# US 2013/0281568 A1 · Flame Retardant Thermoplastic Resin Composition

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2013/0281568 A1
- Document ID: US20130281568A1
- Status: Published application
- Kind: A1
- Application number: 13/924,878
- Filed: 2013-06-24
- Published: 2013-10-24
- Earliest claimed: 2010-12-28
- Assignees: Cheil Industries Inc.
- Applicants: Cheil Industries Inc.
- Inventors: Hwan Seok PARK; Seung Shik SHIN; Kyuong Sik CHIN; Yun Ku NAM; Jong Tae YOON
- Web page: https://patentgrep.com/patent/US20130281568A1

## CPC

- C08K 5/52: Phosphorus bound to oxygen only
- C08J 3/20: Compounding polymers with additives, e.g. colouring
- C08L 51/04: grafted on to rubbers
- C08L 55/02: ABS [Acrylonitrile-Butadiene-Styrene] polymers
- C08L 69/00: Compositions of polycarbonates; Compositions of derivatives of polycarbonates
- C08J 2369/00: Characterised by the use of polycarbonates; Derivatives of polycarbonates
- C08K 5/523: with hydroxyaryl compounds
- C08L 2201/02: Flame or fire retardant/resistant
- C08L 2205/025: containing two or more polymers of the same hierarchy C08L, and differing only in parameters such as density, comonomer content, molecular weight, structure
- C08K: Use of inorganic or non-macromolecular organic substances as compounding ingredients (paints, inks, varnishes, dyes, polishes, adhesives C09)
- C08J: WORKING-UP; GENERAL PROCESSES OF COMPOUNDING; AFTER-TREATMENT NOT COVERED BY SUBCLASSES C08B, C08C, C08F, C08G or C08H (working, e.g. shaping, of plastics B29)
- C08L: COMPOSITIONS OF MACROMOLECULAR COMPOUNDS (compositions based on polymerisable monomers C08F, C08G; artificial filaments or fibres D01F; textile treating compositions D06)

## Abstract

A flame retardant thermoplastic resin composition includes (a) a polycarbonate resin, (b) an impact modifier, and (c) resorcinol bis(diphenyl phosphate). The impact modifier includes (b1) a large rubber particle-modified vinyl graft copolymer wherein the rubber particle has an average particle diameter of about 0.3 to about 0.7 μm, and (b2) a small rubber particle-modified graft copolymer wherein the rubber particle has an average particle diameter of about 0.05 to about 0.27 μm. The flame retardant thermoplastic resin composition can have excellent flowability, mold formability, flame retardancy, impact strength, and gloss characteristics.

## Claims

### Claim 1

A flame retardant thermoplastic resin composition comprising (a) a polycarbonate resin, (b) an impact modifier, and (c) resorcinol bis(diphenyl phosphate) wherein the impact modifier comprises (b1) a large rubber particle-modified vinyl graft copolymer wherein the rubber particle has an average particle diameter of about 0.3 μm to about 0.7 μm, and (b2) a small rubber particle-modified graft copolymer wherein the rubber particle has an average particle diameter of about 0.05 μm to about 0.27 μm.

### Claim 2 (depends on 1)

The flame retardant thermoplastic resin composition according to claim 1, wherein the thermoplastic resin composition comprises about 100 parts by weight of a base resin comprising about 80 wt % to about 99 wt % of the polycarbonate resin (a) and about 1 wt % to about 20 wt % by weight of the impact modifier (b), and about 7 to about 30 parts by weight of resorcinol bis(diphenyl phosphate).

### Claim 3 (depends on 1)

The flame retardant thermoplastic resin composition according to claim 1, wherein the large rubber particle-modified vinyl graft copolymer (b1) and the small rubber particle-modified graft copolymer (b2) are present in a weight ratio of about 1:1.3 to about 1:3.

### Claim 4 (depends on 1)

The flame retardant thermoplastic resin composition according to claim 1, wherein the small rubber particle-modified graft copolymer (b2) includes units derived from a C1-C8 alkyl (meth)acrylate.

### Claim 5 (depends on 1)

The flame retardant thermoplastic resin composition according to claim 1, wherein the thermoplastic resin composition has a gloss of 98 to 105 (ASTM D523, 60°), a melt flow index (ISO 1133, 220° C., 10 kg) of about 100 to about 130 g/10 min, and a flame retardancy rating (UL94, 2 mm) of V-0.

### Claim 6 (depends on 1)

The flame retardant thermoplastic resin composition according to claim 1, further comprising one or more additives selected from the group consisting of antioxidants, nucleating agents, surfactants, coupling agents, fillers, plasticizers, lubricants, antibacterial agents, release agents, heat stabilizers, light stabilizers, compatibilizers, inorganic additives, colorants, stabilizers, lubricating agents, antistatic agents, pigments, dyes, and flame-proofing agents.

### Claim 7 (depends on 1)

A molded article produced by molding the flame retardant thermoplastic resin composition according to claim 1.