# US 2013/0280875 A1 · Method of manufacturing strained source/drain structures

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2013/0280875 A1
- Document ID: US20130280875A1
- Status: Published application
- Kind: A1
- Application number: 13/920,703
- Filed: 2013-06-18
- Published: 2013-10-24
- Earliest claimed: 2011-06-15
- Assignees: Taiwan Semiconductor Manufacturing Company, Ltd.
- Applicants: Taiwan Semiconductor Manufacturing Company, Ltd.
- Inventors: Chun-Fai CHENG; Li-Ping HUANG; Ka-Hing FUNG
- Web page: https://patentgrep.com/patent/US20130280875A1

## CPC

- H10D 30/025: {of vertical IGFETs (of VDMOS H10D30/0291; of vertical TFTs H10D30/0318)}
- H10D 30/0218: {having pocket halo regions selectively formed at the sides of the gates}
- H10D 30/022: {having lightly-doped source or drain extensions selectively formed at the sides of the gates}
- H10D 30/0223: {having source and drain regions or source and drain extensions self-aligned to sides of the gate}
- H10D 30/0275: {forming single crystalline semiconductor source or drain regions resulting in recessed gates, e.g. forming raised source or drain regions}
- H10D 30/60: Insulated-gate field-effect transistors [IGFET] (H10D30/40 takes precedence)
- H10D 30/797: {being in source or drain regions, e.g. SiGe source or drain}
- H10D 62/021: {Forming source or drain recesses by etching e.g. recessing by etching and then refilling}
- H10D 62/307: {the doping variations being parallel to the channel lengths}
- H10D 62/371: {Inactive supplementary semiconductor regions, e.g. for preventing punch-through, improving capacity effect or leakage current}
- H10D 62/822: comprising only Group IV materials heterojunctions, e.g. Si/Ge heterojunctions
- H10D 64/259: {Source or drain electrodes being self-aligned with the gate electrode and having bottom surfaces higher than the interface between the channel and the gate dielectric}
- H10D 64/691: {comprising metallic compounds, e.g. metal oxides or metal silicates (insulators comprising nitrogen H10D64/693)}
- H10D: INORGANIC ELECTRIC SEMICONDUCTOR DEVICES

## Abstract

A method includes forming a gate structure over a semiconductor substrate. The gate structure defines a channel region in the semiconductor substrate. Trenches are formed in the semiconductor substrate, and the trenches are interposed by the channel region. A first semiconductor layer is epitaxially grown in the trenches, and the first semiconductor layer has a first dopant with a first dopant concentration. A second semiconductor layer is epitaxially grown over the first semiconductor layer, and the second semiconductor layer has a second dopant with a second dopant concentration. The second dopant has an electrical carrier type opposite to an electrical carrier type of the first dopant.

## Claims

### Claim 1

A method comprising:
forming a gate structure over a semiconductor substrate, the gate structure defining a channel region in the semiconductor substrate;
forming trenches in the semiconductor substrate, interposed by the channel region;
epitaxially growing a first semiconductor layer in the trenches, the first semiconductor layer having a first dopant with a first dopant concentration; and
epitaxially growing a second semiconductor layer over the first semiconductor layer, the second semiconductor layer having a second dopant with a second dopant concentration, wherein the second dopant has an electrical carrier type opposite to an electrical carrier type of the first dopant.

### Claim 2 (depends on 1)

The method of claim 1, further comprising:
forming spacers adjoining opposite sidewalls of the gate structure;

### Claim 3 (depends on 1)

The method of claim 1, wherein the first dopant concentration ranges from about 1E18 atoms/cm3 to about 5E19 atoms/cm3.

### Claim 4 (depends on 1)

The method of claim 1, wherein the second dopant concentration ranges from about 5E19 atoms/cm3 to about 5E21 atoms/cm3.

### Claim 5 (depends on 1)

The method of claim 1, wherein the epitaxially growing the first semiconductor layer is performed by epitaxially growing SiGe, and the first dopant is phosphorous or arsenic.

### Claim 6 (depends on 1)

The method of claim 1, wherein the epitaxially growing the second semiconductor layer is performed by epitaxially growing SiGe, and the second dopant is boron or BF2.

### Claim 7 (depends on 1)

The method of claim 1, wherein the epitaxially growing the first semiconductor layer is performed by epitaxially growing Si or SiC, and the first dopant is boron or BF2.

### Claim 8 (depends on 1)

The method of claim 1, wherein the epitaxially growing the second semiconductor layer is performed by epitaxially growing Si or SiC, and the second dopant is phosphorous or arsenic.

### Claim 9 (depends on 1)

The method of claim 1, wherein the second dopant concentration is set to be higher than the first dopant concentration.

### Claim 10

A method comprising:
forming a trench in a semiconductor substrate, the trench being adjacent to a channel region;
forming a first structure in the trench, the first structure being in contact with a bottom surface and sidewalls of the trench, and the first structure having a first dopant with a first dopant concentration; and
forming a second structure over the first structure and at least partially in the trench, the second structure having a second dopant with a second dopant concentration, and the second dopant having an electrical carrier type opposite to an electrical carrier type of the first dopant.

### Claim 11 (depends on 10)

The method of claim 10, wherein the first dopant concentration ranges from about 1E18 atoms/cm3 to about 5E19 atoms/cm3.

### Claim 12 (depends on 10)

The method of claim 10, wherein the second dopant concentration ranges from about 5E19 atoms/cm3 to about 5E21 atoms/cm3.

### Claim 13 (depends on 10)

The method of claim 10, wherein the forming the first structure is performed by epitaxially growing SiGe, and the first dopant is phosphorous or arsenic.

### Claim 14 (depends on 10)

The method of claim 10, wherein the forming the second structure is performed by epitaxially growing SiGe, and the second dopant is boron or BF2.

### Claim 15 (depends on 10)

The method of claim 10, wherein the forming the first structure is performed by epitaxially growing Si or SiC, and the first dopant is boron or BF2.

### Claim 16 (depends on 10)

The method of claim 10, wherein the forming the second structure is performed by epitaxially growing Si or SiC, and the second dopant is phosphorous or arsenic.

### Claim 17 (depends on 10)

The method of claim 10, wherein the second dopant concentration is set to be higher than the first dopant concentration.

### Claim 18

A method comprising:
forming a gate structure over a substrate, the gate structure defining a channel region in the substrate;
forming two trenches in the substrate, the two trenches being interposed by the channel region, and sidewalls and the bottom portions of the two trenches being along one or more {111} facets of the substrate;
epitaxially growing a first structure in the trenches, the first structure extending along the sidewalls and bottom portions of the two trenches, and the first structure having a first dopant with a first dopant concentration; and
epitaxially growing a second structure over the first structure, the second structure having a second dopant with a second dopant concentration, the second dopant having an electrical carrier type opposite to an electrical carrier type of the first dopant.

### Claim 19 (depends on 18)

The method of claim 18, wherein the first dopant concentration ranges from about 1E18 atoms/cm3 to about 5E19 atoms/cm3.

### Claim 20 (depends on 18)

The method of claim 18, wherein the second dopant concentration ranges from about 5E19 atoms/cm3 to about 5E21 atoms/cm3.