# US 2013/0277678 A1 · Thin-film semiconductor device and method of manufacturing the same

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2013/0277678 A1
- Document ID: US20130277678A1
- Status: Published application
- Kind: A1
- Application number: 13/918,011
- Filed: 2013-06-14
- Published: 2013-10-24
- Earliest claimed: 2011-10-25
- Assignees: Panasonic Liquid Crystal Display Co., Ltd.; Panasonic Corporation
- Applicants: Panasonic Liquid Crystal Display Co., Ltd.; Panasonic Corporation
- Inventors: Sei OOTAKA; Hiroshi YOSHIOKA; Takahiro KAWASHIMA; Hikaru NISHITANI
- Web page: https://patentgrep.com/patent/US20130277678A1

## CPC

- H10D 30/6732: {Bottom-gate only TFTs}
- H10D 30/0316: {of lateral bottom-gate TFTs comprising only a single gate}
- H10D 30/0321: {comprising silicon, e.g. amorphous silicon or polysilicon}
- H10D 30/6745: {Polycrystalline or microcrystalline silicon}
- H10D 30/6746: {Amorphous silicon}
- H10D 86/0229: {characterised by control of the annealing or irradiation parameters}
- H10D 30/6734: {having gate electrodes arranged on both top and bottom sides of the channel, e.g. dual-gate TFTs}
- H10D 30/6744: {Monocrystalline silicon}
- H10D 30/6758: {characterised by the insulating substrates}
- H10D: INORGANIC ELECTRIC SEMICONDUCTOR DEVICES

## Abstract

A thin-film semiconductor device manufacturing method according to the present disclosure includes: preparing a substrate; forming a gate electrode above the substrate; forming a gate insulating film above the substrate; forming an amorphous film (amorphous silicon film) above the substrate; forming a crystalline film (crystalline silicon film) including a first crystal and a second crystal, by crystallizing the amorphous film, the first crystal (i) containing subgrains formed with different crystal orientations in a single crystal and (ii) including a subgrain boundary formed by plural crystal planes between the subgrains, the second crystal having an average crystal grain size smaller than an average crystal grain size of the first crystal; thinning the crystalline film; and forming a source electrode and a drain electrode above the substrate.

## Claims

### Claim 1

A thin-film semiconductor device manufacturing method comprising:
preparing a substrate;
forming a gate electrode above the substrate;
forming a gate insulating film above the substrate;
forming an amorphous film above the substrate;
forming a crystalline film including a first crystal and a second crystal, by crystallizing the amorphous film, the first crystal (i) containing subgrains formed with different crystal orientations in a single crystal and (ii) including a subgrain boundary formed by plural crystal planes between the subgrains, the second crystal having an average crystal grain size smaller than an average crystal grain size of the first crystal;
thinning the crystalline film; and
forming a source electrode and a drain electrode above the substrate.

### Claim 2 (depends on 1)

The thin-film semiconductor device manufacturing method according to claim 1,
wherein the amorphous film is an amorphous silicon film.

### Claim 3 (depends on 2)

The thin-film semiconductor device manufacturing method according to claim 2,
wherein the amorphous silicon film has a photoluminescence (PL) intensity greater than or equal to 0.65 when photon energy is 1.1 eV in a PL spectrum normalized to have a maximum PL intensity of 1.

### Claim 4 (depends on 1)

The thin-film semiconductor device manufacturing method according to claim 1,
wherein in the forming of the crystalline film, the amorphous film is crystallized by thermal annealing.

### Claim 5 (depends on 4)

The thin-film semiconductor device manufacturing method according to claim 4,
wherein the thermal annealing is performed with a thermal annealing temperature ranging from 700° C. to 800° C. and a thermal annealing time ranging from 1 minute to 30 minutes.

### Claim 6 (depends on 1)

The thin-film semiconductor device manufacturing method according to claim 1,
wherein in the thinning, the crystalline film is thinned by etching.

### Claim 7 (depends on 6)

The thin-film semiconductor device manufacturing method according to claim 6,
wherein the etching is hydrofluoric acid etching.

### Claim 8 (depends on 6)

The thin-film semiconductor device manufacturing method according to claim 6, further comprising
oxidizing an upper surface of the crystalline film before the thinning,
wherein in the thinning, an oxidized upper portion of the crystalline film is removed by the etching.

### Claim 9 (depends on 8)

The thin-film semiconductor device manufacturing method according to claim 8,
wherein the oxidizing is performed by ozone oxidation.

### Claim 10 (depends on 1)

The thin-film semiconductor device manufacturing method according to claim 1,
wherein the crystalline film before the thinning has a thickness of at least 55 nm, and
the crystalline film after the thinning has a thickness ranging from 20 nm to 50 nm.

### Claim 11 (depends on 1)

The thin-film semiconductor device manufacturing method according to claim 1,
wherein the first crystal consists of a crystal grain having an average crystal grain size ranging from 200 nm to 2 μm, and
the second crystal consists of a crystal grain having an average crystal grain size ranging from 20 nm to 50 nm.

### Claim 12

A thin-film semiconductor device comprising:
a substrate;
a gate electrode above the substrate;
a crystalline film above the substrate;
a gate insulating film between the gate electrode and the crystalline film;
a source electrode and a drain electrode which are above the substrate,
wherein the crystalline film includes a first crystal and a second crystal, the first crystal (i) containing subgrains formed with different crystal orientations in a single crystal and (ii) including a subgrain boundary formed by plural crystal planes between the subgrains, the second crystal having an average crystal grain size smaller than an average crystal grain size of the first crystal, and
a percentage of the first crystal in an upper surface of the crystalline film is higher than a percentage of the first crystal in a lower surface of the crystalline film.

### Claim 13 (depends on 12)

The thin-film semiconductor device according to claim 12,
wherein the second crystal is a single-grained structure.

### Claim 14 (depends on 12)

The thin-film semiconductor device according to claim 12,
wherein the crystalline film is formed by thinning a precursor film which includes the first crystal and the second crystal.

### Claim 15 (depends on 14)

The thin-film semiconductor device according to claim 14,
wherein the precursor film has a thickness of at least 55 nm, and
the crystalline film has a thickness ranging from 20 nm to 50 nm.

### Claim 16 (depends on 12)

The thin-film semiconductor device according to claim 12,
wherein the first crystal consists of a crystal grain having an average crystal grain size ranging from 200 nm to 2 μm, and
the second crystal consists of a crystal grain having an average crystal grain size ranging from 20 nm to 50 nm.

### Claim 17 (depends on 12)

The thin-film semiconductor device according to claim 12,
wherein a percentage content of the first crystal included in the crystalline film is higher towards the source electrode and the drain electrode than towards the gate insulating film, in a thickness direction of the crystalline film.

### Claim 18 (depends on 12)

The thin-film semiconductor device according to claim 12,
wherein the thin-film semiconductor device is of a top-gate type.