# US 2013/0270645 A1 · Workfunction metal stacks for a final metal gate

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2013/0270645 A1
- Document ID: US20130270645A1
- Status: Published application
- Kind: A1
- Application number: 13/445,475
- Filed: 2012-04-12
- Published: 2013-10-17
- Earliest claimed: 2012-04-12
- Assignees: Globalfoundries Inc.
- Inventors: Thilo Scheiper; Jan Hoentschel
- Web page: https://patentgrep.com/patent/US20130270645A1

## CPC

- H10D 84/038: {using silicon technology, e.g. SiGe}
- H10D 84/0177: {the gate conductors having different materials or different implants}
- H10D: INORGANIC ELECTRIC SEMICONDUCTOR DEVICES

## Abstract

Transistor devices are formed with a pMOS and an nMOS workfunction stack of substantially equal thickness after gate patterning. Embodiments include forming n-type and p-type areas in a substrate, forming a pMOS workfunction metal stack layer on both areas, forming a hardmask layer on the pMOS workfunction metal stack layer on the n-type area, removing the pMOS workfunction metal stack layer from the p-type area, forming an nMOS workfunction metal stack layer on the p-type area and on the hardmask layer, and removing the nMOS workfunction metal stack layer from the hardmask layer.

## Claims

### Claim 1

A method comprising:
forming an n-type area and a p-type area in a substrate;
forming a pMOS workfunction metal stack layer on the n-type area and the p-type area;
forming a hardmask layer on the pMOS workfunction metal stack layer on the n-type area;
removing the pMOS workfunction metal stack layer from the p-type area;
forming an nMOS workfunction metal stack layer on the p-type area and on the hardmask layer; and
removing the nMOS workfunction metal stack layer from the hardmask layer.

### Claim 2 (depends on 1)

The method according to claim 1, further comprising:
removing the hardmask layer after removing the nMOS workfunction metal stack layer from the hardmask layer;
forming a polycrystalline silicon (poly-Si) or an amorphous silicon (a-Si) layer on the pMOS workfunction metal stack layer and on the nMOS workfunction metal stack layer; and
patterning the pMOS workfunction metal stack layer and the overlying poly-Si or a-Si layer to form a pMOS gate electrode, and patterning the nMOS workfunction metal stack layer and the overlying poly-Si or a-Si layer to form an nMOS gate electrode.

### Claim 3 (depends on 2)

The method according to claim 2, comprising forming the poly-Si or the a-Si to a thickness of 550 angstroms (Å) to 650 Å.

### Claim 4 (depends on 1)

The method according to claim 1, further comprising:
forming a shallow trench isolation (STI) region between the n-type area and the p-type area;
forming a channel silicon germanium (cSiGe) layer in the n-type area of the substrate; and
forming a high-k dielectric layer over the n-type and p-type areas prior to forming the pMOS workfunction metal stack layer.

### Claim 5 (depends on 1)

The method according to claim 1, comprising annealing the pMOS and nMOS workfunction metal stack layers at a temperature of 800° C. to 950° C. subsequent to removing the hardmask layer.

### Claim 6 (depends on 1)

The method according to claim 1, comprising forming the pMOS workfunction metal stack layer by:
forming a first layer of titanium nitride (TiN) to a thickness of 2 Å to 10 Å;
forming a layer of aluminum (Al) to a thickness of 2 Å to 8 Å; and
forming a second layer of TiN to a thickness of 15 Å to 25 Å.

### Claim 7 (depends on 6)

The method according to claim 6, comprising forming the nMOS workfunction metal stack layer by:
forming a layer of lanthanum (La) to a thickness of 2 Å to 10 Å; and
forming a layer of TiN to a thickness of 15 Å to 25 Å.

### Claim 8 (depends on 1)

The method according to claim 1, comprising forming the hardmask layer by:
forming a layer of silicon nitride (SiN) over the p-type area and the n-type area; and
removing the SiN from the p-type area by:
forming a resist over the n-type area; and
dry etching the SiN.

### Claim 9 (depends on 1)

The method according to claim 1, comprising forming the hardmask layer by:
forming a layer of silicon dioxide (SiO2) over the p-type are and the n-type area; and
removing the SiO2 from the p-type area by:
forming a resist over the n-type area; and
etching the SiO2 with hydrofluoric acid (HF).

### Claim 10 (depends on 1)

The method according to claim 1, comprising removing the nMOS workfunction metal stack layer from the n-type area by:
forming a resist on the p-type area; and
wet etching.

### Claim 11 (depends on 1)

The method according to claim 1, comprising removing the pMOS workfunction metal stack layer from the p-type area by:
forming a resist on the n-type area; and
wet etching.

### Claim 12

A device, comprising:
a substrate having a p-type area and an n-type area;
a pMOS workfunction metal stack layer over the n-type area, the pMOS workfunction metal stack layer having a first thickness; and
an nMOS workfunction metal stack layer over the p-type area, the nMOS workfunction metal stack layer having a second thickness substantially equal to the first thickness.

### Claim 13 (depends on 12)

The device according to claim 12, further comprising a high-k dielectric layer on the substrate beneath the nMOS and pMOS workfunction metal stack layers.

### Claim 14 (depends on 12)

The device according to claim 12, further comprising:
a polysilicon (poly-Si) or an amorphous silicon (a-Si) layer on the pMOS and nMOS workfunction metal stack layers having a thickness of 550 angstroms (Å) to 650 Å.

### Claim 15 (depends on 12)

The device according to claim 12, wherein the pMOS workfunction metal stack layer comprises:
a first layer of titanium nitride (TiN) having a thickness of 2 Å to 10 Å;
a layer of aluminum (Al) having a thickness of 2 Å to 8 Å; and
a second layer of TiN having a thickness of 15 Å to 25 Å.

### Claim 16 (depends on 15)

The device according to claim 15, wherein the nMOS workfunction metal stack layer comprises:
a layer of lanthanum (La) having a thickness of 2 Å to 10 Å; and
a layer of TiN with a thickness of 15 Å to 25 Å.

### Claim 17

A method comprising:
forming an n-type area and a p-type area in a substrate separated by a shallow trench isolation (STI) region;
forming a channel silicon germanium (cSiGe) layer in the n-type area;
forming a high-k dielectric layer over the p-type area, the STI region, and the cSiGe layer;
forming a pMOS workfunction metal stack layer on the high-k dielectric layer;
forming a hardmask layer on the pMOS workfunction metal stack layer;
removing a portion of the hardmask layer positioned over the p-type area, exposing a portion of the pMOS workfunction metal stack layer;
removing the exposed portion of the pMOS workfunction metal stack layer, exposing a portion of the high-k dielectric layer;
forming an nMOS workfunction metal stack layer on the exposed portion of the high-k dielectric layer and on a remaining portion of the hardmask layer;
removing a portion of the nMOS workfunction metal stack layer positioned on the remaining portion of the hardmask layer;
removing the remaining portion of the hardmask layer;
forming a polysilicon (poly-Si) or an amorphous silicon (a-Si) layer on a remaining portion of the pMOS workfunction metal stack layer and on a remaining portion of the nMOS workfunction metal stack layer; and
patterning the remaining portion of the nMOS workfunction metal stack layer and the overlying poly-Si or a-Si layer and the remaining portion of the pMOS workfunction metal stack layer and the overlying poly-Si or a-Si layer to form an nMOS gate electrode and a pMOS gate electrode, respectively.

### Claim 18 (depends on 17)

The method according to claim 17, comprising forming the pMOS workfunction by:
forming a first layer of titanium nitride (TiN);
forming a layer of aluminum (Al); and
forming a second layer of TiN.

### Claim 19 (depends on 17)

The method according to claim 17, comprising forming the nMOS workfunction metal stack layer by:
forming a layer of lanthanum (La); and
forming a layer of TiN.

### Claim 20 (depends on 17)

The method according to claim 17, comprising forming the hardmask layer by forming a layer of silicon nitride (SiN) or silicon dioxide (SiO2).