# US 2013/0280858 A1 · Semiconductor device

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2013/0280858 A1
- Document ID: US20130280858A1
- Status: Published application
- Kind: A1
- Application number: 13/919,615
- Filed: 2013-06-17
- Published: 2013-10-24
- Earliest claimed: 2008-12-05
- Assignees: Semiconductor Energy Laboratory Co., Ltd.
- Applicants: Semiconductor Energy Laboratory Co., Ltd.
- Inventors: Hajime KIMURA
- Web page: https://patentgrep.com/patent/US20130280858A1

## CPC

- G02F 1/1368: in which the switching element is a three-electrode device {(G02F1/136277 takes precedence)}
- G02F 1/133345: {Insulating layers (G02F1/1335, G02F1/1337, G02F1/135, G02F1/136 take precedence)}
- G02F 1/133528: {Polarisers}
- G02F 1/13439: {characterised by their electrical, optical, physical properties; materials therefor; method of making}
- G02F 1/136277: {formed on a semiconductor substrate, e.g. of silicon}
- G02F 1/136286: {Wiring, e.g. gate line, drain line}
- H10D 30/6755: {Oxide semiconductors, e.g. zinc oxide, copper aluminium oxide or cadmium stannate}
- H10D 86/0231: {using masks, e.g. half-tone masks}
- H10D 86/423: {comprising semiconductor materials not belonging to the Group IV, e.g. InGaZnO}
- H10D 86/441: {Interconnections, e.g. scanning lines}
- H10D 86/481: {integrated with passive devices, e.g. auxiliary capacitors}
- H10D 86/60: wherein the TFTs are in active matrices
- H10D 99/00: Subject matter not provided for in other groups of this subclass
- G02F 2201/40: Arrangements for improving the aperture ratio
- G02F: OPTICAL DEVICES OR ARRANGEMENTS FOR THE CONTROL OF LIGHT BY MODIFICATION OF THE OPTICAL PROPERTIES OF THE MEDIA OF THE ELEMENTS INVOLVED THEREIN; NON-LINEAR OPTICS; FREQUENCY-CHANGING OF LIGHT; OPTICAL LOGIC ELEMENTS; OPTICAL ANALOGUE/DIGITAL CONVERTERS
- H10D: INORGANIC ELECTRIC SEMICONDUCTOR DEVICES

## Abstract

A semiconductor device includes an oxide semiconductor layer provided over a substrate having an insulating surface; a gate insulating film covering the oxide semiconductor layer; a first conductive layer and a second conductive layer laminated in this order over the gate insulating film; an insulating film covering the oxide semiconductor layer and a gate wiring including a gate electrode (the first and second conductive layers); and a third conductive layer and a fourth conductive layer laminated in this order over the insulating film and electrically connected to the oxide semiconductor layer. The gate electrode is formed using the first conductive layer. The gate wiring is formed using the first conductive layer and the second conductive layer. A source electrode is formed using the third conductive layer. A source wiring is formed using the third conductive layer and the fourth conductive layer.

## Claims

### Claim 1

A method for manufacturing a semiconductor device comprising the steps of:
forming an oxide semiconductor film over a substrate;
forming a silicon nitride film over the oxide semiconductor film;
forming a silicon oxide film over the silicon nitride film;
removing part of the silicon oxide film;
forming a conductive film having a light-transmitting property over the silicon oxide film;
forming a resist mask using a multi-tone mask over the oxide semiconductor film, and
ashing the resist mask to reduce the resist mask in size.

### Claim 2 (depends on 1)

The method for manufacturing the semiconductor device according to claim 1,
wherein the conductive film having a light-transmitting property is an indium tin oxide (ITO) film.

### Claim 3 (depends on 1)

The method for manufacturing the semiconductor device according to claim 1,
wherein the multi-tone mask is a half-tone mask.

### Claim 4 (depends on 1)

The method for manufacturing the semiconductor device according to claim 1,
wherein the ashing step is performed by using oxygen plasma.

### Claim 5 (depends on 1)

The method for manufacturing the semiconductor device according to claim 1,
wherein the oxide semiconductor film includes indium, gallium, and zinc.

### Claim 6 (depends on 1)

The method for manufacturing the semiconductor device according to claim 1,
wherein the semiconductor device comprises a capacitor portion including a second oxide semiconductor film formed by the same process as the oxide semiconductor film and a second conductive film having a light-transmitting property formed by the same process as the conductive film having a light-transmitting property.

### Claim 7

A method for manufacturing a semiconductor device comprising the steps of:
forming an oxide semiconductor film over a substrate;
forming a copper film over the oxide semiconductor film;
forming a resist mask using a multi-tone mask over the copper film;
etching the copper film using the resist mask to form a copper electrode;
ashing the resist mask to reduce the resist mask in size;
forming a first insulating film over the copper electrode;
forming a second insulating film over the first insulating film;
removing part of the second insulating film; and
forming a conductive film having a light-transmitting property over the second insulating film.

### Claim 8 (depends on 7)

The method for manufacturing the semiconductor device according to claim 7,
wherein the conductive film having a light-transmitting property is an indium tin oxide (ITO) film.

### Claim 9 (depends on 7)

The method for manufacturing the semiconductor device according to claim 7,
wherein the multi-tone mask is a half-tone mask.

### Claim 10 (depends on 7)

The method for manufacturing the semiconductor device according to claim 7,
wherein the ashing step is performed by using oxygen plasma.

### Claim 11 (depends on 7)

The method for manufacturing the semiconductor device according to claim 7,
wherein the oxide semiconductor film includes indium, gallium, and zinc.

### Claim 12 (depends on 7)

The method for manufacturing the semiconductor device according to claim 7,
wherein the semiconductor device comprises a capacitor portion including a second oxide semiconductor film formed by the same process as the oxide semiconductor film and a second conductive film having a light-transmitting property formed by the same process as the conductive film having a light-transmitting property.

### Claim 13

A method for manufacturing a semiconductor device comprising the steps of:
forming an oxide semiconductor film over a substrate;
forming a copper film over the oxide semiconductor film;
forming a resist mask using a multi-tone mask over the copper film;
etching the copper film using the resist mask to form a copper electrode;
ashing the resist mask to reduce the resist mask in size;
forming a silicon nitride film over the copper electrode;
forming an insulating film over the silicon nitride film;
removing part of the insulating film; and
forming a conductive film having a light-transmitting property over the insulating film.

### Claim 14 (depends on 13)

The method for manufacturing the semiconductor device according to claim 13,
wherein the conductive film having a light-transmitting property is an indium tin oxide (ITO) film.

### Claim 15 (depends on 13)

The method for manufacturing the semiconductor device according to claim 13,
wherein the multi-tone mask is a half-tone mask.

### Claim 16 (depends on 13)

The method for manufacturing the semiconductor device according to claim 13,
wherein the ashing step is performed by using oxygen plasma.

### Claim 17 (depends on 13)

The method for manufacturing the semiconductor device according to claim 13,
wherein the oxide semiconductor film includes indium, gallium, and zinc.

### Claim 18 (depends on 13)

The method for manufacturing the semiconductor device according to claim 13,
wherein the semiconductor device comprises a capacitor portion including a second oxide semiconductor film formed by the same process as the oxide semiconductor film and a second conductive film having a light-transmitting property formed by the same process as the conductive film having a light-transmitting property.