# US 2013/0280119 A1 · Magnetic material and method for producing the same

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2013/0280119 A1
- Document ID: US20130280119A1
- Status: Published application
- Kind: A1
- Application number: 13/820,903
- Filed: 2011-08-29
- Published: 2013-10-24
- Earliest claimed: 2010-09-06
- Assignees: Daihatsu Motor Co., Ltd.
- Inventors: Kousaku Okamura; Kazuhiko Madokoro
- Web page: https://patentgrep.com/patent/US20130280119A1

## CPC

- C22C 45/02: with iron as the major constituent
- B22F 3/087: using high energy impulses, e.g. magnetic field impulses
- B22F 3/105: by using electric current {other than for infrared radiant energy}, laser radiation or plasma (B22F3/11 takes precedence){; by ultrasonic bonding (B22F3/115 takes precedence)}
- C22C 1/11: Making amorphous alloys
- C22C 28/00: Alloys based on a metal not provided for in groups C22C5/00 - C22C27/00
- C22C 33/003: {making amorphous alloys}
- C22C 33/0278: {with at least one alloying element having a minimum content above 5%}
- C22C 38/001: {containing N}
- C22C 38/005: {containing rare earths, i.e. Sc, Y, Lanthanides}
- C22C 45/00: Amorphous alloys (making amorphous non-ferrous alloys C22C1/11)
- H01F 1/01: of inorganic materials (H01F1/44 takes precedence)
- H01F 1/053: containing rare earth metals
- H01F 1/0571: {in the form of particles, e.g. rapid quenched powders or ribbon flakes}
- H01F 1/0577: {sintered}
- H01F 1/059: and Va elements, e.g. Sm2Fe17N2
- H01F 1/08: pressed, sintered, or bound together
- H01F 1/086: {sintered}
- H01F 41/02: for manufacturing cores, coils, or magnets (H01F41/14 takes precedence; for dynamo-electric machines H02K15/00)
- H01F 41/0246: {Manufacturing of magnetic circuits by moulding or by pressing powder (magnetic cores made by moulding or by pressing powder H01F27/255; soft magnetic particles H01F1/20, H01F1/36)}
- H01F 41/0273: {Imparting anisotropy (methods and devices for magnetising permanent magnets H01F13/003)}
- B22F 2003/1051: {by electric discharge}
- B22F 2999/00: Aspects linked to processes or compositions used in powder metallurgy
- C22C 2202/02: Magnetic
- C22C: ALLOYS (treatment of alloys C21D, C22F)
- B22F: WORKING METALLIC POWDER; MANUFACTURE OF ARTICLES FROM METALLIC POWDER; MAKING METALLIC POWDER (making alloys by powder metallurgy C22C); APPARATUS OR DEVICES SPECIALLY ADAPTED FOR METALLIC POWDER
- H01F: MAGNETS; INDUCTANCES; TRANSFORMERS; SELECTION OF MATERIALS FOR THEIR MAGNETIC PROPERTIES

## Abstract

A magnetic material is produced by mixing a magnet powder with an amorphous metal containing a rare-earth element, iron, and boron, the rare-earth element being in the range of 22 to 44 atomic %, and the boron being in the range of 6 to 28 atomic %; and heating the mixture to a temperature or more, the temperature being lower than the crystallization temperature of the amorphous metal by 30° C., or when the amorphous metal is a metallic glass, to a temperature of the glass transition temperature thereof or more.

## Claims

### Claim 1

A magnetic material in which a magnet powder and an amorphous metal are used as ingredients,
wherein the amorphous metal contains a rare-earth element, iron, and boron;
the amorphous metal contains the rare-earth element in the range of 22 to 44 atomic %, and the boron in the range of 6 to 28 atomic %; and
the magnetic material is obtained by
mixing the magnet powder and the amorphous metal, and
heating the mixture to a temperature or more, the temperature being lower than the crystallization temperature (Tx) of the amorphous metal by 30° C., or
when the amorphous metal is a metallic glass, heating the mixture to a temperature of the glass transition temperature (Tg) thereof or more.

### Claim 2 (depends on 1)

The magnetic material according to claim 1, wherein
the amorphous metal further contains cobalt, and in the amorphous metal, the atomic ratio of the cobalt to iron is 1.5 or less.

### Claim 3 (depends on 1)

The magnetic material according to claim 1, further containing an additive,
and the additive content relative to 100 parts by mass of the magnetic material is below 10 parts by mass.

### Claim 4 (depends on 1)

The magnetic material according to claim 1, wherein
a magnetic anisotropic magnet powder is used as the magnet powder, and a mixture of the magnetic anisotropic magnet powder with the amorphous metal is subjected to magnetic field pressing.

### Claim 5

A method for producing a magnetic material comprising:
mixing a magnet powder with an amorphous metal having an initial softening temperature of 600° C. or less, thereby producing a powder mixture;
charging the powder mixture to a mold, and pressure molding the powder mixture in a magnetic field, thereby producing a compact, and
subjecting the compact to spark plasma sintering in the same mold, thereby heating the compact to a temperature of the initial softening temperature or more of the amorphous metal.