# US 2013/0274512 A1 · Catalysts Conversion Of Hydroxypropionic Acid Or Its Derivatives To Acrylic Acid Or Its Derivatives

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2013/0274512 A1
- Document ID: US20130274512A1
- Status: Published application
- Kind: A1
- Application number: 13/760,472
- Filed: 2013-02-06
- Published: 2013-10-17
- Earliest claimed: 2012-04-11
- Assignees: The Procter & Gamble Company
- Applicants: The Procter & Gamble Company
- Inventors: Janette Villalobos; Juan Estaban Velasquez; Jane Ellen Godlewski; Dimitris Ioannis Collias
- Web page: https://patentgrep.com/patent/US20130274512A1

## CPC

- B01J 27/1806: {with alkaline or alkaline earth metals}
- A61F 13/534: having an inhomogeneous composition through the thickness of the pad (A61F13/538, A61F13/539 take precedence)
- B01J 27/16: containing oxygen {, i.e. acids, anhydrides and their derivates with N, S, B or halogens without carriers or on carriers based on C, Si, Al or Zr; also salts of Si, Al and Zr}
- B01J 27/1811: {with gallium, indium or thallium}
- B01J 27/1817: {with copper, silver or gold}
- B01J 27/1853: {with iron, cobalt or nickel}
- B01J 27/1856: {with platinum group metals}
- B01J 27/186: with arsenic, antimony, bismuth, vanadium, niobium, tantalum, polonium, chromium, molybdenum, tungsten, manganese, technetium or rhenium
- B01J 27/187: with manganese, technetium or rhenium
- B01J 27/188: with chromium, molybdenum, tungsten or polonium
- B01J 27/195: with vanadium, niobium or tantalum
- B01J 27/198: Vanadium
- B01J 27/25: Nitrates
- B01J 35/40: characterised by dimensions, e.g. grain size (in a colloidal state B01J35/23; crystallite size B01J35/77)
- B01J 37/0036: {Grinding}
- B01J 37/04: Mixing {(B01J37/0009, B01J37/0018 take precedence)}
- B01J 37/08: Heat treatment {(B01J37/0009, B01J37/0018 take precedence)}
- C07C 51/09: from carboxylic acid esters or lactones
- C07C 51/377: by splitting-off hydrogen or functional groups; by hydrogenolysis of functional groups {(C07C51/36 - C07C51/373 take precedence)}
- C07C 51/44: by distillation
- C07C 51/48: by liquid-liquid treatment
- C07C 57/04: Acrylic acid; Methacrylic acid
- C08F 2/10: Aqueous solvent
- A61F 13/53: characterised by the absorbing medium (A61F13/20 takes precedence)
- A61F 2013/530489: {being randomly mixed in with other material}
- A61F 2013/530496: {being fixed to fibres}
- B01J: CHEMICAL OR PHYSICAL PROCESSES, e.g. CATALYSIS OR COLLOID CHEMISTRY; THEIR RELEVANT APPARATUS
- A61F: FILTERS IMPLANTABLE INTO BLOOD VESSELS; PROSTHESES; DEVICES PROVIDING PATENCY TO, OR PREVENTING COLLAPSING OF, TUBULAR STRUCTURES OF THE BODY, e.g. STENTS; ORTHOPAEDIC, NURSING OR CONTRACEPTIVE DEVICES; FOMENTATION; TREATMENT OR PROTECTION OF EYES OR EARS; BANDAGES, DRESSINGS OR ABSORBENT PADS; FIRST-AID KITS (dental prosthetics A61C)
- C07C: ACYCLIC OR CARBOCYCLIC COMPOUNDS
- C08F: MACROMOLECULAR COMPOUNDS OBTAINED BY REACTIONS ONLY INVOLVING CARBON-TO-CARBON UNSATURATED BONDS

## Abstract

Methods for catalytically dehydrating hydroxypropionic acid, hydroxypropionic acid derivatives, or mixtures thereof to acrylic acid, acrylic acid derivatives, or mixtures thereof with high yield and selectivity and without significant conversion to undesired side products, such as, acetaldehyde, propionic acid, and acetic acid, are provided. The catalysts are mixed condensed phosphates.

## Claims

### Claim 1

A method of making acrylic acid, acrylic acid derivatives, or mixtures thereof comprising contacting a stream comprising hydroxypropionic acid, hydroxypropionic acid derivatives, or mixtures thereof with a catalyst comprising:
(a) at least one condensed phosphate anion selected from the group consisting of formulae (I), (II), and (III),
[PnO3n+1](n+2)− (I)
[PnO3n]n− (II)
[P(2m+n)O(5m+3n)]n− (III)
wherein n is at least 2 and m is at least 1; and
(b) at least two different cations,
wherein the catalyst is essentially neutrally charged; and further, wherein the molar ratio of phosphorus to said at least two different cations is between about 0.7 and about 1.7, whereby acrylic acid, acrylic acid derivatives, or mixtures thereof are produced as a result of said stream being contacted with said catalyst.

### Claim 2 (depends on 1)

The method of claim 1, wherein said stream further comprises:
(a) diluent; and
(b) inert gas selected from the group consisting of air, nitrogen, helium, argon, carbon dioxide, carbon monoxide, steam, and mixtures thereof.

### Claim 3 (depends on 2)

The method of claim 2, wherein said stream is in the form of a gaseous mixture when contacting the catalyst.

### Claim 4 (depends on 3)

The method of claim 3, wherein said diluent is water.

### Claim 5 (depends on 1)

The method of claim 1, wherein said hydroxypropionic acid is lactic acid.

### Claim 6 (depends on 5)

The method of claim 5, wherein the acrylic acid selectivity from said lactic acid is at least about 50%.

### Claim 7 (depends on 5)

The method of claim 5, wherein the acrylic acid selectivity from said lactic acid is at least about 80%.

### Claim 8 (depends on 5)

The method of claim 5, wherein the propionic acid selectivity from said lactic acid is less than about 5%.

### Claim 9 (depends on 5)

The method of claim 5, wherein the propionic acid selectivity from said lactic acid is less than about 1%.

### Claim 10 (depends on 5)

The method of claim 5, wherein the conversion of said lactic acid is more than about 50%.

### Claim 11 (depends on 5)

The method of claim 5, wherein the conversion of said lactic acid is more than about 80%.

### Claim 12 (depends on 1)

The method of claim 1, wherein said stream contacts said catalyst at a temperature of about 150° C. to about 500° C.

### Claim 13 (depends on 5)

The method of claim 5, wherein said lactic acid contacts said catalyst at a temperature of about 300° C. to about 450° C.

### Claim 14 (depends on 3)

The method of claim 3, wherein said hydroxypropionic acid, hydroxypropionic acid, or mixtures thereof are present in an amount between about 1 mol % and about 10 mol %, based on the total moles of said stream.

### Claim 15 (depends on 3)

The method of claim 3, wherein said stream contacts said catalyst at a GHSV between about 720 h−1 and about 36,000 h−1.

### Claim 16 (depends on 15)

The method of claim 15, wherein said stream contacts said catalyst at a GHSV of about 3,600 h−1.

### Claim 17 (depends on 3)

The method of claim 3, wherein said stream contacts said catalyst at a pressure between about 0 psig and about 550 psig.

### Claim 18 (depends on 3)

The method of claim 3, wherein said stream contacts said catalyst at a pressure of about 360 psig.

### Claim 19 (depends on 1)

The method of claim 1, wherein said stream is contacted with said catalyst in a reactor having an interior surface comprising material selected from the group consisting of quartz, borosilicate glass, silicon, hastelloy, inconel, manufactured sapphire, stainless steel, and mixtures thereof.

### Claim 20 (depends on 19)

The method of claim 19, wherein said material is quartz or borosilicate glass.

### Claim 21 (depends on 1)

The method of claim 1, wherein said cations comprise:
(a) at least one monovalent cation; and
(b) at least one polyvalent cation.

### Claim 22 (depends on 21)

The method of claim 21, wherein said monovalent cation is selected from the group consisting of H+, Li+, Na+, K+, Rb+, Cs+, and mixtures thereof.

### Claim 23 (depends on 21)

The method of claim 21, wherein said polyvalent cation is selected from the group consisting of divalent cations, trivalent cations, tetravalent cations, pentavalent cations, and mixtures thereof.

### Claim 24 (depends on 23)

The method of claim 23, wherein said polyvalent cation is selected from the group consisting of Be2+, Mg2+, Ca2+, Sr2+, Ba2+, Mn2+, Fe2+, Co2+, Ni2+, Cu2+, Zn2+, Cd2+, Sn2+, Pb2+, Ti3+, Cr3+, Mn3+, Fe3+, Al3+, Ga3+, Y3+, In3+, Sb3+, Bi3+, Si4+, Ti4+, V4+, Ge4+, Mo4+, Pt4+, V5+, Nb5+, Sb5+, and mixtures thereof.

### Claim 25 (depends on 1)

The method of claim 1, wherein said condensed phosphate anions are described by formulae (I) and (II).

### Claim 26 (depends on 25)

The method of claim 25, wherein said catalyst comprises:
(a) Ba2−x−sK2xH2sP2O7 or Ca2−x−sK2xH2sP2O7 or Mn1−x−sK1+3xH3sP2O7 or Mn1−x−sK2+2xH2sP2O7; and
(b) (KPO3)n;
wherein x and s are greater or equal to 0 and less than about 0.5 and n is a positive integer.

### Claim 27 (depends on 1)

The method of claim 1, wherein the molar ratio of phosphorus to the cations in said catalyst is between about 0.8 and about 1.3.

### Claim 28 (depends on 1)

The method of claim 1, wherein the molar ratio of phosphorus to the cations in said catalyst is about 1.

### Claim 29 (depends on 28)

The method of claim 28, wherein said cations comprise:
(a) H+, Li+, Na+, K+, Rb+, Cs+, and mixtures thereof; and
(b) Be2+, Mg2+, Ca2+, Sr2+, Ba2+, Mn2+, Fe2+, Co2+, Ni2+, Cu2+, Zn2+, Cd2+, Sn2+, Pb2+, Ti3+, Cr3+, Mn3+, Fe3+, Al3+, Ga3+, Y3+, In3+, Sb3+, Bi3+, Si4+, Ti4+, V4+, Ge4+, Mo4+, Pt4+, V5+, Nb5+, Sb5+, and mixtures thereof.

### Claim 30 (depends on 1)

The method of claim 1, wherein said catalyst includes an inert support that is constructed of a material comprising silicates, aluminates, carbons, metal oxides, and mixtures thereof.

### Claim 31 (depends on 1)

The method of claim 1, wherein said catalyst is prepared by a method comprising mixing and heating at least two different phosphorus containing compounds, wherein each said compound is described by one of the formulae (IV) to (XXV), or any of the hydrated forms of said formulae:
MIy(H3−yPO4) (IV)
MIIy(H3−yPO4)2 (V)
MIIy(H3−yPO4)3 (VI)
MIVy(H3−yPO4)4 (VII)
(NH4)y(H3−yPO4) (VIII)
MIIa(OH)b(PO4)f (IX)
MIIId(OH)e(PO4)f (X)
MIIMIPO4 (XI)
MIIIMI3(PO4)2 (XII)
MIV2MI(PO4)3 (XIII)
MIzR4−zP2O7 (XIV)
MIIwH(4−2v)P2O7 (XV)
MIVP2O7 (XVI)
(NH4)zH4−zP2O7 (XVII)
MIIIMIP2O7 (XVIII)
MIHw(PO3)(1+w) (XIX)
MIIHw(PO3)(2+w) (XX)
MIIIHw(PO3)(3+w) (XXI)
MIVHw(PO3)(4+w) (XXII)
MIIgMIh(PO3)i (XXIII)
MIIIjMIk(PO3)l (XXIV)
P2O5 (XXV)
wherein MI is a monovalent cation; wherein MII is a divalent cation; wherein MIII is a trivalent cation; wherein MIV is a tetravalent cation; wherein y is 0, 1, 2, or 3; wherein z is 0, 1, 2, 3, or 4; wherein v is 0, 1, or 2; wherein w is 0 or any positive integer; and wherein a, b, c, d, e, f, g, h, i, j, k, and l are any positive integers, such that the equations: 2a=b+3c, 3d=e+3f, i=2g+h, and l=3j+k are satisfied.

### Claim 32 (depends on 31)

The method of claim 31, wherein said method of preparation of said catalyst further comprises mixing an inert support with said phosphorus containing compounds either before, during, or after said mixing and heating of the phosphorus containing compounds, wherein said inert support comprises silicates, aluminates, carbons, metal oxides, and mixtures thereof.

### Claim 33 (depends on 1)

The method of claim 1, wherein said catalyst is prepared by a method comprising mixing and heating:
(a) at least one phosphorus containing compound, wherein each said compound is described by one of the formulae (IV) to (XXV), or any of the hydrated forms of said formulae:
MIy(H3−yPO4) (IV)
MIIy(H3−yPO4)2 (V)
MIIIy(H3−yPO4)3 (VI)
MIVy(H3−yPO4)4 (VII)
(NH4)y(H3−yPO4) (VIII)
MIIa(OH)b(PO4)c (IX)
MIIId(OH)e(PO4)f (X)
MIIMIPO4 (XI)
MIIIMI3(PO4)2 (XII)
MIV2MI(PO4)3 (XIII)
MIzR4−zP2O7 (XIV)
MIIwH(4−2v)P2O7 (XV)
MIVP2O7 (XVI)
(NH4)zH4−zP2O7 (XVII)
MIIIMIP2O7 (XVIII)
MIHw(PO3)(1+w) (XIX)
MIIHw(PO3)(2+w) (XX)
MIIIHw(PO3)(3+w) (XXI)
MIVHw(PO3)(4+w) (XXII)
MIIgMIh(PO3)i (XXIII)
MIIIjMIk(PO3)l (XXIV)
P2O5 (XXV)
wherein MI is a monovalent cation; wherein MII is a divalent cation; wherein MIII is a trivalent cation; wherein MIV is a tetravalent cation; wherein y is 0, 1, 2, or 3; wherein z is 0, 1, 2, 3, or 4; wherein v is 0, 1, or 2; wherein w is 0 or any positive integer; and wherein a, b, c, d, e, f, g, h, i, j, k, and l are any positive integers, such that the equations: 2a=b+3c, 3d=e+3f, i=2g+h, and l=3j+k are satisfied; and
(b) at least one non-phosphorus containing compound selected from the group consisting of nitrate salts, carbonate salts, acetate salts, metal oxides, chloride salts, sulfate salts, and metal hydroxides, wherein each said compound is described by one of the formulae (XXVI) to (XL), or any of the hydrated forms of said formulae.
MINO3 (XXVI)
MII(NO3)2 (XXVII)
MIII(NO3)3 (XXVIII)
MI2CO3 (XXIX)
MIICO3 (XXX)
MIII2(CO3)3 (XXXI)
(CH3COO)MI (XXXII)
(CH3COO)2MII (XXXIII)
(CH3COO)3MIII (XXXIV)
(CH3COO)4MIV (XXXV)
MI2O (XXXVI)
MIIO (XXXVII)
MIII2O3 (XXXVIII)
MIVO2 (XXXIX)
MICl (XXXX)
MIIICl2 (XXXXI)
MIIICl3 (XXXXII)
MIVCl4 (XXXXIII)
MI2SO4 (XXXXIV)
MIISO4 (XXXXV)
MIII2(SO4)3 (XXXXVI)
MIV(SO4)2 (XXXXVII)
MIOH (XXXVIII)
MII(OH)2 (XXXIX)
MIII(OH)3 (XL).

### Claim 34 (depends on 33)

The method of claim 33, wherein said method of preparation of said catalyst further comprises mixing an inert support with said phosphorus containing compounds and said non-phosphorus containing compounds wherein the inert support is mixed either before, during, or after said mixing and heating of the compounds, and wherein said inert support comprises silicates, aluminates, carbons, metal oxides, and mixtures thereof.

### Claim 35

A method of making acrylic acid comprising contacting:
(a) a gaseous stream comprising:
(i) lactic acid,
(ii) water, and
(iii) nitrogen,
wherein said lactic acid is present in an amount of about 2.5 mol % and wherein said water is present in an amount of about 50 mol % based on the total moles of said gaseous stream, with
(b) a catalyst comprising:
(i) Ba2−x−sK2xH2sP2O7; and
(ii) (KPO3)n;
wherein x and s are greater or equal to 0 and less than about 0.5 and n is a positive integer, wherein, said contacting of said gaseous stream with said catalyst is performed at a temperature of about 300° C. to about 450° C., at a GHSV of about 3,600 h−1 and at a pressure of about 360 psig, in a reactor having an interior surface comprising material selected from the group consisting of quartz and borosilicate glass, whereby acrylic acid is produced as a result of said lactic acid being contacted with said catalyst.

### Claim 36

A method of making acrylic acid comprising contacting:
(a) a gaseous stream comprising:
(i) lactic acid,
(ii) water, and
(iii) nitrogen,
wherein said lactic acid is present in an amount of about 2.5 mol % and wherein said water is present in an amount of about 50 mol % based on the total moles of said gaseous stream, with
(b) a catalyst prepared by a method comprising the following steps:
(i) combining a phosphorus containing compound, a nitrate salt, phosphoric acid, and water to form a wet mixture, wherein the molar ratio between phosphorus and the cations in both said phosphorus containing compound and said nitrate salt is about 1;
(ii) calcining said wet mixture stepwise at about 50° C., about 80° C., about 120° C., and about 450° C. to about 550° C. to produce a dried solid; and
(iii) grinding and sieving said dried solid to about 100 μm to about 200 μm, to produce said catalyst, and
wherein, said contacting of said gaseous stream with said catalyst is performed at a temperature of about 300° C. to about 450° C., at a GHSV of about 3,600 h−1 and at a pressure of about 360 psig, in a reactor having an interior surface comprising material selected from the group consisting of quartz and borosilicate glass, whereby acrylic acid is produced as a result of said lactic acid being contacted with said catalyst.

### Claim 37 (depends on 36)

The method of claim 36, wherein said combining step is followed by heating said wet mixture to about 80° C. with stirring until near dryness to form a wet solid, and further, wherein said wet mixture of step (b) is a wet solid.

### Claim 38 (depends on 37)

The method of claim 37, wherein said phosphorus containing compound is K2HPO4, wherein said nitrate salt is Ba(NO3)2, and wherein the molar ratio of Ba(NO3)2, K2HPO4, and H3PO4 is about 3:1:4.

### Claim 39 (depends on 37)

The method of claim 37, wherein said phosphorus containing compound is K2HPO4 and said nitrate salt is Mn(NO3)2.4H2O, and wherein the molar ratio of Mn(NO3)2.4H2O, K2HPO4, and H3PO4 is about 1:1.5:2.

### Claim 40 (depends on 36)

The method of claim 36, wherein said phosphorus containing compound is MnPO4.qH2O and said nitrate salt is KNO3, and wherein the molar ratio of MnPO4.qH2O, KNO3, and H3PO4 is about 0.3:1:1, on an anhydrous basis.

### Claim 41 (depends on 36)

The method of claim 36, wherein said phosphorus containing compound is Ca2P2O7 and said nitrate salt is KNO3, and wherein the molar ratio of Ca2P2O7, KNO3, and H3PO4 is about 1.6:1:1.

### Claim 42

A method of making acrylic acid comprising contacting:
(a) a gaseous stream comprising:
(i) lactic acid,
(ii) water, and
(iii) nitrogen,
wherein said lactic acid is present in an amount of about 2.5 mol % and said water is present in an amount of about 50 mol % based on the total moles of said gaseous stream, with
(b) a catalyst prepared by a method comprising the following steps:
(i) combining Ca2P2O7 and KH2PO4 in a molar ratio of about 3:1 to form a solid mixture; and
(ii) calcining said solid mixture stepwise at about 50° C., about 80° C., about 120° C., and about 450° C. to about 550° C., to produce said catalyst; and
wherein, said contacting of said gaseous stream with said catalyst is performed at a temperature of about 300° C. to about 450° C., at a GHSV of about 3,600 h−1 and at a pressure of about 360 psig, in a reactor having an interior surface comprising material selected from the group consisting of quartz and borosilicate glass, whereby acrylic acid is produced as a result of said lactic acid being contacted with said catalyst.