# US 2013/0280601 A1 · Preparation of polymeric resins and carbon materials

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2013/0280601 A1
- Document ID: US20130280601A1
- Status: Published application
- Kind: A1
- Application number: 13/763,448
- Filed: 2013-02-08
- Published: 2013-10-24
- Earliest claimed: 2012-02-09
- Assignees: EnerG2 Technologies, Inc.
- Applicants: EnerG2 Technologies, Inc.
- Inventors: Katharine Geramita; Benjamin Kron; Henry R. Costantino; Aaron M. Feaver; Avery J. Sakshaug; Leah A. Thompkins; Alan Tzu-Yang Chang
- Web page: https://patentgrep.com/patent/US20130280601A1

## CPC

- C08G 8/22: Resorcinol
- C01B 32/05: Preparation or purification of carbon not covered by groups C01B32/15, C01B32/20, C01B32/25, C01B32/30
- C01B 32/30: Active carbon
- C01B 32/312: Preparation
- C01B 32/336: characterised by gaseous activating agents
- H01G 11/34: characterised by carbonisation or activation of carbon
- H01G 11/44: Raw materials therefor, e.g. resins or coal
- H01M 4/133: Electrodes based on carbonaceous material, e.g. graphite-intercalation compounds or CFx
- H01M 4/14: Electrodes for lead-acid accumulators
- H01M 4/36: Selection of substances as active materials, active masses, active liquids
- H01M 4/587: for inserting or intercalating light metals
- H01M 4/96: Carbon-based electrodes
- H01M 10/0525: Rocking-chair batteries, i.e. batteries with lithium insertion or intercalation in both electrodes; Lithium-ion batteries
- H01M 10/054: Accumulators with insertion or intercalation of metals other than lithium, e.g. with magnesium or aluminium
- H01M 12/08: composed of a half-cell of a fuel-cell type and a half-cell of the secondary-cell type
- H01M 4/625: {Carbon or graphite}
- H01M 10/06: Lead-acid accumulators (semi-lead accumulators H01M10/20)
- H01M 12/06: with one metallic and one gaseous electrode
- Y02E 60/10: Energy storage using batteries
- Y02E 60/13: Energy storage using capacitors
- C08G: MACROMOLECULAR COMPOUNDS OBTAINED OTHERWISE THAN BY REACTIONS ONLY INVOLVING UNSATURATED CARBON-TO-CARBON BONDS
- C01B: NON-METALLIC ELEMENTS; COMPOUNDS THEREOF; {METALLOIDS OR COMPOUNDS THEREOF NOT COVERED BY SUBCLASS C01C}
- H01G: CAPACITORS; CAPACITORS, RECTIFIERS, DETECTORS, SWITCHING DEVICES, LIGHT-SENSITIVE OR TEMPERATURE-SENSITIVE DEVICES OF THE ELECTROLYTIC TYPE (selection of specified materials as dielectric H01B3/00; capacitors having potential barriers H10D1/62, H10K10/10)
- H01M: PROCESSES OR MEANS, e.g. BATTERIES, FOR THE DIRECT CONVERSION OF CHEMICAL ENERGY INTO ELECTRICAL ENERGY
- Y02E: REDUCTION OF GREENHOUSE GAS [GHG] EMISSIONS, RELATED TO ENERGY GENERATION, TRANSMISSION OR DISTRIBUTION

## Abstract

The present application is directed to methods for preparation of carbon materials. The carbon materials comprise enhanced electrochemical properties and find utility in any number of electrical devices, for example, as electrode material in ultracapacitors or batteries.

## Claims

### Claim 1

A method for making polymer particles in gel form via an emulsion or suspension process, the method comprising:
a) preparing a reactant mixture comprising a monomer component comprising one or more phenolic compounds, one or more crosslinking compounds, and a carrier fluid; and
b) polymerizing the one or more phenolic compounds with the one or more crosslinking compounds,
wherein the carrier fluid comprises a surfactant in a concentration equal to or greater than the critical micelle concentration and the volume average particle size (Dv,50) of the polymer particles is less than or equal to 1 mm.

### Claim 2

A method for making polymer particles in gel form via an emulsion or suspension process, the method comprising:
a) preparing a reactant mixture comprising a monomer component comprising one or more phenolic compounds, one or more crosslinking compounds, and a carrier fluid; and
b) polymerizing the one or more phenolic compounds with the one or more crosslinking compounds,
wherein the carrier fluid comprises 50 wt % or more of cyclohexane, based on the total weight of the carrier fluid, and the volume average particle size (Dv,50) of the polymer particles is less than or equal to 1 mm.

### Claim 3

A method for making polymer particles in gel form via an emulsion or suspension process, the method comprising:
a) preparing a reactant mixture comprising a monomer component comprising one or more phenolic compounds, one or more crosslinking compounds, and a carrier fluid; and
b) polymerizing the one or more phenolic compounds with the one or more crosslinking compounds,
wherein the carrier fluid comprises a surfactant in a concentration equal to or greater than the critical micelle concentration and 50 wt % or more of cyclohexane, based on the total weight of the carrier fluid, and the volume average particle size (Dv,50) of the polymer particles is greater than or equal to 1 mm.

### Claim 4 (depends on 1)

The method according to claim 1, wherein the Dv,50 of the polymer particles is less than or equal to 0.5 mm.

### Claim 5 (depends on 1)

The method according to claim 1, wherein the Dv,50 of the polymer particles is less than or equal to 0.1 mm.

### Claim 6

(canceled)

### Claim 7 (depends on 3)

The method according to claim 3, wherein the Dv,50 of the polymer greater than or equal to 4 mm.

### Claim 8 (depends on 1)

The method according to claim 1, wherein the carrier fluid comprises one or more vegetable oils, one or more minerals oils having from about 15 to about 40 carbon atoms, one or more chlorinated hydrocarbons, one or more paraffinic oils, or any combination thereof.

### Claim 9 (depends on 1)

The method according to claim 1, wherein the monomer component is an aqueous mixture comprising the one or more phenolic compounds and one or more catalysts.

### Claim 10 (depends on 9)

The method according to claim 9, wherein the one or more catalysts comprises an organic acid.

### Claim 11 (depends on 9)

The method according to claim 9, wherein the one or more catalysts comprises a volatile basic salt.

### Claim 12 (depends on 9)

The method according to claim 9, wherein the one or more catalysts comprises a volatile basic salt and comprises an organic acid.

### Claim 13 (depends on 1)

The method according to claim 1, wherein the volatile basic salt is ammonium carbonate, ammonium bicarbonate, ammonium acetate, or ammonium hydroxide, or a combination thereof.

### Claim 14 (depends on 11)

The method according to claim 11, wherein the organic acid is acetic acid, formic acid, propionic acid, maleic acid, oxalic acid, uric acid, lactic acid, or a combination thereof.

### Claim 15 (depends on 9)

The method according to claim 9, wherein the one or more catalysts contains a total of less than 500 ppm halogens, arsenic, antimony, bismuth, or ions thereof.

### Claim 16 (depends on 9)

The method according to claim 9, wherein a molar ratio of the one or more phenolic compounds to the one or more catalysts ranges from about 5 to about 400.

### Claim 17 (depends on 9)

The method according to claim 9, wherein a molar ratio of the one or more phenolic compounds to the one or more catalysts ranges from about 5 to about 50.

### Claim 18 (depends on 1)

The method according to claim 1, wherein the polymer particles in gel form are made via the suspension process, the reactant mixture is a suspension and the method further comprises agitation of the suspension with a mixer.

### Claim 19 (depends on 1)

The method according to claim 1, further comprising separating the polymer particles from the carrier fluid to provide separated polymer particles in gel form.

### Claim 20 (depends on 1)

The method according to claim 1, further comprising heating the reactant mixture to a temperature ranging from about 30° C. to about 100° C.

### Claim 21 (depends on 1)

The method according to claim 1, wherein the reactant mixture has a pH of less than 7 during polymerization.

### Claim 22 (depends on 1)

The method according to claim 1, wherein the reactant mixture has a pH of less than 5 during polymerization.

### Claim 23 (depends on 1)

The method according to claim 1, wherein the reactant mixture has a pH of less than 4 during polymerization.

### Claim 24 (depends on 1)

The method according to claim 1, wherein the reactant mixture is at a temperature of about 80° C. or more during polymerization of the reactant mixture.

### Claim 25 (depends on 1)

The method according to claim 1, wherein the reactant mixture is at a temperature ranging from about 80° C. to about 150° C. during polymerization of the monomer component.

### Claim 26 (depends on 1)

The method according to claim 1, wherein the one or more phenolic compounds and the one or more crosslinking compounds are prepolymerized with one another to form a prepolymer prior to making the polymer particles in gel form via the emulsion or suspension process.

### Claim 27 (depends on 1)

The method according to claim 1, further comprising admixing a silicon-containing electrochemical modifier with the polymer precursor mixture, the polymer phase or the continuous phase.

### Claim 28 (depends on 1)

The method according to claim 1, further comprising admixing a nitrogen-containing electrochemical modifier with the polymer precursor mixture, the polymer phase or the continuous phase.

### Claim 29 (depends on 28)

The method according to claim 28, wherein the nitrogen-containing electrochemical modifier is urea, melamine, or combination thereof.

### Claim 30 (depends on 1)

The method of claim 1, wherein the surfactant is a non-ionic surfactant having molecular weight of from about 100 Daltons to about 2,000 Daltons, and the critical micelle concentration ranges from 0.01% to 20%.

### Claim 31 (depends on 1)

The method according to claim 1, wherein the reactant mixture is aged for 12 hours or less at a temperature between about 45 and 70 C.

### Claim 32 (depends on 1)

The method according to claim 1, wherein the reactant mixture is aged for 6 hours or less at a temperature between about 45 and 70 C.

### Claim 33 (depends on 1)

The method according to claim 1, wherein the polymer gel particles comprise a total pore volume of between about 0.01 and 1.5 cm3/g.

### Claim 34 (depends on 1)

The method according to claim 1, wherein the polymer gel particles comprise a total pore volume of between about 0.1 and 0.9 cm3/g.

### Claim 35 (depends on 1)

The method according to claim 1, further comprising pyrolyzing the polymer gel particles by a method comprising heating the polymer gel particles in an inert atmosphere at temperatures ranging from 500° C. to 2400° C.

### Claim 36 (depends on 35)

The method according to claim 35, wherein the pyrolyzed polymer gel particles have a total pore volume greater than 0.8 cm3/g and a gerameter (GM) between 9 and 21.

### Claim 37 (depends on 1)

The method according to claim 1, further comprising:
a) pyrolyzing the polymer gel particles by a method comprising heating the condensation polymer gel particles in an inert atmosphere at temperatures ranging from 500° C. to 2400° C., and
b) activating the pyrolzyed polymer gel particles in an atmosphere comprising carbon dioxide, carbon monoxide, steam, oxygen or combinations thereof at a temperature may ranging from 800° C. to 1300° C.

### Claim 38 (depends on 37)

The method according to claim 37, wherein the pyrolyzed and activated polymer gel particles have a total pore volume greater than 0.6 cm3/g and a gerameter (GM) greater than or equal to 21.

### Claim 39 (depends on 38)

The method according to claim 38, wherein the pyrolyzed and activated polymer gel particles have a total pore volume greater than 1 cm3/g and a gerameter (GM) ranging from 9 to 21.

### Claim 40

A polymer gel having a particle size distribution such that Dv,50 is less than about 1 mm and (Dv,90-Dv,10)/Dv,50 is less than 3, wherein Dv,10, Dv,50 and Dv,90 are the particle size at 10%, 50% and 90%, respectively of the particle size distribution by volume.

### Claim 41

A polymer gel having a particle size distribution such that Dv,50 is less than about 0.5 mm and (Dv,90-Dv,10)/Dv,50 is less than 3, wherein Dv,10, Dv,50 and Dv,90 are the particle size at 10%, 50% and 90%, respectively of the particle size distribution by volume.

### Claim 42

(canceled)

### Claim 43 (depends on 40)

The polymer gel according to claim 40, wherein (Dv,90-Dv,10)/Dv,50 is less than 2.

### Claim 44

(canceled)

### Claim 45

A carbon material, wherein the maximum theoretical capacitance of the carbon material is greater than 25 F/cm3 as measured at a current density of 0.5 Amp/g employing an electrolyte comprising tetraethylammonium tetrafluoroborane in acetonitrile, and wherein the carbon material comprises less than 500 ppm of all atoms having a molecular weight between 11 and 92 as measured by photon induced x-ray emissions.

### Claim 46 (depends on 35)

An electrode comprising a carbon material produced according to claims 35.

### Claim 47 (depends on 35)

An electrical energy storage device comprising a carbon material produced according to claim 35.

### Claim 48 (depends on 47)

The electrical energy storage device of claim 47, wherein the electrical energy storage device is a double layer ultracapacitor, a lithium/carbon battery, a zinc/carbon battery, a lithium air battery or a lead acid battery.

### Claim 49

(canceled)

### Claim 50

An electrode comprising carbon, wherein the carbon comprises a maximum theoretical capacitance of greater than 25 F/cm3 and wherein the electrode retains greater than 90% of its capacitance after incubation at 2.85 V and 85 C for 32 h, wherein the capacitance is measured at a current density of 0.5 Amp/g employing an electrolyte comprising tetraethylammonium tetrafluoroborane in acetonitrile.

### Claim 51

An electrode comprising carbon, wherein the carbon comprises a maximum theoretical capacitance of greater than 20 F/cm3, wherein the capacitance is measured after incubation at 2.85 V and 85 C for 32 h, and at a current density of 0.5 Amp/g employing an electrolyte comprising tetraethylammonium tetrafluoroborane in acetonitrile.

### Claim 52

(canceled)

### Claim 53 (depends on 50)

An electrical energy storage device comprising the electrode according to claim 50.

### Claim 54

(canceled)

### Claim 55 (depends on 3)

The method according to claim 3, wherein the Dv,50 of the polymer is less than or equal to 5 mm.