# US 2013/0280432 A1 · Formaldehyde-free flame retardant compositions and their use for manufacturing durable formaldehyde-free flame retardant cellulosic materials

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2013/0280432 A1
- Document ID: US20130280432A1
- Status: Published application
- Kind: A1
- Application number: 13/801,181
- Filed: 2013-03-13
- Published: 2013-10-24
- Earliest claimed: 2012-04-24
- Assignees: Winnitex Limited
- Applicants: Winnitex Limited
- Inventors: James R. Johnson; Kenneth Y.M. Chan; Charles Wang
- Web page: https://patentgrep.com/patent/US20130280432A1

## CPC

- B05D 5/00: Processes for applying liquids or other fluent materials to surfaces to obtain special surface effects, finishes or structures
- C09K 21/04: containing phosphorus
- C09K 21/12: containing phosphorus
- D06M 11/71: Salts of phosphoric acids
- D06M 11/72: with metaphosphoric acids or their salts; with polyphosphoric acids or their salts; with perphosphoric acids or their salts
- D06M 15/673: containing phosphorus and nitrogen in the main chain
- D06M 2101/06: cellulosic
- D06M 2200/30: Flame or heat resistance, fire retardancy properties
- B05D: PROCESSES FOR APPLYING FLUENT MATERIALS TO SURFACES, IN GENERAL (conveying articles or workpieces through baths of liquid B65G, e.g. B65G49/02)
- C09K: MATERIALS FOR MISCELLANEOUS APPLICATIONS, NOT PROVIDED FOR ELSEWHERE
- D06M: TREATMENT, NOT PROVIDED FOR ELSEWHERE IN CLASS D06, OF FIBRES, THREADS, YARNS, FABRICS, FEATHERS OR FIBROUS GOODS MADE FROM SUCH MATERIALS

## Abstract

Provided herein are formaldehyde-free flame retardant compositions, comprising a flame retardant acid and a fixing agent; and methods of their use for manufacturing durable formaldehyde-free flame retardant cellulosic materials. Also provided herein are durable formaldehyde-free flame retardant cellulosic materials and articles comprising the same.

## Claims

### Claim 1

A method for preparing a durable formaldehyde-free flame retardant cellulosic material, comprising curing a cellulosic material in the presence of a formaldehyde-free flame retardant composition comprising an ammonium salt of a phosphorus containing acid and a fixing reagent.

### Claim 2 (depends on 1)

The method of claim 1, wherein the phosphorus containing acid is a phosphoric acid, a phosphonic acid, or a mixture thereof.

### Claim 3 (depends on 1)

The method of claim 1, wherein the ammonium salt of the phosphorus containing acid is diammonium orthophosphate, an ammonium polyphosphate, ammonium methyl phosphonate, ammonium phenyl phosphonate, ammonium aminotrimethylene phosphonate, or a mixture thereof.

### Claim 4 (depends on 1)

The method of claim 1, wherein the phosphorus containing acid is orthophosphoric acid, a polyphosphoric acid, or mixture thereof.

### Claim 5 (depends on 1)

The method of claim 1, wherein the flame retardant acid is orthophosphoric acid.

### Claim 6 (depends on 1)

The method of claim 1, wherein the phosphorus containing acid is a polyphosphoric acid.

### Claim 7 (depends on 1)

The method of claim 1, wherein the ammonium salt of the phosphorus containing acid is diammonium orthophosphate.

### Claim 8 (depends on 1)

The method of claim 1, wherein the is an ammonium polyphosphate.

### Claim 9 (depends on 1)

The method of claim 1, wherein the formaldehyde-free flame retardant composition has a formaldehyde content of no greater than 50 ppm.

### Claim 10 (depends on 1)

The method of claim 1, wherein the formaldehyde-free flame retardant composition comprises from about 5% to about 50% by weight of the ammonium salt of the phosphorus containing acid.

### Claim 11 (depends on 1)

The method of claim 1, wherein the fixing agent is urea, dicyandiamide, cyanamide, or a mixture thereof.

### Claim 12 (depends on 1)

The method of claim 1, wherein the fixing agent is urea.

### Claim 13 (depends on 1)

The method of claim 1, wherein the formaldehyde-free flame retardant composition comprises from about 5% to about 50% by weight of the fixing agent.

### Claim 14 (depends on 1)

The method of claim 1, wherein the molar ratio of the fixing agent to the ammonium salt of the phosphorus containing acid is ranging from about 1 to about 10.

### Claim 15 (depends on 1)

The method of claim 1, wherein the molar ratio of the fixing agent to the ammonium salt of the flame-retardant acid is no less than about 1.2.

### Claim 16 (depends on 1)

The method of claim 1, wherein the composition comprises from about 5% to about 50% by weight of diammonium orthophosphate and from about 5% to about 50% by weight of urea.

### Claim 17 (depends on 1)

The method of claim 1, wherein the composition comprises from about 5% to about 50% by weight of an ammonium polyphosphate and from about 5% to about 50% by weight of urea.

### Claim 18 (depends on 1)

The method of claim 1, wherein the curing step is performed at a temperature ranging from about 130 to about 200° C.

### Claim 19 (depends on 1)

The method of claim 1, wherein the cellulosic material is treated during the curing step with heat in the amount ranging from about 3000 to about 20,000° C.-seconds above 130° C.

### Claim 20 (depends on 1)

The method of claim 1, wherein the cellulosic material is treated during the curing step with heat in the amount ranging from about 4000 to about 10,000° C.-seconds above 130° C.

### Claim 21 (depends on 1)

The method of claim 1, wherein the curing step is performed at an absolute humidity of no greater than about 20%.

### Claim 22 (depends on 1)

The method of claim 1, wherein the cellulosic material comprises cotton, flax, jute, hemp, ramie, lyocell, rayon, or a combination thereof.

### Claim 23 (depends on 1)

The method of claim 1, wherein the cellulosic material comprises cotton.

### Claim 24 (depends on 1)

The method of claim 1, wherein the cellulosic material is a cotton blend.

### Claim 25

A method for preparing a durable formaldehyde-free flame retardant cellulosic material, comprising the steps of:
a) contacting a cellulosic material with a formaldehyde-free flame retardant composition to form a wet cellulosic material; wherein the formaldehyde-free flame retardant composition comprises an ammonium salt of a phosphorus containing acid and a fixing agent;
b) drying the wet cellulosic material; and
c) curing the cellulosic material to form the durable formaldehyde-free flame retardant cellulosic material.

### Claim 26 (depends on 26)

The method of claim 26, wherein the drying step is performed at a temperature ranging from about 50 to about 150° C.

### Claim 27 (depends on 26)

The method of claim 26, wherein the curing step is performed at a temperature ranging from about 130 to about 200° C.

### Claim 28 (depends on 26)

The method of claim 26, wherein the cellulosic material is treated during the curing step with heat in the amount ranging from about 3000 to about 20,000° C.-seconds above 130° C.

### Claim 29 (depends on 26)

The method of claim 26, wherein the curing step is performed at an absolute humidity of no greater than about 10%.

### Claim 30 (depends on 26)

The method of claim 26, wherein the cellulosic material comprises cotton, flax, jute, hemp, ramie, lyocell, rayon, or a combination thereof.