# US 2013/0279987 A1 · Installation of leakage barriers to enhance yield of mineral deposits in unlined solar pond systems

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2013/0279987 A1
- Document ID: US20130279987A1
- Status: Published application
- Kind: A1
- Application number: 13/922,755
- Filed: 2013-06-20
- Published: 2013-10-24
- Earliest claimed: 2010-09-22
- Assignees: Great Salt Lake Minerals Corporation
- Applicants: Great Salt Lake Minerals Corporation
- Inventors: Mark Reynolds; Thomas S. Burton; Corey R. Milne; Steven R. Day
- Web page: https://patentgrep.com/patent/US20130279987A1

## CPC

- E02B 7/02: Fixed barrages
- C04B 28/02: containing hydraulic cements other than calcium sulfates
- C04B 28/08: Slag cements
- E02B: HYDRAULIC ENGINEERING (ship-lifting E02C; dredging E02F)
- C04B: LIME, MAGNESIA; SLAG; CEMENTS; COMPOSITIONS THEREOF, e.g. MORTARS, CONCRETE OR LIKE BUILDING MATERIALS; ARTIFICIAL STONE {(roofing granules E04D7/005)}; CERAMICS (devitrified glass-ceramics C03C10/00); REFRACTORIES; TREATMENT OF NATURAL STONE

## Abstract

Slurry walls and methods of using those slurry walls to seal unlined solar ponds are provided. The slurry walls are formed from a mixture comprising clay and cement in water. A trench is keyed into the dike surrounding the solar pond, down to a geotechnically predetermined level. The slurry is deposited into the trench and allowed to harden, after which it is covered with a membrane or other covering. The inventive slurry walls reduce, and preferably prevent, leakage of water from the solar pond.

## Claims

### Claim 1

A slurry wall formed from a hardened mixture, the mixture before hardening comprising:
from about 3% to about 25% by weight cement, based upon the total weight of the mixture taken as 100% by weight;
from about 1% to about 15% by weight clay, based upon the total weight of the mixture taken as 100% by weight; and
water.

### Claim 2 (depends on 1)

The wall of claim 1, wherein said cement is selected from the group consisting of Types II-V Portland cements, blast furnace slag cement, and mixtures thereof.

### Claim 3 (depends on 1)

The wall of claim 1, wherein said clay is selected from the group consisting of bentonite clay, modified bentonite clay, sepiolite clay, attapulgite clay, and mixtures thereof.

### Claim 4 (depends on 1)

The wall of claim 1, wherein said water comprises the following properties:
a pH of from about 6.0 to about 9.5;
a hardness of less than about 400 ppm;
an alkalinity of less than about 400 ppm;
a total dissolved solids of less than about 4,000 ppm;
a density of from about 1.0 gm/cc to about 1.04 gm/cc; and
an apparent viscosity of from about 0.8 cP to about 2 cP.

### Claim 5 (depends on 4)

The wall of claim 4, wherein said mixture comprises Portland Cement and bentonite.

### Claim 6 (depends on 5)

The wall of claim 5, wherein said mixture comprises about 17% by weight Portland Cement and about 6% by weight benonite, based upon the total weight of the mixture taken as 100% by weight.

### Claim 7 (depends on 1)

The wall of claim 1, wherein said water comprises the following properties:
a pH of from about 7.0 to about 9.0;
a hardness of less than about 600 ppm;
an alkalinity of less than about 400 ppm;
a total dissolved solids of less than about 200,000 ppm;
a density of from about 1.05 gm/cc to about 1.21 gm/cc; and
an apparent viscosity of from about 0.8 cP to about 2 cP.

### Claim 8 (depends on 7)

The wall of claim 7, wherein said mixture comprises Portland Cement, blast furnace slag cement, and sepiolite.

### Claim 9 (depends on 8)

The wall of claim 8, wherein said mixture comprises about 1% by weight Portland Cement, about 12.5% by weight blast furnace slag cement, and about 5.5% by weight sepiolite, based upon the total weight of the mixture taken as 100% by weight.

### Claim 10 (depends on 1)

The wall of claim 1, wherein said slurry wall has a permeability of less than about 1×10−4 cm/sec.

### Claim 11 (depends on 1)

The wall of claim 1, wherein said slurry wall has an unconfined compressive strength of at least about 2.5 psig about 7 days after said slurry wall is formed.

### Claim 12 (depends on 1)

The wall of claim 1, wherein said slurry wall has a slake decay of less than about 20% by volume at about 30 days after said slurry wall is formed.

### Claim 13 (depends on 1)

The wall of claim 1, wherein said mixture is capable of hardening within about 7 days after said slurry wall is formed, as measured by a penetrometer.

### Claim 14 (depends on 1)

The wall of claim 1, wherein said mixture has a Marsh Funnel viscosity of from about 20 seconds to about 70 seconds.