# US 2013/0279174 A1 · Methods for tailoring the properties of a reflective coating

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2013/0279174 A1
- Document ID: US20130279174A1
- Status: Published application
- Kind: A1
- Application number: 13/711,991
- Filed: 2012-12-12
- Published: 2013-10-24
- Earliest claimed: 2012-04-19
- Assignees: GE Lighting Solutions, LLC
- Applicants: Ge Lighting Solutions, LLC
- Inventors: Dengke CAI; Gary Robert ALLEN; Ashfaqul I. CHOWDHURY; Jeyachandrabose CHINNIAH
- Web page: https://patentgrep.com/patent/US20130279174A1

## CPC

- F21V 7/24: characterised by the material
- B05D 5/063: {Reflective effect (B05D5/067 takes precedence)}
- F21V 7/28: characterised by coatings
- G02B 5/0236: {the diffusion taking place within the volume of the element}
- G02B 5/0284: {used in reflection}
- G02B 5/0294: {adapted to provide an additional optical effect, e.g. anti-reflection or filter}
- G02B 5/0808: {having a single reflecting layer (G02B5/0883, G02B5/0891 take precedence)}
- F21V: FUNCTIONAL FEATURES OR DETAILS OF LIGHTING DEVICES OR SYSTEMS THEREOF; STRUCTURAL COMBINATIONS OF LIGHTING DEVICES WITH OTHER ARTICLES, NOT OTHERWISE PROVIDED FOR
- B05D: PROCESSES FOR APPLYING FLUENT MATERIALS TO SURFACES, IN GENERAL (conveying articles or workpieces through baths of liquid B65G, e.g. B65G49/02)
- G02B: OPTICAL ELEMENTS, SYSTEMS OR APPARATUS

## Abstract

Methods are provided for forming a reflective coating by applying a precursor material onto the substrate; soft curing the precursor material at a first curing energy level; and thereafter, hard curing the precursor material at a second curing energy level having a higher amount of energy than the first curing energy level to form the reflective coating. Other methods are provided for forming a reflective coating a surface of a plastic substrate by heating the surface of the plastic substrate to a deposition temperature, applying a polymeric resin onto the heated surface, and crosslinking the polymeric resin to form the reflective coating. The polymeric resin can include a cross-linkable powder, a cross-linker, and a pigment, with the deposition temperature being about 10° C. or greater than the melting point of the cross-linkable binder. Lighting apparatus formed from such methods are also provided.

## Claims

### Claim 1

A method for forming a reflective coating on a substrate, the method comprising:
applying a precursor material onto the substrate, wherein the precursor material comprises a cross-linkable binder resin, a cross-linker, and a pigment;
soft curing the precursor material at a first curing energy level for a first curing duration; and thereafter,
hard curing the precursor material at a second curing energy level for a second curing duration to form the reflective coating, wherein the second curing energy level has a higher amount of energy than the first curing energy level.

### Claim 2 (depends on 1)

The method as in claim 1, wherein soft curing at the first energy level is achieved via heating to a first curing temperature, and wherein hard curing at the second energy level is achieved via heating to a second curing temperature.

### Claim 3 (depends on 2)

The method as in claim 2, wherein the first curing temperature is about 75° C. to about 100° C., and wherein the second curing temperature is at least about 10° C. greater than the first curing temperature.

### Claim 4 (depends on 2)

The method as in claim 2, wherein the first curing temperature is below the softening point of the cross-linkable binder resin in the precursor material.

### Claim 5 (depends on 2)

The method as in claim 2, wherein the first curing temperature is about 5° C. or more below the softening point of the cross-linkable binder resin in the precursor material.

### Claim 6 (depends on 1)

The method as in claim 1, wherein the first curing duration is about 10 minutes or longer, and wherein the second curing duration is about 10 minutes or longer.

### Claim 7 (depends on 2)

The method as claim 2, wherein the second curing temperature is about 100° C. to about 150° C.

### Claim 8 (depends on 1)

The method as in claim 1, wherein the cross-linkable binder resin comprises monomers, oligomers, polymers, or copolymers that contain reactive carboxyl groups, reactive hydroxyl groups, or mixtures thereof, and wherein the cross-linkable polymeric binder interacts with the cross-linker to form a 3-dimensional cross-linked polymeric structure.

### Claim 9 (depends on 8)

The method as in claim 8, wherein the cross-linker comprises polyfunctional aziridines, epoxy resins, carbodiimide, oxazoline functional polymers, melamine-formaldehyde, urea formaldehyde, amine-epichlorohydrin, multi-functional isocyanates, or combinations thereof.

### Claim 10 (depends on 1)

The method as in claim 1, wherein the pigment comprises an inorganic particle.

### Claim 11 (depends on 1)

The method as in claim 1, further comprising,
further curing the precursor material at a third curing energy level for a third duration, wherein the third curing energy level is higher than the second curing energy level.

### Claim 12 (depends on 1)

A lighting apparatus comprising:
a glass sheet;
optionally, a primer coating on the glass sheet; and
a reflective coating formed on a glass sheet such that any primer coating is positioned between the reflective coating and the glass sheet, wherein the reflective coating is formed according to the method of claim 1.

### Claim 13

A method of forming a reflective coating on a surface of a plastic substrate, the method comprising:
heating the surface of the plastic substrate to a deposition temperature;
applying a polymeric resin onto the surface of the plastic substrate while at the deposition temperature, wherein the polymeric resin comprises a cross-linkable powder, a cross-linker, and a pigment, and wherein the deposition temperature is about 10° C. or greater than the melting point of the cross-linkable binder; and
crosslinking the cross-linkable powder and a cross-linker to form the reflective coating on the surface of the plastic substrate.

### Claim 14 (depends on 13)

The method as in claim 13, wherein the polymeric resin is applied directly onto the surface of the plastic substrate.

### Claim 15 (depends on 13)

The method as in claim 13, wherein the cross-linkable powder has a melting point that is less than about 100° C.

### Claim 16 (depends on 13)

The method as in claim 13, wherein the cross-linkable powder has a melting point that is about 60° C. to about 90° C.

### Claim 17 (depends on 13)

The method as in claim 13, wherein the deposition temperature of the surface of the plastic substrate is greater than about 100° C. and less than the melting point of the substrate.

### Claim 18 (depends on 13)

The method as in claim 13, wherein the deposition temperature of the surface of the plastic substrate is about 100° C. to about 150° C.

### Claim 19 (depends on 13)

The method as in claim 13, wherein the polymeric resin is sprayed onto the surface of the plastic substrate.

### Claim 20 (depends on 13)

The method as in claim 13, wherein the reflective coating has a coating thickness of about 100 μm to about 200 μm.

### Claim 21 (depends on 13)

The method as in claim 13, wherein the cross-linkable powder comprises a polyester material, a (meth)acrylic material, an epoxy material, or a mixture thereof.

### Claim 22 (depends on 13)

The method as in claim 13, wherein the reflective coating is reflective in the visible spectrum of light.

### Claim 23

A lighting system, comprising:
a lamp;
a reflector positioned to reflect light emitted by the lamp, wherein the reflector comprises a plastic substrate; and
a reflective coating deposited directly on a light reflecting surface of the reflector, wherein the reflective coating comprises a cross-linked polymeric powder and a pigment.

### Claim 24 (depends on 23)

The lighting system as in claim 23, wherein the reflective coating reflects at least about 95% of light in the visible spectrum, with a matte finish having a glossy number of about 1 LU or less at 60 degree incident angle.

### Claim 25 (depends on 23)

The lighting system as in claim 23, wherein the cross-linked polymeric powder is formed from a cross-linkable powder and a cross-linker.