# US 2013/0280120 A1 · Hard and Super-hard Metal Alloys and Methods for Making the Same

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2013/0280120 A1
- Document ID: US20130280120A1
- Status: Published application
- Kind: A1
- Application number: 13/844,751
- Filed: 2013-03-15
- Published: 2013-10-24
- Earliest claimed: 2010-04-23
- Inventors: Iver E. Anderson; Bruce A. Cook; Joel Harringa; Adam Boesenberg; Joel Rieken; Dave Byrd
- Web page: https://patentgrep.com/patent/US20130280120A1

## CPC

- C22C 9/01: with aluminium as the next major constituent
- B22F 1/00: Metallic powder; Treatment of metallic powder, e.g. to facilitate working or to improve properties
- B22F 3/14: simultaneously
- B22F 3/16: in successive or repeated steps
- B22F 5/00: Manufacture of workpieces or articles from metallic powder characterised by the special shape of the product
- B22F 9/04: starting from solid material, e.g. by crushing, grinding or milling ({C22C1/1084 takes precedence}; crushing, grinding or milling, in general, see the relevant subclasses, e.g. B02C)
- C22C 1/0425: {Copper-based alloys}
- C22C 1/047: comprising intermetallic compounds {(C22C1/0441 takes precedence)}
- C22C 13/00: Alloys based on tin
- B22F 3/12: Both compacting and sintering (by forging B22F3/17)
- B22F 2998/10: Processes characterised by the sequence of their steps
- C22C: ALLOYS (treatment of alloys C21D, C22F)
- B22F: WORKING METALLIC POWDER; MANUFACTURE OF ARTICLES FROM METALLIC POWDER; MAKING METALLIC POWDER (making alloys by powder metallurgy C22C); APPARATUS OR DEVICES SPECIALLY ADAPTED FOR METALLIC POWDER

## Abstract

The present invention relates to Cu33Al17 alloys and Cu33Al17-based bulk alloys and coatings that exhibit significantly increased hardness characteristics compared to traditional copper-aluminum alloys

## Claims

### Claim 1

A method for producing Cu33Al17 based alloys in bulk form comprising:
mixing Cu powder and Al powder in sufficient amounts to form a blended copper-aluminum based mixture consisting essentially of: 77-80 wt. % Cu and 20-23 wt. % Al with the remainder consisting of one or more elements selected from the group consisting of: Zn, Sn, Ga, Ge and combinations thereof, or unavoidable impurities, and wherein the wt. % ratio of Cu to Al is between about 3:1 and 4:1;
cold pressing the blended copper-aluminum based mixture to form a copper-aluminum green body; and
sintering the pressed copper aluminum to form a uniform, single-phase Cu33Al17 alloy.

### Claim 2 (depends on 1)

The method of claim 1, wherein the sintering step is followed by pressure driven consolidation.

### Claim 3 (depends on 1)

The method of claim 1, wherein the sintering step is replaced by a pressure driven consolidation step wherein the green body is hot pressed to form a uniform, single-phase Cu33Al17 alloy.

### Claim 4 (depends on 1)

The method of claim 1, wherein the copper-aluminum based mixture consists of: 77-80 wt. % Cu and 20-23 wt. % Al.

### Claim 5 (depends on 1)

The method of claim 1, wherein the copper-aluminum based mixture consists essentially: 77.4-79.2 wt. % Cu and 20.7-22.6 wt. % Al.

### Claim 6 (depends on 1)

The method of claim 1 wherein the copper-aluminum based mixture consists of: 77.4-79.2 wt. % Cu and 20.7-22.6 wt. % Al.

### Claim 7 (depends on 1)

The method of claim 1, wherein the copper-aluminum based mixture consists essentially: 77.43-79.28 wt. % Cu and 20.72-22.57 wt. % Al.

### Claim 8 (depends on 1)

The method of claim 1, wherein the copper-aluminum based mixture consists of: 77.43-79.28 wt. % Cu and 20.72-22.57 wt. % Al.

### Claim 9 (depends on 1)

The method of claim 1, wherein the copper-aluminum based mixture consists essentially: 78.4-79.3 wt. % Cu and 20.72-21.56 wt. % Al.

### Claim 10 (depends on 1)

The method of claim 1, wherein the copper-aluminum based mixture consists of: 78.4-79.3 wt. % Cu and 20.72-21.56 wt. % Al.

### Claim 11 (depends on 1)

The method of claim 1, wherein Cu and Al are mixed in a wt. % ratio of between about 3.4:1 to 3.9:1, Cu to Al.

### Claim 12 (depends on 1)

The method of claim 1, wherein Cu and Al are mixed in a wt. % ratio of between about 3.43:1 and 3.83:1, Cu to Al.

### Claim 13 (depends on 1)

The method of claim 1, wherein mixture consists essentially of: 77.4-79.2 wt. % Cu and 20.72-22.57 wt. % Al with the remainder consisting of one or more elements selected from the group consisting of: Zn, Sn, Ga, Ge, and combinations thereof.

### Claim 14 (depends on 1)

The method of claim 1, wherein mixture consists essentially of: 77.4-79.2 wt. % Cu and 20.72-22.57 wt. % Al with the remainder consisting: Sn, wherein the wt. % ratio of Cu to Al is between about 3.4:1 and 3:9:1.

### Claim 15 (depends on 1)

The method of claim 1, wherein the copper-aluminum green body is sintered at a temperature of between about 500-650° C.

### Claim 16 (depends on 1)

A product made according to the method of claim 1.

### Claim 17

A Cu33Al17 based bulk alloy consisting essentially of: 77-82 wt. % Cu and 18-23 wt. % Al with the remainder consisting of one or more elements selected from the group consisting of: Zn, Sn, Ga, Ge and combinations thereof, and wherein the wt. % ratio of Cu to Al is between about 3:1 and 4.6:1;

### Claim 18 (depends on 17)

The alloy of claim 17, wherein the alloy consists essentially of: 77.4-79.2 wt. % Cu and 18-23 wt. % Al with the remainder consisting of one or more elements selected from the group consisting of: Zn, Sn, Ga, Ge and combinations thereof, and wherein the wt. % ratio of Cu to Al is between about 3:4 and 3.9:1.

### Claim 19 (depends on 17)

The alloy of claim 17, wherein the alloy consists essentially of: 78.4-79.3 wt. % Cu and 20.72-21.56 wt. % Al with the remainder consisting of one or more elements selected from the group consisting of: Zn, Sn, Ga, Ge and combinations thereof.

### Claim 20 (depends on 17)

The Cu33Al17 based alloy of claim 17, wherein the alloy consists essentially of 77-80 wt. % Cu and 20-23 wt. % Al.

### Claim 21 (depends on 17)

The Cu33Al17 based alloy of claim 17, wherein the alloy consists essentially of 77.4-79.2 wt. % Cu and 20.7-22.6 wt. % Al.

### Claim 22 (depends on 17)

The Cu33Al17 based alloy of claim 17, wherein the alloy consists essentially of 78.4-79.3 wt. % Cu and 20.72-21.56 wt. % Al.

### Claim 23 (depends on 17)

The Cu33Al17 based alloy of claim 17, wherein the alloy consists of 77-80 wt. % Cu and 20-23 wt. % Al.

### Claim 24 (depends on 17)

The Cu33Al17 based alloy of claim 17, wherein the alloy consists of 78.4-79.3 wt. % Cu and 20.72-21.56 wt. % Al.