# US 2013/0276480 A1 · Method for producing tio2-sio2 glass body, method for heat-treating tio2-sio2 glass body, tio2-sio2 glass body, and optical base for euvl

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2013/0276480 A1
- Document ID: US20130276480A1
- Status: Published application
- Kind: A1
- Application number: 13/922,908
- Filed: 2013-06-20
- Published: 2013-10-24
- Earliest claimed: 2009-05-18
- Assignees: Asahi Glass Company, Limited
- Applicants: Asahi Glass Company, Limited
- Inventors: Akio KOIKE; Takahiro Mitsumori; Yasutomi Iwahashi; Tomonori Ogawa
- Web page: https://patentgrep.com/patent/US20130276480A1

## CPC

- C03B 25/00: Annealing glass products
- B82Y 10/00: Nanotechnology for information processing, storage or transmission, e.g. quantum computing or single electron logic
- B82Y 40/00: Manufacture or treatment of nanostructures
- C03B 19/1453: {Thermal after-treatment of the shaped article, e.g. dehydrating, consolidating, sintering}
- G03F 1/24: Reflection masks; Preparation thereof
- C03B 2201/12: doped with fluorine (C03B2201/14 takes precedence)
- C03B 2201/23: doped with hydroxyl groups
- C03B 2201/42: doped with titanium
- Y02P 40/57: Improving the yield, e-g- reduction of reject rates
- Y10T 428/24355: Continuous and nonuniform or irregular surface on layer or component [e.g., roofing, etc.]
- C03B: MANUFACTURE, SHAPING, OR SUPPLEMENTARY PROCESSES
- B82Y: SPECIFIC USES OR APPLICATIONS OF NANOSTRUCTURES; MEASUREMENT OR ANALYSIS OF NANOSTRUCTURES; MANUFACTURE OR TREATMENT OF NANOSTRUCTURES
- G03F: PHOTOMECHANICAL PRODUCTION OF TEXTURED OR PATTERNED SURFACES, e.g. FOR PRINTING, FOR PROCESSING OF SEMICONDUCTOR DEVICES; MATERIALS THEREFOR; ORIGINALS THEREFOR; APPARATUS SPECIALLY ADAPTED THEREFOR; (phototypographic composing devices B41B; photosensitive materials or processes for photographic purposes G03C; electrophotography, sensitive layers or processes therefor G03G)
- Y02P: CLIMATE CHANGE MITIGATION TECHNOLOGIES IN THE PRODUCTION OR PROCESSING OF GOODS
- Y10T: TECHNICAL SUBJECTS COVERED BY FORMER US CLASSIFICATION

## Abstract

The present invention relates to a process for production of a TiO2—SiO2 glass body, comprising: a step of, when an annealing point of a TiO2—SiO2 glass body after transparent vitrification is taken as T1 (° C.), heating the glass body after transparent vitrification at a temperature of T1+400° C. or more for 20 hours or more; and a step of cooling the glass body after the heating step up to T1−400 (° C.) from T1 (° C.) in an average temperature decreasing rate of 10° C./hr or less.

## Claims

### Claim 1

(canceled)

### Claim 2

A process for production of a TiO2—SiO2 glass body, comprising:
a step of, when an annealing point of a TiO2—SiO2 glass body after transparent vitrification is taken as T1 (° C.), heating the glass body after transparent vitrification at a temperature of T1+400° C. or more for 20 hours or more; and
a step of holding the glass body after the heating step in a temperature region of from T1−90 (° C.) to T1−220 (° C.) for 120 hours or more.

### Claim 3 (depends on 2)

The process for production of a TiO2—SiO2 glass body according to claim 2, wherein a step of cooling the glass body after the heating step up to T1−220 (° C.) from T1−90 (° C.) in an average temperature decreasing rate of 1° C./hr or less is carried out as the step of holding the glass body in a temperature region of from T1−90 (° C.) to T1−220 (° C.) for 120 hours or more.

### Claim at position 4

4-8. (canceled)

### Claim 9

A heat treatment process of a TiO2—SiO2 glass body, comprising carrying out a heat treatment containing: a step of, when an annealing point of a TiO2—SiO2 glass body to be heat-treated is taken as T1 (° C.), heating the TiO2—SiO2 glass body, which has standard deviation (dev [σ]) of stress caused by striae is 0.1 MPa or less, at a temperature of T1+400° C. or more for 20 hours or more; and a step of holding the glass body after the heating step in a temperature region of from T1−90 (° C.) to T1−220 (° C.) for 120 hours or more, thereby decreasing the standard deviation (dev [σ]) of stress 0.01 MPa or more lower than that before carrying out the heat treatment.

### Claim 10

(canceled)

### Claim 11

A heat treatment process of a TiO2—SiO2 glass body, comprising carrying out a heat treatment containing: a step of, when an annealing point of a TiO2—SiO2 glass body to be heat-treated is taken as T1 (° C.), heating the TiO2—SiO2 glass body, which has a difference (Δσ) between the maximum value and the minimum value of stress caused by striae is 0.5 MPa or less, at a temperature of T1+400° C. or more for 20 hours or more after transparent vitrification; and a step of holding the glass body after the heating step in a temperature region of from T1−90 (° C.) to T1−220 (° C.) for 120 hours or more, thereby decreasing the difference (Δσ) between the maximum value and the minimum value of stress 0.05 MPa or more lower than that before carrying out the heat treatment.

### Claim 12 (depends on 9)

The heat treatment process of a TiO2—SiO2 glass body according to claim 9, wherein a step of cooling the glass body after the heating step up to T1−220 (° C.) from T1−90 (° C.) in an average temperature decreasing rate of 1° C./hr or less is carried out as the step of holding the glass body in a temperature region of from T1−90 (° C.) to T1−220 (° C.) for 120 hours or more.

### Claim at position 9

13-19. (canceled)

### Claim 20 (depends on 11)

The heat treatment process of a TiO2—SiO2 glass body according to claim 11, wherein a step of cooling the glass body after the heating step up to T1−220 (° C.) from T1−90 (° C.) in an average temperature decreasing rate of 1° C./hr or less is carried out as the step of holding the glass body in a temperature region of from T1−90 (° C.) to T1−220 (° C.) for 120 hours or more.