# US 2013/0266791 A1 · Method of preparing Ag- based oxide contact materials with directionally arranged reinforcing particles

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2013/0266791 A1
- Document ID: US20130266791A1
- Status: Published application
- Kind: A1
- Application number: 13/577,897
- Filed: 2011-04-11
- Published: 2013-10-10
- Earliest claimed: 2010-12-30
- Assignees: Wenzhou Hongfeng Electrical Alloy Co., Ltd.
- Inventors: Lesheng Chen; Xiao Chen; Gengxin Qi; Chengfa Mu
- Web page: https://patentgrep.com/patent/US20130266791A1

## CPC

- H01H 1/0237: and containing oxides
- B22F 3/04: by applying fluid pressure {, e.g. by cold isostatic pressing [CIP]}
- B22F 3/10: Sintering only
- B22F 3/14: simultaneously
- B22F 3/20: by extruding
- C22C 5/06: Alloys based on silver
- C22C 49/02: characterised by the matrix material
- C22C 49/14: characterised by the fibres or filaments
- H01H 1/02372: {containing as major components one or more oxides of the following elements only: Cd, Sn, Zn, In, Bi, Sb or Te}
- H01H 1/02374: {containing as major component CdO}
- H01H 1/02376: {containing as major component SnO2}
- Y10T 428/249921: Web or sheet containing structurally defined element or component
- H01H: ELECTRIC SWITCHES; RELAYS; SELECTORS; EMERGENCY PROTECTIVE DEVICES (contact cables H01B7/10; electrolytic self-interrupters H01G9/18; emergency protective circuit arrangements H02H; switching by electronic means without contact-making H03K17/00)
- B22F: WORKING METALLIC POWDER; MANUFACTURE OF ARTICLES FROM METALLIC POWDER; MAKING METALLIC POWDER (making alloys by powder metallurgy C22C); APPARATUS OR DEVICES SPECIALLY ADAPTED FOR METALLIC POWDER
- C22C: ALLOYS (treatment of alloys C21D, C22F)
- Y10T: TECHNICAL SUBJECTS COVERED BY FORMER US CLASSIFICATION

## Abstract

In the present invention, a method of preparing Ag-based oxide contact materials with directionally arranged reinforcing particles is disclosed, comprising steps of: a) preparing evenly dispersed composite powders by chemical co-precipitation method combining with roasting, b) granulating the composite powders by high energy ball milling, and sieving the powders, c) mixing the powders and Ag matrix in a powder mixing machine, d) cold isostatic pressing, e) sintering, f) hot-pressing, g) hot-extruding to obtain Ag-based oxide contact materials with directionally arranged reinforcing particles. This method can obtain particle reinforced Ag-based material with good electrical performance even when the reinforced (oxide) particles are very small. This method is simple, easy to operate, and does not require special equipment. The resistance to welding and arc erosion, electric conductivity and the processability of the material prepared through this present invention can be greatly improved.

## Claims

### Claim 1

A preparation method of a particle directional arrangement reinforced Ag-based oxide contact material comprising steps of:
a) preparing mixed solution containing Ag+ and reinforcing phase metal ion, adding co-precipitator while stirring, obtaining precipitate, washing and roasting the precipitate, and obtaining evenly dispersed composite powder, wherein the proportion of the Ag+ and reinforcing phase metal ion is obtained by calculating constituents of the composite powders to be prepared; the co-precipitator is a precipitant that can precipitate the solution of Ag+ and reinforcing phase metal ion, and the precipitate can be decomposed to metal oxide after roasting, wherein the co-precipitator should be in sufficient amount so as to completely precipitate the solution of Ag+ and reinforcing phase metal ion;
b) granulating the composite powders obtained in step a) by high energy ball milling, sieving the powder, reprocessing the powder that fail to be sieved, and sieving again;
c) mixing the powders granulated in step (b) and Ag matrix in a powder mixing machine, wherein the weight ratio of the granulated powders and the Ag matrix is calculated according to the material to be prepared;
d) pressing the powders obtained in step c) by cold isostatic pressing to obtain a green body;
e) sintering the green body obtained by cold isostatic pressing;
f) hot-pressing the green body after sintering;
g) hot-extruding the green body after hot-pressing, and obtaining the Ag-based oxide contact material with directionally arranged reinforcing particles.

### Claim 2 (depends on 1)

The preparation method according to claim 1, wherein in step a) the proportion of Ag+ and reinforcing phase metal ion is calculated according to the oxide taking up the composite powder from ¾ to ½ in weight

### Claim 3 (depends on 1)

The preparation method according to claim 1, wherein in step a) the stirring speed is between 80 revolutions per minute and 120 revolutions per minute; the reaction time is between 2 and 4 hours; the roasting temperature is between 300° C. and 500° C. and the roasting time is between 1 hour and 5 hours.

### Claim 4 (depends on 1)

The preparation method according to claim 1, wherein in step b) a rotating speed of ball mill is between 180 revolutions per minute and 350 revolutions per minute; ball milling time is between 5 and 15 hours; ball-to-powder weight ratio is between 10 and 20; the number of sieving meshes is between 100 and 400.

### Claim 5 (depends on 1)

The preparation method according to claim 1, wherein in step c) the rotating speed of the mixing powder machine is between 20 revolutions per minute and 35 revolutions per minute; the mixing time is between 2 and 6 hours.

### Claim 6 (depends on 1)

The preparation method according to claim 1, wherein in step d) the pressure of isostatic pressing is between 100 and 500 Mpa.

### Claim 7 (depends on 1)

The preparation method according to claim 1, wherein in step e) the sintering temperature is between 600° C. and 800° C.; the sintering time is between 8 and 15 hours.

### Claim 8 (depends on 1)

The preparation method according to claim 1, wherein in step f) the hot-pressing temperature is between 500° C. and 900° C.; the pressure of hot-pressing is between 300 and 700 Mpa; the hot-pressing time is between 5 min and 20 min.

### Claim 9 (depends on 1)

The preparation method according to claim 1, wherein in step g) the temperature of the green body during the hot-extruding is between 700° C. and 900° C.; the extruding ratio is between 100 and 400; the extruding speed is between 5 and 15 cm/min; the preheating temperature of the extrusion is between 300° C. and 600° C.

### Claim 10 (depends on 1)

Ag-based oxide contact materials with directionally arranged reinforcing particles prepared by the method according to claim 1, wherein the reinforcing particles in the matrix display in the form of particles connecting with each other and being directionally arranged, and the reinforcing material can be a single type of material or a mixture of several materials.