# US 2013/0280893 A1 · Method for production of selective growth masks using imprint lithography

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2013/0280893 A1
- Document ID: US20130280893A1
- Status: Published application
- Kind: A1
- Application number: 13/867,629
- Filed: 2013-04-22
- Published: 2013-10-24
- Earliest claimed: 2012-04-23
- Assignees: Nanocrystal Asia Inc.
- Applicants: Nanocrystal Asia Inc.
- Inventors: Chong-Ming LEE; Andrew Eng-Jia Lee
- Web page: https://patentgrep.com/patent/US20130280893A1

## CPC

- H10P 76/00: Manufacture or treatment of masks on semiconductor bodies, e.g. by lithography or photolithography
- H10H 20/01335: {the light-emitting regions comprising nitride materials}
- H10P 14/271: {characterised by the preparation of substrate for selective deposition}
- H10P 14/2921: {being crystalline insulating materials}
- H10P 14/3216: {Nitrides}
- H10P 14/3416: {Nitrides}
- H10P 14/3462: {Nanowires}
- H10H 20/818: within the light-emitting regions
- H10P: GENERIC PROCESSES OR APPARATUS FOR THE MANUFACTURE OR TREATMENT OF DEVICES COVERED BY CLASS H10
- H10H: INORGANIC LIGHT-EMITTING SEMICONDUCTOR DEVICES HAVING POTENTIAL BARRIERS

## Abstract

The present invention discloses a method for production of selective growth masks using imprint lithography. The method includes steps of: providing a sapphire substrate, forming a GaN layer, an insulation layer, and a photo-resistive layer, performing imprint lithography, performing exposure and development, performing dry etching, and removing the remained photo-resistive layer. The selective growth masks produced by the method of the present invention make the growth of nanowires cylindrical and perpendicular to the GaN layer, and each nanowire is parallel to one another.

## Claims

### Claim 1

A method for production of selective growth masks using imprint lithography, comprising steps of:
providing a sapphire substrate, wherein the sapphire substrate is a base for forming material layers;
forming a GaN layer, an insulation layer, and a photo-resistive layer, wherein the GaN layer is formed on the sapphire substrate, the insulation layer is formed on the GaN layer, and the photo-resistive layer is formed on the insulation layer;
performing imprint lithography, wherein the photo-resistive layer is imprinted with a pattern of plural holes so as to transfer the pattern of said holes on the surface of the photo-resistive layer;
performing exposure and development, wherein the imprinted photo-resistive layer is illuminated by a light source to form corresponding holes in the photo-resistive layer so as to expose the insulation layer through said holes of the photo-resistive layer;
performing dry etching, wherein the insulation layer under said holes of the photo-resistive layer is removed by dry etching and the GaN layer is exposed through said holes of the photo-resistive layer; and
removing the remained photo-resistive layer.

### Claim 2 (depends on 1)

The method for production of selective growth masks of claim 1, wherein the GaN layer is formed by Metal-Organic Chemical Vapor Deposition (MOCVD).

### Claim 3 (depends on 1)

The method for production of selective growth masks of claim 1, wherein the insulation layer is formed by Plasma Enhanced Chemical Vapor Deposition (PECVD).

### Claim 4 (depends on 1)

The method for production of selective growth masks of claim 1, wherein the insulation layer is made of silicon oxide (SiO2) or silicon nitride (SiNx).

### Claim 5 (depends on 1)

The method for production of selective growth masks of claim 1, wherein the thickness of the insulation layer is 20˜2,000 nm.

### Claim 6 (depends on 1)

The method for production of selective growth masks of claim 1, wherein the thickness of the photo-resistive layer is 20˜2,000 nm.

### Claim 7 (depends on 1)

The method for production of selective growth masks of claim 1, wherein the thickness of the photo-resistive layer is the same as the thickness of the insulation layer.

### Claim 8 (depends on 1)

The method for production of selective growth masks of claim 1, wherein the imprint lithography is a nano-meter imprint lithography or a micro-meter imprint lithography.

### Claim 9 (depends on 1)

The method for production of selective growth masks of claim 1, wherein the light source is a 248 nm KrF light source, a 193 nm ArF light source, or a 13.5 nm EUV light source.

### Claim 10 (depends on 1)

The method for production of selective growth masks of claim 1, wherein the dry etching is a chemical dry etching, a plasma etching, or a combined physical-chemical etching.