# US 2013/0280495 A1 · Glass film cutting method and glass film laminate

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2013/0280495 A1
- Document ID: US20130280495A1
- Status: Published application
- Kind: A1
- Application number: 13/856,125
- Filed: 2013-04-03
- Published: 2013-10-24
- Earliest claimed: 2012-04-05
- Assignees: Nippon Electric Glass Co., Ltd.
- Applicants: Nippon Electric Glass Co., Ltd.
- Inventors: Yasuhiro MATSUMOTO
- Web page: https://patentgrep.com/patent/US20130280495A1

## CPC

- C03B 33/091: {using at least one focussed radiation beam, e.g. laser beam (C03B33/0955 takes precedence)}
- B32B 17/06: comprising glass as the main or only constituent of a layer, next to another layer of a specific {material}
- C03B 33/033: Apparatus for opening score lines in glass sheets
- C03B 33/076: {Laminated glass comprising interlayers}
- Y10T 428/24612: Composite web or sheet
- Y10T 428/2495: Thickness [relative or absolute]
- C03B: MANUFACTURE, SHAPING, OR SUPPLEMENTARY PROCESSES
- B32B: LAYERED PRODUCTS, i.e. PRODUCTS BUILT-UP OF STRATA OF FLAT OR NON-FLAT, e.g. CELLULAR OR HONEYCOMB, FORM
- Y10T: TECHNICAL SUBJECTS COVERED BY FORMER US CLASSIFICATION

## Abstract

A glass film laminate is manufactured by setting a surface roughness Ra of a surface of a glass film having a thickness of 200 μm or less to contact a support glass, which supports the glass film, and a surface of the support glass to contact the glass film to 2.0 nm or less, and by bringing the surfaces of the glass film and the support glass into surface contact with each other. After that, a laser scribing operation is carried out, in which a scribe line is formed in the glass film by propagating an initial crack through laser heating of the glass film followed by subsequent cooling of the glass film.

## Claims

### Claim 1

A glass film cutting method, comprising:
a laser scribing step of forming a scribe line in a glass film having a thickness of 200 μm or less by propagating an initial crack through laser heating of the glass film followed by subsequent cooling of the glass film; and
a laminate manufacturing step of manufacturing a glass film laminate by setting a surface roughness Ra of each of a surface of the glass film to be brought into contact with a support glass, which is configured to support the glass film, and a surface of the support glass to be brought into contact with the glass film to 2.0 nm or less, and by bringing the surface of the glass film and the surface of the support glass into surface contact with each other, followed by the laser scribing step.

### Claim 2 (depends on 1)

The glass film cutting method according to claim 1, further comprising:
a separation step of separating, from the support glass, the glass film having the scribe line formed therein; and
a snapping step of snapping the separated glass film along the scribe line,
the separation step and the snapping step following the laser scribing step.

### Claim 3 (depends on 1)

The glass film cutting method according to claim 1, wherein the laser scribing step comprises forming a plurality of scribe lines crossing each other.

### Claim 4 (depends on 1)

The glass film cutting method according to claim 1, wherein the support glass of the glass film laminate comprises support glasses arranged so as to extend along preset cleaving lines, along which the scribe lines are to be formed in the glass film.

### Claim 5 (depends on 1)

The glass film cutting method according to claim 1, wherein the support glass of the glass film laminate is thinner than the glass film.

### Claim 6

A glass film laminate, comprising:
a glass film having a thickness of 200 μm or less; and
a support glass, which is configured to support the glass film,
wherein a surface of the glass film to be brought into contact with the support glass has a surface roughness Ra of 2.0 nm or less, and a surface of the support glass to be brought into contact with the glass film has a surface roughness Ra of 2.0 nm or less,
wherein the surface of the glass film and the surface of the support glass are brought into surface contact with each other to laminate the glass film and the support glass,
wherein the glass film comprises a scribe line formed therein by propagating an initial crack through laser heating of the glass film followed by subsequent cooling of the glass film, and
wherein the support glass is thinner than the glass film.

### Claim 7

A glass film laminate, comprising:
a glass film having a thickness of 200 μm or less; and
a support glass, which is configured to support the glass film,
wherein a surface of the glass film to be brought into contact with the support glass has a surface roughness Ra of 2.0 nm or less, and a surface of the support glass to be brought into contact with the glass film has a surface roughness Ra of 2.0 nm or less,
wherein the surface of the glass film and the surface of the support glass are brought into surface contact with each other to laminate the glass film and the support glass, and
wherein the support glass is thinner than the glass film.

### Claim 8 (depends on 2)

The glass film cutting method according to claim 2, wherein the laser scribing step comprises forming a plurality of scribe lines crossing each other.

### Claim 9 (depends on 2)

The glass film cutting method according to claim 2, wherein the support glass of the glass film laminate comprises support glasses arranged so as to extend along preset cleaving lines, along which the scribe lines are to be formed in the glass film.

### Claim 10 (depends on 3)

The glass film cutting method according to claim 3, wherein the support glass of the glass film laminate comprises support glasses arranged so as to extend along preset cleaving lines, along which the scribe lines are to be formed in the glass film.

### Claim 11 (depends on 8)

The glass film cutting method according to claim 8, wherein the support glass of the glass film laminate comprises support glasses arranged so as to extend along preset cleaving lines, along which the scribe lines are to be formed in the glass film.

### Claim 12 (depends on 2)

The glass film cutting method according to claim 2, wherein the support glass of the glass film laminate is thinner than the glass film.

### Claim 13 (depends on 3)

The glass film cutting method according to claim 3, wherein the support glass of the glass film laminate is thinner than the glass film.

### Claim 14 (depends on 4)

The glass film cutting method according to claim 4, wherein the support glass of the glass film laminate is thinner than the glass film.

### Claim 15 (depends on 8)

The glass film cutting method according to claim 8, wherein the support glass of the glass film laminate is thinner than the glass film.

### Claim 16 (depends on 9)

The glass film cutting method according to claim 9, wherein the support glass of the glass film laminate is thinner than the glass film.

### Claim 17 (depends on 10)

The glass film cutting method according to claim 10, wherein the support glass of the glass film laminate is thinner than the glass film.

### Claim 18 (depends on 11)

The glass film cutting method according to claim 11, wherein the support glass of the glass film laminate is thinner than the glass film.