# US 2013/0280857 A1 · Manufacturing method of semiconductor device

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2013/0280857 A1
- Document ID: US20130280857A1
- Status: Published application
- Kind: A1
- Application number: 13/917,012
- Filed: 2013-06-13
- Published: 2013-10-24
- Earliest claimed: 2009-09-04
- Assignees: Semiconductor Energy Laboratory Co., Ltd.
- Applicants: Semiconductor Energy Laboratory Co., Ltd.
- Inventors: Masashi TSUBUKU; Shuhei YOSHITOMI; Takahiro TUJI; Miyuki HOSOBA; Junichiro SAKATA; Hiroyuki TOMATSU; Masahiko HAYAKAWA
- Web page: https://patentgrep.com/patent/US20130280857A1

## CPC

- H10D 86/0212: {comprising manufacture, treatment or coating of substrates}
- H10D 30/0316: {of lateral bottom-gate TFTs comprising only a single gate}
- H10D 30/0321: {comprising silicon, e.g. amorphous silicon or polysilicon}
- H10D 30/6755: {Oxide semiconductors, e.g. zinc oxide, copper aluminium oxide or cadmium stannate}
- H10D 86/0221: {comprising manufacture, treatment or patterning of TFT semiconductor bodies}
- H10D 86/451: {characterised by the compositions or shapes of the interlayer dielectrics}
- H10D 86/60: wherein the TFTs are in active matrices
- H10D 99/00: Subject matter not provided for in other groups of this subclass
- H10P 14/22: using physical deposition, e.g. vacuum deposition or sputtering
- H10P 14/3426: {Oxides}
- H10P 14/3434: {being oxide semiconductor materials (Group IIB-VIA semiconductor materials H10P14/3424)}
- H10P 14/3456: {Polycrystalline}
- H10P 14/3802: {Crystallisation or recrystallisation of non-monocrystalline semiconductor materials, e.g. regrowth}
- H10D: INORGANIC ELECTRIC SEMICONDUCTOR DEVICES
- H10P: GENERIC PROCESSES OR APPARATUS FOR THE MANUFACTURE OR TREATMENT OF DEVICES COVERED BY CLASS H10

## Abstract

It is an object to provide a manufacturing method of a structure of a thin film transistor including an oxide semiconductor film, in which threshold voltage at which a channel is formed is positive and as close to 0 V as possible. A protective insulating layer is formed to cover a thin film transistor including an oxide semiconductor layer that is dehydrated or dehydrogenated by first heat treatment, and second heat treatment at a temperature that is lower than that of the first heat treatment, in which the increase and decrease in temperature are repeated plural times, is performed, whereby a thin film transistor including an oxide semiconductor layer, in which threshold voltage at which a channel is formed is positive and as close to 0 V as possible without depending on the channel length, can be manufactured.

## Claims

### Claim 1

(canceled)

### Claim 2

A manufacturing method of a semiconductor device comprising the steps of:
forming a gate electrode layer over a substrate having an insulating surface;
forming a gate insulating layer over the gate electrode layer;
forming an oxide semiconductor layer over the gate insulating layer;
dehydrating or dehydrogenating the oxide semiconductor layer as a first treatment;
forming a source electrode layer and a drain electrode layer over the oxide semiconductor layer;
forming an insulating layer on the oxide semiconductor layer; and
performing a heat treatment as a second treatment, after forming the insulating layer,
wherein a thickness of the oxide semiconductor layer is greater than or equal to 5 nm and less than or equal to 200 nm, and
wherein a treatment temperature of the second treatment is lower than a treatment temperature of the first treatment.

### Claim 3 (depends on 2)

The manufacturing method of a semiconductor device according to claim 2,
wherein the step of dehydrating or dehydrogenating the oxide semiconductor layer is performed in a nitrogen atmosphere or a rare gas atmosphere.

### Claim 4 (depends on 2)

The manufacturing method of a semiconductor device according to claim 2,
wherein a temperature of the step of dehydrating or dehydrogenating the oxide semiconductor layer is higher than or equal to 350° C. and lower than or equal to 750° C.

### Claim 5 (depends on 2)

The manufacturing method of a semiconductor device according to claim 2,
wherein the insulating layer is a protective insulating layer.

### Claim 6 (depends on 2)

The manufacturing method of a semiconductor device according to claim 2,
wherein the insulating layer is one of silicon oxide layer, a silicon nitride oxide layer, a silicon nitride layer, an aluminum oxide layer, an aluminum oxynitride layer, and an aluminum nitride layer.

### Claim 7 (depends on 2)

The manufacturing method of a semiconductor device according to claim 2,
wherein the insulating layer contains silicon and nitride.

### Claim 8 (depends on 2)

The manufacturing method of a semiconductor device according to claim 2,
wherein a temperature of the heat treatment is higher than or equal to 100° C. and lower than or equal to 300° C.

### Claim 9

A manufacturing method of a semiconductor device comprising the steps of:
forming a gate electrode layer over a substrate having an insulating surface;
forming a gate insulating layer over the gate electrode layer;
forming an oxide semiconductor layer over the gate insulating layer;
dehydrating or dehydrogenating the oxide semiconductor layer as a first treatment;
forming a source electrode layer and a drain electrode layer over the oxide semiconductor layer;
forming an insulating layer on the oxide semiconductor layer; and
performing a heat treatment as a second treatment, after forming the insulating layer,
wherein a thickness of the oxide semiconductor layer is greater than or equal to 5 nm and less than or equal to 200 nm,
wherein a treatment temperature of the second treatment is lower than a treatment temperature of the first treatment,
wherein the oxide semiconductor layer contains indium, gallium and zinc,
wherein the gate insulating layer is a stacked-layer structure of a first layer containing silicon and nitrogen and a second layer containing silicon and oxygen, and
wherein the insulating layer is a stacked-layer structure of a third layer containing silicon and oxygen and a fourth layer containing silicon and nitrogen over the third layer.

### Claim 10 (depends on 9)

The manufacturing method of a semiconductor device according to claim 9,
wherein the step of dehydrating or dehydrogenating the oxide semiconductor layer is performed in a nitrogen atmosphere or a rare gas atmosphere.

### Claim 11 (depends on 9)

The manufacturing method of a semiconductor device according to claims 9,
wherein a temperature of the step of dehydrating or dehydrogenating the oxide semiconductor layer is higher than or equal to 350° C. and lower than or equal to 750° C.

### Claim 12 (depends on 9)

The manufacturing method of a semiconductor device according to claim 9,
wherein the insulating layer is a protective insulating layer.

### Claim 13 (depends on 9)

The manufacturing method of a semiconductor device according to claim 9,
wherein the insulating layer is one of silicon oxide layer, a silicon nitride oxide layer, a silicon nitride layer, an aluminum oxide layer, an aluminum oxynitride layer, and an aluminum nitride layer.

### Claim 14 (depends on 9)

The manufacturing method of a semiconductor device according to claim 9,
wherein the insulating layer contains silicon and nitride.

### Claim 15 (depends on 9)

The manufacturing method of a semiconductor device according to claim 9,
wherein a temperature of the heat treatment is higher than or equal to 100° C. and lower than or equal to 300° C.