# US 2013/0276587 A1 · Method for producing a coking additive by delayed coking

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2013/0276587 A1
- Document ID: US20130276587A1
- Status: Published application
- Kind: A1
- Application number: 13/701,229
- Filed: 2010-12-28
- Published: 2013-10-24
- Earliest claimed: 2010-06-01
- Inventors: Gennady Georgirvich Valyavin; Nikolai Ivanovich Vetoshkin; Victor Pavlovich Zaporin; Sergei Vital'evich Sukhov; Mikhail Vladimirovich Mamaev; Igor Viktorovich Bidilo; Konstantin Gennad'evich Valyavin; Mikhail Ivanovich Stukov; Vladimir Semenovich Zagainov
- Web page: https://patentgrep.com/patent/US20130276587A1

## CPC

- C10B 55/00: Coking mineral oils, bitumen, tar, and the like or mixtures thereof with solid carbonaceous material (cracking oils C10G)
- C10B 57/045: {containing mineral oils, bitumen, tar or the like or mixtures thereof}
- C10G 9/005: {Coking (in order to produce liquid products mainly)}
- C10B: DESTRUCTIVE DISTILLATION OF CARBONACEOUS MATERIALS FOR PRODUCTION OF GAS, COKE, TAR, OR SIMILAR MATERIALS (cracking oils C10G; underground gasification of minerals E21B43/295)
- C10G: CRACKING HYDROCARBON OILS; PRODUCTION OF LIQUID HYDROCARBON MIXTURES, e.g. BY DESTRUCTIVE HYDROGENATION, OLIGOMERISATION, POLYMERISATION (cracking to hydrogen or synthesis gas C01B; cracking or pyrolysis of hydrocarbon gases to individual hydrocarbons or mixtures thereof of definite or specified constitution C07C; cracking to cokes C10B); RECOVERY OF HYDROCARBON OILS FROM OIL-SHALE, OIL-SAND, OR GASES; REFINING MIXTURES MAINLY CONSISTING OF HYDROCARBONS; REFORMING OF NAPHTHA; MINERAL WAXES

## Abstract

This invention relates to the field of oil refining and, in particular, to a delayed coking process that produces coke with a volatile substances content of 15-25% for use as a coking additive in a coal coking charge in the production of metallurgical coke. The invention is directed towards increasing the content of volatile substances in coke and increasing the efficiency of a plant. The method comprises preheating a primary raw material, mixing the latter with recycle in a tank in order to form a secondary raw material, heating the secondary raw material to 455-470° C. and supplying the latter to a coking chamber, and coking to form a coking additive. It is expedient to feed an antifoaming additive into the coking chamber 3-5 hours before coking is finished. It is preferable to feed in the antifoaming addition agent at two-four points around the perimeter of the coking chamber.

## Claims

### Claim at position 1

1-3. (canceled)

### Claim 4

A method of producing a coking additive in delayed coking, comprising:
heating a primary charge to 270-330° C.;
mixing the primary charge with a recirculate in a tank to form a secondary charge;
heating the secondary charge and introducing it into a coking chamber; and
coking to form a target product;
wherein the secondary charge is introduced into the coking chamber at 455-470° C.

### Claim 5 (depends on 4)

The method according to claim 4, further comprising introducing an anti-foaming dope into the coke chamber 3-5 hours before the end of coking.

### Claim 6 (depends on 5)

The method according to claim 5, wherein the anti-foaming dope is introduced into 2-4 areas around a perimeter of the coking chamber.