# US 2013/0280438 A1 · Method for producing polarizing film, and liquid crystal display device

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2013/0280438 A1
- Document ID: US20130280438A1
- Status: Published application
- Kind: A1
- Application number: 13/926,549
- Filed: 2013-06-25
- Published: 2013-10-24
- Earliest claimed: 2006-04-27
- Assignees: Nitto Denko Corporation
- Applicants: Nitto Denko Corporation
- Inventors: Yasuko Iwakawa; Shuusaku Nakano; Tetsuo Inoue; Shouichi Matsuda
- Web page: https://patentgrep.com/patent/US20130280438A1

## CPC

- G02B 5/3033: {in the form of a thin sheet or foil, e.g. Polaroid}
- G02F 1/133528: {Polarisers}
- G02B: OPTICAL ELEMENTS, SYSTEMS OR APPARATUS
- G02F: OPTICAL DEVICES OR ARRANGEMENTS FOR THE CONTROL OF LIGHT BY MODIFICATION OF THE OPTICAL PROPERTIES OF THE MEDIA OF THE ELEMENTS INVOLVED THEREIN; NON-LINEAR OPTICS; FREQUENCY-CHANGING OF LIGHT; OPTICAL LOGIC ELEMENTS; OPTICAL ANALOGUE/DIGITAL CONVERTERS

## Abstract

A method for producing a polarizing film includes a step (1) of preparing a lyotropic liquid crystalline solution having electric conductivity of not more than 50 μS/cm (expressed in terms of 0.05% by weight) and containing a dichroic dye and a solvent, a step (2) of preparing a base material having at least one surface subjected to a hydrophilization treatment, and a step (3) of coating the solution prepared in the step (1) on the hydrophilized surface of the base material prepared in the step (2) at a coating rate of not less than 100 mm/second, and drying the solution. The polarizing film produced in the method has a dichroic ratio of 25 or more at a wavelength of 600 nm.

## Claims

### Claim 1

A method for producing a polarizing film having a dichroic ratio of 25 or more at a wavelength of 600 nm, comprising the following steps (1) to (3-2):
(1) a step of preparing a lyotropic liquid crystalline solution having electric conductivity of not more than 50 μS/cm (expressed in terms of 0.05% by weight) and containing a dichroic dye and a solvent;
(2) a step of preparing a base material having at least one surface subjected to a hydrophilization treatment;
thereby achieving a reduction of contact angle of water to the hydrophilization treated surface of the base material of 10° to 60° at 23° C.;
(3-1) a step of forming a coating layer by coating solution prepared in the step (1) on a hydrophilized surface of the base material prepared in the step (2) at a coating rate of not less than 100 mm/second; and
(3-2) a step of evaporating the solvent in the coating layer formed in the step (3-1) until the dichroic dye is fixed in an oriented state.

### Claim 2 (depends on 1)

The method for producing a polarizing film according to claim 1, wherein the lyotropic liquid crystalline solution of the step (1) contains sulfuric acid ions, and the step (I) comprises a treatment of decreasing the sulfuric acid ions from the solution by using a reverse osmosis membrane.

### Claim 3 (depends on 1)

The method for producing a polarizing film according to claim 1, wherein the dichroic dye is either an organic compound having a sulfone group, a carboxyl group or an amino group, or a salt thereof.

### Claim 4 (depends on 1)

The method for producing a polarizing film according to claim 1, wherein the solvent is water.

### Claim 5 (depends on 4)

The method for producing a polarizing film according to claim 4, wherein electric conductivity of the water is not more than 20 μS/cm.

### Claim 6 (depends on 1)

The method for producing a polarizing film according to claim 1, wherein a concentration of the dichroic dye in the solution is from 5% by weight to 40% by weight.

### Claim 7 (depends on 1)

The method for producing a polarizing film according to claim 1, wherein the hydrophilization treatment is a treatment of adjusting a contact angle of water to the base material within a range from 20% to 60° at 23° C.

### Claim 8 (depends on 1)

The method for producing a polarizing film according to claim 1, wherein the hydrophilization treatment is a corona treatment, a plasma treatment, an alkali treatment, or an anchor coat treatment.

### Claim 9 (depends on 1)

The method for producing a polarizing film according to claim 1, wherein base material is a glass base material or a polymer film.

### Claim 10 (depends on 9)

The method for producing a polarizing film according to claim 9, wherein the polymer film contains a cellulose-based resin.

### Claim 11 (depends on 1)

The method for producing a polarizing film according to claim 1, wherein the dichroic dye is an organic compound having a sulfone group and the solvent is water.

### Claim 12 (depends on 1)

The method for producing a polarizing film according to claim 1, wherein the dichroic dye is represented by (Chromogen) (SO3M)n, wherein M represents a cation.

### Claim 13 (depends on 1)

The method for producing a polarizing film according to claim 1, wherein the coating rate is 1000 mm/second to 4000 mm/second.

### Claim 14 (depends on 1)

The method for producing a polarizing film according to claim 1, further comprising (4) a step of contacting a solution containing a compound salt to the coating layer dried in the step (3-2).

### Claim 15 (depends on 14)

The method for producing a polarizing film according to claim 14, wherein the concentration of the compound salt in the solution containing a compound salt is 3 to 40% by weight.