# US 2013/0271256 A1 · Dust core, method for manufacturing the same, and coil component

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2013/0271256 A1
- Document ID: US20130271256A1
- Status: Published application
- Kind: A1
- Application number: 13/995,770
- Filed: 2012-07-06
- Published: 2013-10-17
- Earliest claimed: 2011-07-22
- Assignees: Sumitomo Electric Sintered Alloy, Ltd.; Sumitomo Electric Industries, Ltd.
- Inventors: Tomoyuki Ueno; Yoshiyuki Shimada
- Web page: https://patentgrep.com/patent/US20130271256A1

## CPC

- H01F 41/0206: {Manufacturing of magnetic cores by mechanical means (magnetic cores per se H01F27/24)}
- B22F 3/24: After-treatment of workpieces or articles {(B22F3/1146 takes precedence)}
- H01F 3/08: made from powder (powder coatings on sheets H01F3/02; on strips or ribbons H01F3/04; on wires H01F3/06)
- H01F 41/0246: {Manufacturing of magnetic circuits by moulding or by pressing powder (magnetic cores made by moulding or by pressing powder H01F27/255; soft magnetic particles H01F1/20, H01F1/36)}
- B22F 2998/10: Processes characterised by the sequence of their steps
- H01F 7/081: {Magnetic constructions}
- H01F: MAGNETS; INDUCTANCES; TRANSFORMERS; SELECTION OF MATERIALS FOR THEIR MAGNETIC PROPERTIES
- B22F: WORKING METALLIC POWDER; MANUFACTURE OF ARTICLES FROM METALLIC POWDER; MAKING METALLIC POWDER (making alloys by powder metallurgy C22C); APPARATUS OR DEVICES SPECIALLY ADAPTED FOR METALLIC POWDER

## Abstract

A method includes a step of compacting an insulation-coated pure iron powder or an iron-based alloy powder mainly containing iron using a die to obtain a dust core, a step of heat-treating the obtained dust core, and a step of post-machining at least one portion of the heat-treated dust core using a grinding wheel. In the post-machining step, grinding is performed in such a manner that the dust core and the grinding wheel are rotated, whereby isotropic machining marks are formed on a machined surface of the dust core.

## Claims

### Claim at position 1

1-17. (canceled)

### Claim 18

A method for manufacturing a dust core, comprising:
a step of compacting an insulation-coated pure iron powder or an iron-based alloy powder mainly containing iron using a die to obtain the dust core;
a step of heat-treating the obtained dust core; and
a step of post-machining at least one portion of the heat-treated dust core using a grinding wheel,
wherein the post-machining step is a step of performing grinding in such a manner that the dust core and the grinding wheel are rotated.

### Claim 19 (depends on 18)

The manufacturing method according to claim 18, wherein the die includes a first die and second die facing each other, at least one of the first die and the second die exhibits a stepped shape having a convex portion and/or a concave portion or a shape that a plurality of stepped portions are separated, and the dust core obtained by compacting has a density of 7.0 g/cm3 to 7.6 g/cm3.

### Claim 20 (depends on 18)

The manufacturing method according to claim 18, wherein the rotational speed of the dust core ranges from 150 rpm to 1,500 rpm and the grinding wheel is rotated at a peripheral speed of 720 m/min or more and not more than the maximum allowable peripheral speed thereof.

### Claim 21 (depends on 18)

The manufacturing method according to claim 18, wherein the grinding wheel contains abrasive grains which have a median diameter of 25 μm to 88 μm and which are made of diamond or cubic boron nitride.

### Claim 22 (depends on 18)

The manufacturing method according to claim 18, wherein the grinding wheel has a grinding surface which contributes to machining and which has at least one grooved portion extending to the outer edge of the grinding wheel and the width of the grooved portion ranges from 0.05% to 1.00% of the effective outermost circumference of the grinding wheel.

### Claim 23 (depends on 18)

The manufacturing method according to claim 18, further comprising a step of dressing the grinding wheel, wherein a major component of a dresser used for dressing is at least one selected from the group consisting of white alumina, green silicon carbide, diamond, and cubic boron nitride and the dresser has a median diameter of 18 μm to 105 μm.

### Claim 24 (depends on 18)

The manufacturing method according to claim 18, wherein in the post-machining step, a water-soluble grinding solution containing 0.3% to 1.5% by mass of at least one of diethanolamine and triethanolamine is used.

### Claim 25 (depends on 18)

The manufacturing method according to claim 18, wherein the pure iron powder or the iron-based alloy powder mainly containing iron has a median diameter of 60 μm to 250 μm.

### Claim 26 (depends on 18)

The manufacturing method according to claim 18, wherein the pure iron powder or the iron-based alloy powder mainly containing iron is compacted at a contact pressure of 6 ton/cm2 to 13 ton/cm2.

### Claim 27 (depends on 18)

The manufacturing method according to claim 18, wherein in the heat-treating step, the dust core is heat-treated at a temperature of 300° C. to 600° C. for at least ten minutes in air, a nitrogen atmosphere, or a flow of a mixture thereof.

### Claim 28 (depends on 18)

The manufacturing method according to claim 18, further comprising a step of removing burrs formed on the surface of the dust core during compacting or post-machining, wherein the burrs are removed using a brush prepared from a synthetic resin combined with hard abrasive grains made of white alumina or green silicon carbide.

### Claim 29 (depends on 18)

The manufacturing method according to claim 18, further comprising a step of performing degaussing subsequently to the removal of the burrs such that the remanence is 5 mT or less.

### Claim 30 (depends on 29)

The manufacturing method according to claim 29, further comprising a step of washing the dust core with a washing liquid containing the water-soluble grinding solution used during post-machining at a discharge pressure of 0.05 MPa to 0.40 MPa subsequently to degaussing.

### Claim 31

A dust core formed by compacting an insulation-coated pure iron powder or an iron-based alloy powder mainly containing iron using a die, having a machined surface having isotropic machining marks formed on at least one portion thereof by a grinding wheel, the dust core exhibiting a stepped shape having a convex portion or a concave portion or a shape that a plurality of stepped portions are separated, the dust core having a density of 7.0 g/cm3 to 7.6 g/cm3.

### Claim 32 (depends on 31)

The dust core according to claim 31, wherein the dimensional accuracy of the flatness and parallelism of the machined surface is 50 μm or less in terms of machining error.

### Claim 33 (depends on 31)

The dust core according to claim 31, comprising at least one portion coated with a rust-proof layer containing at least one of diethanolamine and triethanolamine which is a component of a water-soluble grinding solution used during machining due to a grinding wheel.

### Claim 34 (depends on 18)

A coil component prepared by coiling a copper wire around a dust core manufactured by a manufacturing method according to claim 18.