# US 2013/0276940 A1 · High strength hot rolled steel sheet having excellent fatigue resistance and method for manufacturing the same

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2013/0276940 A1
- Document ID: US20130276940A1
- Status: Published application
- Kind: A1
- Application number: 13/820,660
- Filed: 2011-09-15
- Published: 2013-10-24
- Earliest claimed: 2010-09-17
- Assignees: Jfe Steel Corporation
- Inventors: Katsumi Nakajima; Hayato Saito; Yoshimasa Funakawa; Noriaki Moriyasu; Takayuki Murata
- Web page: https://patentgrep.com/patent/US20130276940A1

## CPC

- C22C 38/08: containing nickel {(C22C38/105 takes precedence)}
- C21D 8/0226: {Hot rolling}
- C21D 8/0263: {following hot rolling}
- C21D 9/46: for sheet metals
- C22C 38/001: {containing N}
- C22C 38/002: {containing In, Mg, or other elements not provided for in one single group C22C38/001 - C22C38/60}
- C22C 38/005: {containing rare earths, i.e. Sc, Y, Lanthanides}
- C22C 38/02: containing silicon
- C22C 38/04: containing manganese
- C22C 38/06: containing aluminium
- C22C 38/12: containing tungsten, tantalum, molybdenum, vanadium, or niobium
- C22C 38/14: containing titanium or zirconium
- C22C 38/16: containing copper
- C22C 38/18: containing chromium
- C22C 38/28: with titanium or zirconium
- C22C 38/40: with nickel
- C21D 2211/002: Bainite
- Y02P 10/20: Recycling
- C22C: ALLOYS (treatment of alloys C21D, C22F)
- C21D: MODIFYING THE PHYSICAL STRUCTURE OF FERROUS METALS; GENERAL DEVICES FOR HEAT TREATMENT OF FERROUS OR NON-FERROUS METALS OR ALLOYS; MAKING METAL MALLEABLE, e.g. BY DECARBURISATION OR TEMPERING (surface treatment of metallic material involving at least one process provided for in class C23 and at least one process covered by this subclass C23F17/00; unidirectional solidification of eutectic materials or unidirectional demixing of eutectoid materials C30B)
- Y02P: CLIMATE CHANGE MITIGATION TECHNOLOGIES IN THE PRODUCTION OR PROCESSING OF GOODS

## Abstract

A steel having a composition that includes C: 0.05 to 0.15%, Si: 0.2 to 1.2%, Mn: 1.0 to 2.0%, Al: 0.005 to 0.10%, N: 0.006% or less, and at least one selected from Ti: 0.03 to 0.13%, Nb: 0.02 to 0.10%, and V: 0.02 to 0.15% is subjected to rough rolling at a reduction of 80% or more and finish rolling at a finish rolling delivery temperature in the range of 800 to 950° C. The finish rolled sheet is subjected to cooling including cooling the finish rolled sheet from the finish rolling delivery temperature to a cooling end temperature in the range of 550 to 610° C. at an average cooling rate of 25° C./sec. or more and cooling the finish rolled sheet from the cooling end temperature of the previous process to a coiling temperature at an average cooling rate of 100° C./sec. or more.

## Claims

### Claim 1

A high strength hot rolled steel sheet having excellent fatigue resistance and a composition containing, in terms of mass %,
C: 0.05 to 0.15%, Si: 0.2 to 1.2%,
Mn: 1.0 to 2.0%, P: 0.03% or less,
S: 0.0030% or less, Al: 0.005 to 0.10%,
N: 0.006% or less,
and at least one selected from Ti: 0.03 to 0.13%, Nb: 0.02 to 0.10%, and V: 0.02 to 0.15%, the balance being Fe and unavoidable impurities, wherein a surface layer portion having a depth of 500 μm from the surface in the sheet thickness direction contains 50% or more of a bainite phase in terms of area fraction, the bainite phase having an average grain diameter of 5 μm or less; a sheet thickness center portion that extends from a position located at a depth of ¼ of the sheet thickness to a position located at a depth of ¾ of the sheet thickness contains 90% or more of a bainite phase in terms of area fraction, the bainite phase having an average grain diameter of 4 μm or less; and a tensile strength TS is 780 MPa or more.

### Claim 2 (depends on 1)

The high strength hot rolled steel sheet according to claim 1, wherein, in addition to the composition, at least one selected from Cr: 0.01 to 0.2%, Mo: 0.005 to 0.2%, Cu: 0.005 to 0.2%, and Ni: 0.005 to 0.2% is contained in terms of mass %.

### Claim 3 (depends on 1)

The high strength hot rolled steel sheet according to claim 1, wherein, in addition to the composition, B: 0.0002 to 0.003% is contained in terms of mass %.

### Claim 4 (depends on 1)

The high strength hot rolled steel sheet according to claim 1, wherein, in addition to the composition, one or both of Ca: 0.0005 to 0.03% and REM: 0.0005 to 0.03% are contained in terms of mass %.

### Claim 5

A method for manufacturing a high strength hot rolled steel sheet having excellent fatigue resistance, comprising heating a steel to 1100 to 1250° C., the steel having a composition that contains, in terms of mass %,
C: 0.05 to 0.15%, Si: 0.2 to 1.2%,
Mn: 1.0 to 2.0%, P: 0.03% or less,
S: 0.0030% or less, Al: 0.005 to 0.10%,
N: 0.006% or less,
and at least one selected from Ti: 0.03 to 0.13%, Nb: 0.02 to 0.10%, and V: 0.02 to 0.15%, the balance being Fe and unavoidable impurities, and performing hot rolling that includes rough rolling and finish rolling so as to prepare a hot rolled steel sheet, wherein a reduction during the rough rolling is 80% or more, a finish rolling delivery temperature of the finish rolling is set to a temperature in the range of 800 to 950° C., cooling is immediately started after completion of the finish rolling, the cooling is conducted in two stages including a first-stage cooling process of cooling the finish rolled sheet from the finish rolling delivery temperature to a first-stage cooling end temperature in the range of 550 to 610° C. at an average cooling rate of 25° C./sec. or more and a second-stage cooling process of cooling the finish rolled sheet from the first-stage cooling end temperature to a coiling temperature at an average cooling rate of 100° C./sec. or more, and coiling is conducted at a coiling temperature of 350 to 550° C.

### Claim 6 (depends on 5)

The method for manufacturing a high strength hot rolled steel sheet according to claim 5, wherein the steel contains at least one selected from Cr: 0.01 to 0.2%, Mo: 0.005 to 0.2%, Cu: 0.005 to 0.2%, and Ni: 0.005 to 0.2% in terms of mass % in addition to the composition.

### Claim 7 (depends on 5)

The method for manufacturing a high strength hot rolled steel sheet according to claim 5, wherein the steel contains B: 0.0002 to 0.003% in terms of mass % in addition to the composition.

### Claim 8 (depends on 5)

The method for manufacturing a high strength hot rolled steel sheet according to claim 5, wherein the steel contains one or both of Ca: 0.0005 to 0.03% and REM: 0.0005 to 0.03% in terms of mass % in addition to the composition.