# US 2013/0273377 A1 · Method of making heat treated coated article using tco and removable protective film

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2013/0273377 A1
- Document ID: US20130273377A1
- Status: Published application
- Kind: A1
- Application number: 13/448,733
- Filed: 2012-04-17
- Published: 2013-10-17
- Earliest claimed: 2012-04-17
- Assignees: Guardian Industries Corp.
- Inventors: Vijayen S. VEERASAMY
- Web page: https://patentgrep.com/patent/US20130273377A1

## CPC

- C03C 17/2453: {Coating containing SnO2}
- B05D 3/068: {using ionising radiations (gamma, X, electrons)}
- C03C 17/3423: {at least one of the coatings comprising a suboxide}
- C03C 17/3429: {at least one of the coatings being a non-oxide coating}
- C03C 17/3435: {comprising a nitride, oxynitride, boronitride or carbonitride}
- C03C 17/3441: {comprising carbon, a carbide or oxycarbide}
- H10F 77/30: Coatings (arrangements for preventing damage to photovoltaic cells caused by corpuscular radiation H10F77/80)
- H10F 77/955: {for photovoltaic devices}
- B05D 3/0254: {After-treatment}
- B05D 5/12: to obtain a coating with specific electrical properties
- B05D 7/56: {Three layers or more}
- B32B 9/00: Layered products comprising a {layer of a} particular substance not covered by groups B32B11/00 - B32B29/00
- B32B 17/06: comprising glass as the main or only constituent of a layer, next to another layer of a specific {material}
- C03C 2217/231: In2O3/SnO2
- C03C 2217/948: Layers comprising indium tin oxide [ITO]
- C03C 2218/355: Temporary coating
- C03C 2218/365: Coating different sides of a glass substrate
- H10F 77/20: Electrodes
- Y02E 10/50: Photovoltaic [PV] energy
- C03C: CHEMICAL COMPOSITION OF GLASSES, GLAZES OR VITREOUS ENAMELS; SURFACE TREATMENT OF GLASS; SURFACE TREATMENT OF FIBRES OR FILAMENTS MADE FROM GLASS, MINERALS OR SLAGS; JOINING GLASS TO GLASS OR OTHER MATERIALS
- B05D: PROCESSES FOR APPLYING FLUENT MATERIALS TO SURFACES, IN GENERAL (conveying articles or workpieces through baths of liquid B65G, e.g. B65G49/02)
- H10F: INORGANIC SEMICONDUCTOR DEVICES SENSITIVE TO INFRARED RADIATION, LIGHT, ELECTROMAGNETIC RADIATION OF SHORTER WAVELENGTH OR CORPUSCULAR RADIATION
- B32B: LAYERED PRODUCTS, i.e. PRODUCTS BUILT-UP OF STRATA OF FLAT OR NON-FLAT, e.g. CELLULAR OR HONEYCOMB, FORM
- Y02E: REDUCTION OF GREENHOUSE GAS [GHG] EMISSIONS, RELATED TO ENERGY GENERATION, TRANSMISSION OR DISTRIBUTION

## Abstract

A method for making a heat treated (HT) coated article including an electrode, to be used in applications such as windows, electronic devices, or other applications. The method may include heat treating a substrate coated with at least a transparent conductive oxide (TCO) layer and an overlying film. From the TCO outwardly, the overlying film may include any combination of two, three or four of: (i) a gettering and/or doping layer(s); (ii) a stabilizing layer(s); (iii) a release layer(s); and (iv) an oxygen blocking or barrier layer. After HT, the protective film may be entirely or partially removed. Other embodiments relate to the pre-HT coated article, or the post-HT coated article.

## Claims

### Claim 1

A method of making a heat treated coated article, the method comprising:
heat treating a coated substrate comprising a substrate, a transparent conductive oxide (TCO) layer on the substrate, and a protective film on the substrate over at least the TCO layer, wherein the protective film includes a release layer and an oxygen barrier layer where the release layer and the oxygen barrier layer are of different material and/or different stoichiometry relative to each other, wherein the heat treating comprises heating at least the substrate to temperature(s) of at least 500 degrees C.;
during said heat treating of the coated substrate with the TCO layer and the protective film thereon, the protective film protects the TCO layer so that the TCO layer does not lose a significant amount of electrical conductivity and/or a significant amount of visible transmission during said heat treating; and
exposing the protective film to a release liquid and removing at least part of the protective film during and/or after said heat treating.

### Claim 2 (depends on 1)

The method of claim 1, wherein the substrate is a glass substrate.

### Claim 3 (depends on 1)

The method of claim 1, wherein the TCO layer comprises indium tin oxide (ITO).

### Claim 4 (depends on 1)

The method of claim 1, wherein the release layer comprises zinc oxide.

### Claim 5 (depends on 1)

The method of claim 1, wherein the barrier layer comprises aluminum nitride.

### Claim 6 (depends on 1)

The method of claim 1, wherein the release layer comprises zinc oxide and the barrier layer comprises aluminum nitride.

### Claim 7 (depends on 1)

The method of claim 1, wherein the release layer comprises a suboxide of Zn so that the release layer is substoichiometric at least prior to said heat treating.

### Claim 8 (depends on 7)

The method of claim 7, wherein, prior to said heat treating, the release layer comprises ZnOy where “y” is from about 0.1 to 0.9.

### Claim 9 (depends on 1)

The method of claim 1, wherein, in the protective film prior to said heat treating, the release layer is more metallic than is the barrier layer.

### Claim 10 (depends on 1)

The method of claim 1, wherein said heat treating comprises heating the substrate to temperature(s) of at least 580 degrees C.

### Claim 11 (depends on 1)

The method of claim 1, wherein, prior to said heat treating, the coated substrate further comprises a stabilizing layer located between at least the release layer and the TCO layer.

### Claim 12 (depends on 11)

The method of claim 11, wherein the stabilizing layer comprises zinc oxynitride.

### Claim 13 (depends on 1)

The method of claim 1, wherein, prior to said heat treating, the coated article further comprises a gettering and/or doping layer between at least the release layer and the TCO layer.

### Claim 14 (depends on 13)

The method of claim 13, wherein the gettering and/or doping layer comprises at least one of C and F.

### Claim 15 (depends on 13)

The method of claim 13, wherein the gettering and/or doping layer comprises C and F, getters oxygen during said heat treating and helps dope the TCO layer with F to improve conductivity.

### Claim 16 (depends on 1)

The method of claim 1, further comprising implanting C and/or F ions into the TCO layer prior to said heat treating.

### Claim 17 (depends on 1)

The method of claim 1, further comprising implanting F ions into the TCO layer via an ion beam prior to said heat treating.

### Claim 18 (depends on 1)

The method of claim 1, wherein the release liquid comprises water and/or vinegar.

### Claim 19 (depends on 1)

The method of claim 1, wherein the coated article is substantially transparent and following the heat treating the TCO layer is provided as an electrode in an electronic device.

### Claim 20 (depends on 1)

The method of claim 1, wherein after said removing step at least part of the TCO layer is exposed so as to be an outermost layer of the coated article.

### Claim 21 (depends on 1)

The method of claim 1, wherein the barrier layer comprises zirconium nitride.

### Claim 22 (depends on 1)

The method of claim 1, wherein the protective film further includes a layer comprising zirconium nitride located directly under or directly over the barrier layer.

### Claim 23 (depends on 1)

The method of claim 1, wherein the coated substrate further comprises an underlayer located between the substrate and the TCO layer.

### Claim 24 (depends on 1)

The method of claim 1, wherein the coated substrate further comprises a layer comprising silver located between the TCO layer and the substrate.

### Claim 25 (depends on 1)

The method of claim 1, wherein the substrate is a semiconductor substrate.

### Claim 26

A method of making a heat treated coated article, the method comprising:
heat treating a coated glass substrate comprising a glass substrate, a transparent conductive layer comprising ITO on the glass substrate, and a protective film on the glass substrate over at least the layer comprising ITO, wherein the protective film includes a release layer comprising zinc oxide and an oxygen barrier layer comprising metal nitride;
during said heat treating of the coated glass substrate with the layer comprising ITO and the protective film thereon, the protective film protects the layer comprising ITO so that the layer comprising ITO does not lose a significant amount of electrical conductivity and/or a significant amount of visible transmission during said heat treating; and
removing at least part of the protective film during and/or after said heat treating.

### Claim 27

A heat treated coated article comprising:
a thermally tempered glass substrate;
a transparent conductive layer comprising ITO on the tempered glass substrate; and
wherein at least an upper portion of the layer comprising ITO is doped with carbon and/or fluorine.

### Claim 28 (depends on 27)

The coated article of claim 27, wherein at least the upper portion of the layer comprising ITO contains from about 0.1 to 15% fluorine (atomic %).

### Claim 29 (depends on 27)

The coated article of claim 27, wherein at least the upper portion of the layer comprising ITO contains from about 0.1 to 15% carbon (atomic %).