# US 2013/0280122 A1 · Aluminum alloy sheet that exhibits excellent surface quality after anodizing and method for producing the same

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2013/0280122 A1
- Document ID: US20130280122A1
- Status: Published application
- Kind: A1
- Application number: 13/864,777
- Filed: 2013-04-17
- Published: 2013-10-24
- Earliest claimed: 2012-04-20
- Assignees: Sumitomo Light Metal Industries, Ltd.
- Inventors: Mineo ASANO; Yusuke YAMAMOTO
- Web page: https://patentgrep.com/patent/US20130280122A1

## CPC

- C22C 21/08: with silicon
- B21B 1/26: by hot-rolling {, e.g. Steckel hot mill}
- C22C 21/00: Alloys based on aluminium
- C22C 21/06: with magnesium as the next major constituent
- C22C 21/14: with silicon
- C22C 21/16: with magnesium
- C22F 1/047: of alloys with magnesium as the next major constituent
- C22F 1/057: of alloys with copper as the next major constituent
- C25D 11/04: of aluminium or alloys based thereon
- C22C: ALLOYS (treatment of alloys C21D, C22F)
- B21B: ROLLING OF METAL (auxiliary operations used in connection with metal-working operations covered in B21, see B21C; bending by rolling B21D; manufacture of particular objects, e.g. screws, wheels, rings, barrels, balls, by rolling B21H; pressure welding by means of a rolling mill B23K20/04)
- C22F: CHANGING THE PHYSICAL STRUCTURE OF NON-FERROUS METALS AND NON-FERROUS ALLOYS (surface treatment of metallic material involving at least one process provided for in class C23 and at least one process covered by this subclass, C23F17/00)
- C25D: PROCESSES FOR THE ELECTROLYTIC OR ELECTROPHORETIC PRODUCTION OF COATINGS; ELECTROFORMING; APPARATUS THEREFOR

## Abstract

An aluminum alloy sheet that exhibits excellent surface quality after anodizing, includes a peritectic element that undergoes a peritectic reaction with at least aluminum, and requires an anodic oxide coating is characterized in that the concentration of the peritectic element in a solid-solution state that is present in the outermost surface area of the aluminum alloy sheet varies in the widthwise direction of the aluminum alloy sheet in the form of a band having a width of 0.05 mm or less, and the difference in the concentration of the peritectic element between adjacent bands is 0.008 mass % or less.

## Claims

### Claim 1

An aluminum alloy sheet that exhibits excellent surface quality after anodizing, the aluminum alloy sheet comprising a peritectic element that undergoes a peritectic reaction with at least aluminum, and requiring an anodic oxide coating, a concentration of the peritectic element in a solid-solution state that is present in an outermost surface area of the aluminum alloy sheet varying in a widthwise direction of the aluminum alloy sheet in a form of a band having a width of 0.05 mm or more, and a difference in the concentration of the peritectic element between adjacent bands being 0.008 mass % or less.

### Claim 2 (depends on 1)

The aluminum alloy sheet according to claim 1, comprising either or both of 0.001 to 0.1 mass % of Ti and 0.0001 to 0.4 mass % of Cr as the peritectic element.

### Claim 3 (depends on 1)

The aluminum alloy sheet according to claim 1, comprising either or both of 0.001 to 0.1 mass % of Ti and 0.0001 to 0.4 mass % of Cr as the peritectic element, and one or more elements among 0.3 to 6.0 mass % of Mg, 0.5 mass % or less of Cu, 0.5 mass % or less of Mn, 0.4 mass % or less of Fe, and 0.3 mass % or less of Si, with the balance being Al and unavoidable impurities.

### Claim 4

A method for producing the aluminum alloy sheet comprising subjecting an ingot to hot rolling and cold rolling to produce an aluminum alloy sheet, a rolling target side of the ingot having a structure in which a difference in concentration of a peritectic element between an area having a diameter of 5 μm and positioned in a center area of a crystal grain and an area having a diameter of 5 μm and positioned away from a grain boundary of the crystal grain by 2.5 μm is 0.040% or less.