on 14)

The method of claim 14, wherein the lignin is selected from the group consisting of alkali lignin and organosolv lignin.

### Claim 18

A copolymer, the copolymer comprising:
polylactide; and
a butyrated lignin.

### Claim 19 (depends on 18)

The copolymer of claim 18, wherein the butyrated polymer is selected from the group consisting of butyrated alkali lignin and butyrated organosolv lignin.

### Claim 20 (depends on 18)

The copolymer of claim 18, wherein the weight percent of the butyrated lignin is between 0.5 wt. % to about 40 wt. % of the copolymer.