# US 2013/0273801 A1 · Non-Woven Polymeric Webs

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2013/0273801 A1
- Document ID: US20130273801A1
- Status: Published application
- Kind: A1
- Application number: 13/916,194
- Filed: 2013-06-12
- Published: 2013-10-17
- Earliest claimed: 2008-11-25
- Assignees: E. I. Du Pont de Nemours and Company
- Applicants: E I Du Pont De Nemours and Company
- Inventors: PATRICK HENRY YOUNG
- Web page: https://patentgrep.com/patent/US20130273801A1

## CPC

- D04H 3/16: with bonds between thermoplastic filaments produced in association with filament formation, e.g. immediately following extrusion
- D01D 5/0069: {characterised by the spinning section, e.g. capillary tube, protrusion or pin}
- D01D 5/18: by means of rotating spinnerets
- D04H 1/43838: {Ultrafine fibres, e.g. microfibres}
- D04H 1/72: the fibres being randomly arranged
- D04H 3/03: at random
- Y10T 442/614: Strand or fiber material specified as having microdimensions [i.e., microfiber]
- Y10T 442/626: Microfiber is synthetic polymer
- Y10T 442/68: Melt-blown nonwoven fabric
- Y10T 442/681: Spun-bonded nonwoven fabric
- D04H: MAKING TEXTILE FABRICS, e.g. FROM FIBRES OR FILAMENTARY MATERIAL (weaving D03; knitting D04B; braiding D04C; net-making D04G; sewing D05B; tufting D05C; finishing non-woven fabrics D06); FABRICS MADE BY SUCH PROCESSES OR APPARATUS, e.g. FELTS, NON-WOVEN FABRICS; COTTON-WOOL; WADDING {; NON-WOVEN FABRICS FROM STAPLE FIBRES, FILAMENTS OR YARNS, BONDED WITH AT LEAST ONE WEB-LIKE MATERIAL DURING THEIR CONSOLIDATION}(non-woven fabrics having an intermediate or external layer of a different kind, e.g. of woven fabric, B32B)
- D01D: MECHANICAL METHODS OR APPARATUS IN THE MANUFACTURE OF ARTIFICIAL FILAMENTS, THREADS, FIBRES, BRISTLES OR RIBBONS
- Y10T: TECHNICAL SUBJECTS COVERED BY FORMER US CLASSIFICATION

## Abstract

A non-woven web, comprising one or more polymeric fibers, wherein the number-average fiber diameter distribution of said one or more polymeric fibers conforms to a Johnson unbounded distribution. Non-woven webs comprising such polymeric fibers are rendered with mean-flow pore size and porosity desirable for specific filtration applications such as hepafiltration.

## Claims

### Claim 1

A non-woven web, comprising one or more polymeric fibers, wherein said one or more polymeric fibers have a number-average fiber diameter distribution that conforms to a Johnson unbounded distribution.

### Claim 2 (depends on 1)

The non-woven web as recited in claim 1, wherein said one or more polymeric fibers are produced from the same spinning head.

### Claim 3 (depends on 1)

The non-woven web as recited in claim 1, wherein the number-average mean fiber size of said one or more polymeric fibers is less than 1,000 nm.

### Claim 4 (depends on 1)

The non-woven web as recited in claim 1, wherein said non-woven web has a Frazier porosity in the range of from about 5 ft3.ft-2min−1 (0.0254 m3.m−2.sec−1) to about 100 ft3.ft-2min−1 (0.508 m3.m−2.sec−1) at a basis weight of approximately 25 g.m−2.

### Claim 5 (depends on 1)

The non-woven web as recited in claim 1, wherein said non-woven web flux barrier properties is greater than 0.01 at a basis weight of ˜25 g.m−2.

### Claim 6

A non-woven web, comprising one or more fibers, wherein said non-woven web is prepared by a method comprising the steps of:
(i) supplying a spinning melt or solution of at least one thermoplastic polymer to an inner spinning surface of a rotating distribution disc having a forward-surface, fiber-discharge edge;
(ii) issuing said spinning melt or solution along said inner spinning surface of said rotating distribution disc so as to distribute said spinning melt or solution into a thin film and toward the forward-surface, fiber-discharge edge; and
(iii) discharging separate molten or solution polymer fiber streams from said forward-surface, discharge-edge into a gas stream to attenuate the fiber stream to produce polymeric fibers that have a mean fiber diameter less than about 1,000 nm;
wherein said polymer melt or solution has a viscosity that is above a minimum effective viscosity for producing said polymeric fibers with the number-average fiber diameter distribution of said polymeric fibers conforms to a Johnson unbounded distribution; and/or
wherein said polymer melt or solution has a flow-rate that is below a maximum effective flow-rate for producing said polymeric fibers with the number-average fiber diameter distribution of said polymeric fibers conforms to a Johnson unbounded distribution; and/or
wherein said polymer solution has a concentration that is above a minimum effective concentration for producing said polymeric fibers with the number-average fiber diameter distribution of said polymeric fibers conforms to a Johnson unbounded distribution; and/or
wherein the rotational speed of said rotating distribution disc is below a maximum effective rotational speed for producing said polymeric fibers with the number-average fiber diameter distribution of said polymeric fibers conforms to a Johnson unbounded distribution.