# US 2013/0280879 A1 · Method for Producing a Conductor Line

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2013/0280879 A1
- Document ID: US20130280879A1
- Status: Published application
- Kind: A1
- Application number: 13/452,044
- Filed: 2012-04-20
- Published: 2013-10-24
- Earliest claimed: 2012-04-20
- Assignees: Infineon Technologies Austria AG
- Inventors: Matthias Stecher; Markus Menath; Andreas Zankl; Anja Gissibl
- Web page: https://patentgrep.com/patent/US20130280879A1

## CPC

- H10W 20/082: {the openings being tapered via holes}
- H10D 64/011: {of electrodes ohmically coupled to a semiconductor}
- H10P 32/20: Diffusion for doping of insulating layers
- H10P 36/00: Gettering within semiconductor bodies
- H10P 50/28: of insulating materials
- H10P 50/73: {using masks for insulating materials}
- H10W 20/021: {of interconnections within wafers or substrates}
- H10W 20/081: {by forming openings in the dielectric parts}
- H10W 20/089: {using processes for implementing desired shapes or dispositions of the openings, e.g. double patterning}
- H10W 20/423: {Shielding layers}
- H10W 20/425: {Barrier, adhesion or liner layers}
- H10W 20/435: {Cross-sectional shapes or dispositions of interconnections}
- H10W 20/47: comprising two or more dielectric layers having different properties, e.g. different dielectric constants
- H10W 20/48: Insulating materials thereof
- H10W 20/495: {Capacitive arrangements or effects of, or between wiring layers}
- H10W 20/497: {Inductive arrangements or effects of, or between, wiring layers}
- H10W: GENERIC PACKAGES, INTERCONNECTIONS, CONNECTORS OR OTHER CONSTRUCTIONAL DETAILS OF DEVICES COVERED BY CLASS H10
- H10D: INORGANIC ELECTRIC SEMICONDUCTOR DEVICES
- H10P: GENERIC PROCESSES OR APPARATUS FOR THE MANUFACTURE OR TREATMENT OF DEVICES COVERED BY CLASS H10

## Abstract

A method for producing a rounded conductor line of a semiconductor component is disclosed. In that method, a partially completed semiconductor component is provided. The partially completed semiconductor component has a bottom side and a top side spaced distant from the bottom side in a vertical direction. Also provided is an etchant. On the top side, a dielectric layer is arranged. The dielectric layer has at least two different regions that show different etch rates when they are etched with the etchant. Subsequently, a trench is formed in the dielectric layer such that the trench intersects each of the different regions. Then, the trench is widened by etching the trench with the etchant at different etch rates. By filling the widened trench with an electrically conductive material, a conductor line is formed.

## Claims

### Claim 1

A method for producing a conductor line of a semiconductor component, the method comprising:
providing a partially completed semiconductor component with a bottom side and a top side, the top side spaced distant from the bottom side in a vertical direction;
providing an etchant;
arranging a dielectric layer on the top side, the dielectric layer having at least two different regions with different etch rates when being etched with the etchant;
forming a trench in the dielectric layer such that the trench intersects each of the at least two different regions;
widening the trench by etching the trench with the etchant such that the at least two different regions are etched with the different etch rates;
forming the conductor line by filling the widened trench with an electrically conductive material.

### Claim 2 (depends on 1)

The method of claim 1, wherein the dielectric layer comprises a base material which is doped with at least one dopant having, in the vertical direction, a nonconstant course of concentration, wherein the at least one dopant affects an etch rate of the doped base material if the latter is etched with the etchant.

### Claim 3 (depends on 2)

The method as claimed in claim 2, wherein
the at least two different regions are formed as sub-layers; and
the nonconstant course of concentration of the at least one dopant in adjacent ones of the sub-layers is different.

### Claim 4 (depends on 2)

The method as claimed in claim 2, wherein the at least one dopant has, in the vertical direction, a gradient of at least at least 1 weight % per μm or of at least 2 atom % per μm.

### Claim 5 (depends on 2)

The method as claimed in claim 2, wherein the at least one dopant has, in the vertical direction, a gradient of at less than or equal to −1 weight % per μm, or of less than or equal to −2 weight % per μm.

### Claim 6 (depends on 2)

The method as claimed in claim 2, wherein
the at least one dopant comprises, within the dielectric layer and along a line parallel to the vertical direction, a maximum dopant concentration;
a place of the maximum dopant concentration is spaced distant from the top side.

### Claim 7 (depends on 2)

The method as claimed in claim 2, wherein the at least one dopant is one of phosphorus (P), boron (B), silver (Ag), arsenic (As), argon (Ar).

### Claim 8 (depends on 1)

The method as claimed in claim 1, further comprising:
arranging a mask layer on the top side, the mask layer comprising an opening;
forming the trench by etching the dielectric layer underneath the opening, thereby using the mask layer as an etching mask.

### Claim 9 (depends on 8)

The method as claimed in claim 8, wherein filling the widened trench comprises introducing the electrically conductive material through the opening into the widened trench.

### Claim 10 (depends on 8)

The method as claimed in claim 8, further comprising removing partially or completely the mask layer and a part of the electrically conductive material arranged in the opening.

### Claim 11 (depends on 8)

The method as claimed in claim 8, wherein, in a cross-sectional plane perpendicular to a running direction of the widened trench,
(a) the opening comprises a minimum width;
(b) the widened trench comprises, in a region between the opening and the bottom side, a maximum width, wherein the maximum width is greater than the minimum width.

### Claim 12 (depends on 11)

The method as claimed in claim 11, wherein, in the cross-sectional plane perpendicular to the running direction of the widened trench, the maximum width is greater than a difference between
(a) a distance between the bottom side and the opening; and
(b) a distance between the bottom side and the conductor line.

### Claim 13 (depends on 8)

The method as claimed in claim 8, wherein no additional material is deposited on a surface of the widened trench, prior to filling the widened trench with the electrically conductive material.

### Claim 14 (depends on 1)

The method as claimed in claim 1, wherein the dielectric layer comprises a silicon oxide (SiOx).

### Claim 15 (depends on 1)

The method as claimed in claim 1, wherein the conductor line comprises, in a cross-sectional plane perpendicular to a running direction of the widened trench, a surface with a surface location at which a radius of curvature of the location is in the range from 0.4 μm to 3.2 μm.

### Claim 16 (depends on 1)

The method as claimed in claim 1, wherein the conductor line comprises, in a cross-sectional plane perpendicular to a running direction of the widened trench, a continuous surface path that extends, in the vertical direction, over a distance of at least 100 nm or of at least 0.8 μm and that has everywhere a radius of curvature in a range from 0.4 μm 3.2 μm.

### Claim 17 (depends on 1)

The method as claimed in claim 1, wherein the electrically conductive material
(a) consists of copper or aluminum; or
(b) comprises copper or aluminum; or
(c) consists of copper and aluminum; or
(d) comprises copper and aluminum; or
(e) comprises or consists of polycrystalline semiconductor material.

### Claim 18 (depends on 1)

The method as claimed in claim 1, wherein the conductor line is an outer winding of a coil of a coreless transformer of the semiconductor component.

### Claim 19 (depends on 18)

The method as claimed in claim 18, wherein the coreless transformer galvanically decouples a control circuit configured to control a semiconductor element from a control electrode of the semiconductor element.

### Claim 20 (depends on 1)

The method as claimed in claim 1, wherein the conductor line is an electrode of a capacitor.

### Claim 21 (depends on 20)

The method as claimed in claim 20, wherein the capacitor galvanically decouples a control circuit configured to control a semiconductor element from a control electrode of the semiconductor element.

### Claim 22

A method for producing a conductor line of a semiconductor component, the method comprising:
providing a partially completed semiconductor component with a bottom side and a top side spaced distant from the bottom side in a vertical direction;
arranging a dielectric layer on the top side, the dielectric layer being doped with a dopant having, in the vertical direction, a nonconstant course of concentration;
forming a trench in the dielectric layer such that the trench intersects regions of the dielectric layer, the regions having different dopant concentrations;
widening the trench by etching the trench at different etch rates caused by the different dopant concentrations;
forming a conductor line by filling the widened trench with an electrically conductive material.

### Claim 23 (depends on 22)

The method as claimed in claim 22, wherein the conductor line comprises, in a cross-sectional plane perpendicular to a running direction of the widened trench, a surface location at which a radius of curvature of the surface location is in a range from 0.4 μm to 3.2 μm.

### Claim 24 (depends on 23)

The method of claim 23 wherein
the trench is spiral-shaped; and;
the conductor line is spiral-shaped and forms an outer winding of a coil of a coreless transformer of the semiconductor component.

### Claim 25

A method for producing a conductor line of a semiconductor component, the method comprising:
providing a partially completed semiconductor component with a bottom side and a top side spaced distant from the bottom side in a vertical direction;
providing an etchant;
arranging a dielectric layer that is doped with a dopant on the top side by subsequently depositing a number of at least two sub-layers, wherein in any two adjacent ones of the at least two sub-layers a concentration of the dopant is
(a) different; or
(b) zero in one of the two adjacent ones of the at least two sub-layers and greater than zero in the other one of the two adjacent ones of the at least two sub-layers;
forming a trench in the dielectric layer such that the trench intersects each of the at least two sub-layers;
widening the trench by etching the trench at different etch rates caused by different concentrations of the dopant;
forming a conductor line by filling the widened trench with an electrically conductive material.

### Claim 26 (depends on 25)

The method as claimed in claim 25, wherein the conductor line comprises, in a cross-sectional plane, a surface with a surface location at which a radius of curvature of the location is in a range from 0.4 μm to 3.2 μm.