# US 2013/0277786 A1 · Photodiode and Photodiode Array with Improved Performance Characteristics

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2013/0277786 A1
- Document ID: US20130277786A1
- Status: Published application
- Kind: A1
- Application number: 13/725,803
- Filed: 2012-12-21
- Published: 2013-10-24
- Earliest claimed: 2008-08-27
- Assignees: OSI Optoelectronics, Inc.
- Applicants: OSI Optoelectronics
- Inventors: Peter Steven Bui; Narayan Dass Taneja
- Web page: https://patentgrep.com/patent/US20130277786A1

## CPC

- H10F 77/40: Optical elements or arrangements (surface textures H10F77/70)
- G01T 1/20183: {Arrangements for preventing or correcting crosstalk, e.g. optical or electrical arrangements for correcting crosstalk}
- H10F 30/295: Surface barrier or shallow PN junction radiation detectors, e.g. surface barrier alpha-particle detectors
- H10F 77/306: {for devices having potential barriers}
- H10F 77/496: {Luminescent members, e.g. fluorescent sheets (wavelength conversion means for photovoltaic cells H10F77/45)}
- H10F: INORGANIC SEMICONDUCTOR DEVICES SENSITIVE TO INFRARED RADIATION, LIGHT, ELECTROMAGNETIC RADIATION OF SHORTER WAVELENGTH OR CORPUSCULAR RADIATION
- G01T: MEASUREMENT OF NUCLEAR OR X-RADIATION (radiation analysis of materials, mass spectrometry G01N23/00; tubes for determining the presence, intensity, density or energy of radiation or particles H01J47/00)

## Abstract

The present invention is a photodiode and/or photodiode array, having a p+ diffused area that is smaller than the area of a mounted scintillator crystal, designed and manufactured with improved device characteristics, and more particularly, has relatively low dark current, low capacitance and improved signal-to-noise ratio characteristics. More specifically, the present invention is a photodiode and/or photodiode array that includes a metal shield for reflecting light back into a scintillator crystal, thus allowing for a relatively small p+ diffused area.

## Claims

### Claim 1

A photodiode comprising:
a low resistivity substrate having at least a front side and a back side, wherein said low resistivity is in the range of 1000 ohm cm to 2000 ohm cm;
a shallow p+ diffused region on said front side, wherein said shallow p+ region is smaller than a scintillator crystal mounted on the front side of the photodiode;
at least one front side cathode contact and at least one front side anode contact, comprised of metal; and
a reflective metal shield on at least a portion of said front side, wherein said metal shield reflects incident light back into said scintillator crystal.

### Claim 2 (depends on 1)

The photodiode of claim 1 wherein said scintillator crystal mounted on the front side of the photodiode has a top surface area of 2 mm×2 mm.

### Claim 3 (depends on 1)

The photodiode of claim 1 wherein the shallow p+ diffused region is on the order of 1 mm or less in length and 1 mm or less in width.

### Claim 4 (depends on 1)

The photodiode of claim 1 wherein the reflective metal shield comprises aluminum.

### Claim 5 (depends on 1)

The photodiode of claim 1, wherein a distance between the shallow p+ diffused region and an edge of the photodiode ranges from 0.3 mm to 0.5 mm.

### Claim 6 (depends on 1)

The photodiode of claim 1 further comprising an anti-reflective layer formed from SiO2 having a thickness of 900 Å.

### Claim 7 (depends on 1)

The photodiode of claim 1 further comprising an anti-reflective layer formed from SiO2 having a thickness of 150 Å and Si3N4 having a thickness of 400 Å, for a total layer thickness of 550 Å.

### Claim 8

A photodiode array comprising:
a low resistivity substrate having at least a front side and a back side, wherein said low resistivity is in the range of 1000 ohm cm to 2000 ohm cm;
a plurality of diode elements integrally formed in the substrate forming said array, wherein each diode element has a shallow p+ diffused region on said front side, wherein said shallow p+ region is smaller than a scintillator crystal mounted on the front side of the photodiode;
at least one front side cathode contact and at least one front side anode contact, comprised of metal; and
a reflective metal shield on at least a portion of said front side, wherein said metal shield reflects incident light back into the scintillator crystal.

### Claim 9 (depends on 8)

The photodiode array of claim 8 wherein said scintillator crystal mounted on the front side of the photodiode element has a top surface area of 2 mm×2 mm.

### Claim 10 (depends on 8)

The photodiode array of claim 8 wherein the shallow p+ diffused region is approximately 1 mm or less in length and 1 mm or less in width.

### Claim 11

A method of fabricating a photodiode on a low resistivity substrate wafer having a front side and a back side, said method comprising the steps of:
providing an oxide layer on both the front side and the back side;
implementing an etching process on both the front side and back side to define a plurality of regions on the front side and back side;
filling the plurality of regions with n+ dopant;
depositing an oxide layer on both the front side and the back side of the wafer;
creating a deep p+ diffused region on the front side;
fabricating an active area on said front side, wherein said active area is smaller than a scintillator crystal mounted on the front side of the photodiode;
forming an anti-reflective layer on the front side of said device;
forming a shallow p+ active area region;
forming at least one contact window; and
performing a metal deposition process to etch metal on both the front side and back side of the device wafer, wherein said metal deposition process creates connections and wherein said metal deposition process forms a reflective metal shield on the front side.

### Claim 12 (depends on 11)

The method of claim 11 wherein said low resistivity substrate has a resistivity in the range of 1000 ohm cm to 2000 ohm cm.

### Claim 13 (depends on 11)

The method of claim 11 wherein the step of providing an oxide layer on both the front side and the back side results in an oxide layer having a thickness of approximately 10,000 Å.

### Claim 14 (depends on 11)

The method of claim 11 wherein said anti-reflective later is formed on said front side of said device via thermal growth of a layer of SiO2, having a thickness of 150 Å followed by LPCVD deposition of Si3N4, having a thickness of 400 Å, for a total layer thickness of 550 Å.

### Claim 15 (depends on 12)

The method of claim 12 wherein the metal shield on the front side of the device wafer reflects incident light back into the scintillator crystal mounted on the photodiode.