# US 2013/0277614 A1 · Synthesis of water soluble non-toxic nanocrystalline quantum dots and uses thereof

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2013/0277614 A1
- Document ID: US20130277614A1
- Status: Published application
- Kind: A1
- Application number: 13/920,922
- Filed: 2013-06-18
- Published: 2013-10-24
- Earliest claimed: 2006-11-27
- Assignees: Drexel University
- Inventors: Wei-Heng Shih; Wan Y. Shih; Hui Li
- Web page: https://patentgrep.com/patent/US20130277614A1

## CPC

- C09K 11/565: {with zinc cadmium}
- B82Y 30/00: Nanotechnology for materials or surface science, e.g. nanocomposites
- C01G 9/08: Sulfides
- C01G 11/02: Sulfides
- C01P 2002/72: by d-values or two theta-values, e.g. as X-ray diagram
- C01P 2002/82: by IR- or Raman-data
- C01P 2002/84: by UV- or VIS- data
- C01P 2004/04: obtained by TEM, STEM, STM or AFM
- C01P 2004/64: Nanometer sized, i.e. from 1-100 nanometer
- C01P 2006/22: Rheological behaviour as dispersion, e.g. viscosity, sedimentation stability
- C01P 2006/60: Optical properties, e.g. expressed in CIELAB-values
- Y10T 428/2982: Particulate matter [e.g., sphere, flake, etc.]
- C09K: MATERIALS FOR MISCELLANEOUS APPLICATIONS, NOT PROVIDED FOR ELSEWHERE
- B82Y: SPECIFIC USES OR APPLICATIONS OF NANOSTRUCTURES; MEASUREMENT OR ANALYSIS OF NANOSTRUCTURES; MANUFACTURE OR TREATMENT OF NANOSTRUCTURES
- C01G: COMPOUNDS CONTAINING METALS NOT COVERED BY SUBCLASSES C01D OR C01F (metal hydrides {monoborane, diborane or addition complexes thereof} C01B6/00; salts of oxyacids of halogens C01B11/00; peroxides, salts or peroxyacids C01B15/00; thiosulfates, dithionites, polythionates C01B17/64; compounds containing selenium, or tellurium C01B19/00; binary compounds of nitrogen with metals C01B21/06; azides C01B21/08; {compounds containing nitrogen, other non-metals and metal C01B21/082}; metal amides C01B21/092; nitrites C01B21/50; {compounds of noble gases C01B23/0005}; phosphides C01B25/08; salts of oxyacids of phosphorus C01B25/16; carbides C01B32/90; compounds containing silicon C01B33/00; compounds containing boron C01B35/00; compounds having molecular sieve properties but not having base-exchange properties C01B37/00; compounds having molecular sieve and base-exchange properties, e.g. crystalline zeolites, C01B39/00; cyanides C01C3/08; salts of cyanamide C01C3/16; thiocyanates C01C3/20)
- C01P: INDEXING SCHEME RELATING TO STRUCTURAL AND PHYSICAL ASPECTS OF SOLID INORGANIC COMPOUNDS
- Y10T: TECHNICAL SUBJECTS COVERED BY FORMER US CLASSIFICATION

## Abstract

An economic, direct synthetic method for producing water soluble ZnS QDs that are ready for bioconjugation is provided. The method can produce aqueous ZnS QDs with emission wavelengths varying from 400 nm to 700 nm. Highly luminescent metal sulfide (MS) QDs are produced via an aqueous synthesis route. MS QDs are capped with thiol-containing charged molecules in a single step. The resultant MS QDs exhibit the distinctive excitonic photoluminescence desired of QDs and can be fabricated to avoid undesirable broadband emissions at higher wavelengths. The aqueous ZnS QDs are stable in biological fluids over a long period of time. In addition, non-toxic ZnS QDs have been produced with good photoluminescence properties.

## Claims

### Claim 1

A method for making quantum dots suitable for bioconjugation, said method comprising the steps of:
a. providing an aqueous solution of at least one metal salt, and at least one thiol-containing compound;
b. adjusting the pH of the aqueous solution of metal salt and thiol-containing compound to a pH of at least 8;
c. adding a water-soluble sulfide to the aqueous solution of at least one metal salt, and at least one thiol-containing compound to precipitate metal sulfide and form quantum dots; and
d. quenching to about a freezing point of water to form a suspension of quantum dots having an emission wavelength in the range of about 400-700 nm.

### Claim 2 (depends on 1)

The method as claimed in claim 1, further comprising the step of:
e. refluxing the quenched suspension for a period of time sufficient to improve the emission intensity of the quantum dots.

### Claim 3 (depends on 1)

The method as claimed in claim 1, wherein the at least one thiol-containing compound is 3-mercaptopropyltrimethoxysilane.

### Claim 4 (depends on 3)

The method as claimed in claim 3, wherein the metal sulfide is ZnS.

### Claim 5 (depends on 1)

The method as claimed in claim 1, wherein the water-soluble sulfide is employed in an amount of about 0.1 to about 10 times the stoichiometric amount of the water-soluble sulfide required to react with the metal salt.

### Claim 6 (depends on 1)

The method as claimed in claim 1, wherein the molar ratio of thiol groups to metal is from about 1 to about 8.

### Claim 7 (depends on 1)

The method as claimed in claim 1, wherein the process is performed in an atmosphere that is substantially free of oxygen.

### Claim 8 (depends on 1)

The method as claimed in claim 1, wherein the metal salt is zinc nitrate, the thiol-containing compound is 3-mercaptopropyltrimethoxysilane and the sulfide is sodium sulfide.

### Claim 9 (depends on 1)

The method as claimed in claim 1, further comprising the step of:
e. replacing at least some thiol-containing capping groups of the QDs formed in step d, with a different thiol containing group.

### Claim 10 (depends on 9)

The method as claimed in claim 9, wherein the thiol-containing capping groups of the QDs formed in step d are groups derived from 3-mercaptopropionic acid and the different thiol containing groups are groups derived from 3-mercaptopropyltrimethoxysilane.

### Claim at position 11

11-26. (canceled)

### Claim 27 (depends on 1)

The method as claimed in claim 1, wherein the quantum dots having an emission wavelength in the range of about 410-500 nm.

### Claim 28 (depends on 4)

The method as claimed in claim 4, wherein the quantum dots having an emission wavelength in the range of about 410-440 nm.

### Claim 29 (depends on 1)

The method as claimed in claim 1, wherein the metal salt is selected from the group consisting of Cd(NO3)2, Cd(ClO4)2, CdCl2, CdSO4, cadmium acetate, Zn(NO3)2, Zn(ClO4)2, ZnSO4, ZnCl2, zinc acetate, Mn(NO3)2, Mn(ClO4)2, MnSO4, MnCl2, manganese acetate, Pb(NO3)2, Pb(ClO4)2, PbSO4, PbCl2, lead acetate and mixtures thereof.

### Claim 30 (depends on 29)

The method as claimed in claim 29, wherein the water soluble sulfide is selected from the group consisting of as Na2S, K2S and H2S.

### Claim 31 (depends on 1)

The method as claimed in claim 1, wherein the water-soluble sulfide is employed in an amount of about 0.5 to about 5 times the stoichiometric amount of the water-soluble sulfide required to react with the metal salt.

### Claim 32 (depends on 1)

The method as claimed in claim 1, wherein the water-soluble sulfide is employed in an amount of about 0.8 to about 1.2 times the stoichiometric amount of the water-soluble sulfide required to react with the metal salt.

### Claim 33 (depends on 1)

The method as claimed in claim 1, wherein the at least one thiol-containing compound is selected from the group consisting of 4-aminothiophenol, mercaptosilanes, mercaptocarboxylic acids and mixtures thereof.

### Claim 34 (depends on 1)

The method as claimed in claim 1, wherein the at least one thiol-containing compound is selected from the group consisting of mercaptoacetic acid, mercaptopropionic acid, mercaptosuccinic acid, mercaptobenzoic acid, mercaptoundecanoic acid and mixtures thereof.

### Claim 35 (depends on 1)

The method as claimed in claim 1, wherein the at least one thiol-containing compound comprises 3-mercaptopropyltrimethoxysilane.

### Claim 36 (depends on 4)

The method as claimed in claim 4, wherein the metal salt, thiol-containing compound and sulfide are employed in an amount which provides a ratio of MPS:Zn:S of from about 0.125:4:1 to about 12:4:1.