# US 2013/0277619 A1 · PROCESS FOR THE PREPARATION OF HIGH VOLTAGE NANO COMPOSITE CATHODE (4.9vV) FOR LITHIUM ION BATTERIES

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2013/0277619 A1
- Document ID: US20130277619A1
- Status: Published application
- Kind: A1
- Application number: 13/880,704
- Filed: 2011-03-30
- Published: 2013-10-24
- Earliest claimed: 2010-10-20
- Assignees: Council of Scientific and Industrial Research
- Inventors: Sukumaran Gopukumar; Chandrasekaran Nithya; Ramasamy Thirunakaran; Arumugam Sivashanmugam
- Web page: https://patentgrep.com/patent/US20130277619A1

## CPC

- H01M 4/364: {as mixtures}
- C01B 25/45: containing plural metal, or metal and ammonium
- C01B 32/05: Preparation or purification of carbon not covered by groups C01B32/15, C01B32/20, C01B32/25, C01B32/30
- H01M 4/366: {as layered products}
- H01M 4/5825: {Oxygenated metallic salts or polyanionic structures, e.g. borates, phosphates, silicates, olivines}
- H01M 4/625: {Carbon or graphite}
- H01M 4/136: Electrodes based on inorganic compounds other than oxides or hydroxides, e.g. sulfides, selenides, tellurides, halogenides or LiCoFy
- Y02E 60/10: Energy storage using batteries
- H01M: PROCESSES OR MEANS, e.g. BATTERIES, FOR THE DIRECT CONVERSION OF CHEMICAL ENERGY INTO ELECTRICAL ENERGY
- C01B: NON-METALLIC ELEMENTS; COMPOUNDS THEREOF; {METALLOIDS OR COMPOUNDS THEREOF NOT COVERED BY SUBCLASS C01C}
- Y02E: REDUCTION OF GREENHOUSE GAS [GHG] EMISSIONS, RELATED TO ENERGY GENERATION, TRANSMISSION OR DISTRIBUTION

## Abstract

An olivine structured nano-composite LiMxMn1−xPO4/C was synthesized by a sol-gel assisted high energy ball mill method and the synthesis method does not require any inert atmosphere. Electrochemical cycling studies were carried out between 3.0-4.6V using 1M LiPF6 in 1:1 EC/DEC as electrolyte. The charge/discharge cycling studies of the nano-composite exhibit an average discharge capacity of 158 mAh/g at 0.1 C rate over the investigated 50 cycles.

## Claims

### Claim 1

A process for the synthesis of high voltage nano composite cathode material LiMxMn1−xPO4/C wherein M is a transition metal cation dopant and x varies from 0 to 0.12 for lithium ion batteries and the said process comprising the steps of:
i. mixing salts of lithium, manganese, dopant and ammonium dihydrogen orthophosphate in the ratio ranging between 4.1:9.8:0:4.6 to 4.1:8.8:1:4.6;
ii. dissolving the mixture as obtained in step (i) in water in the ratio ranging between 1:1 at temperature in the range of 27-30° C.;
iii. adding the solution as obtained in step (ii) in glycine in the ratio ranging between 1:1;
iv. heating the solution as obtained in step (iii) at temperature in the range of 60 to 75° C. for period in the range of 2 to 4 hours;
v. drying the heated solution as obtained in step (iv) for period in the range of 10 to 12 hrs at temperature in the range of 100-120° C.;
vi. grinding and calcining the mixture as obtained in step (v) at temperature in the range of 800-850° C. for period in the range of 4 to 5 hrs in air atmosphere to obtain high voltage nano composite cathode material.

### Claim 2 (depends on 1)

A process as claimed in step (i) of claim 1, wherein salts used are selected from acetates or nitrates.

### Claim 3 (depends on 1)

A process as claimed in claim 1, wherein dopants are selected from Co and Ni.

### Claim 4 (depends on 1)

A process as claimed in claim 1, wherein said process is simple and economically viable combined sol-gel ball milling technique.

### Claim 5 (depends on 1)

A process as claimed in claim 1, wherein said process does not involve inert environment.

### Claim 6 (depends on 1)

High voltage cathode material prepared by the process as claimed in claim 1, wherein dopant provides high capacity and cycling stability up to 4.9V.

### Claim 7 (depends on 1)

High voltage cathode material prepared by the process as claimed in claim 1, wherein said cathode material delivers a discharge capacity in the range of 139 to 165 mAh/g at 0.2 to 0.05 C rate.

### Claim 8 (depends on 1)

High voltage cathode material prepared by the process as claimed in claim 1, wherein said cathode material shows high retention of capacity in the range of 95-98% at high rates up to 40 to 50 cycles.