# US 2013/0260650 A1 · Composition for polishing and method of polishing semiconductor substrate using same

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2013/0260650 A1
- Document ID: US20130260650A1
- Status: Published application
- Kind: A1
- Application number: 13/882,280
- Filed: 2011-11-07
- Published: 2013-10-03
- Earliest claimed: 2010-11-08
- Assignees: Fujimi Incorporated
- Inventors: Toshio Shinoda; Kayoko Nagahara; Yutaka Inoue; Shuhei Takahashi; Toshihiro Miwa
- Web page: https://patentgrep.com/patent/US20130260650A1

## CPC

- C09G 1/02: containing abrasives or grinding agents {(abrasives as such C09K3/14; polishing of semi-conductors H10P52/40)}
- B24B 31/003: {whereby the workpieces are mounted on a holder and are immersed in the abrasive material}
- H10P 90/129: {by polishing}
- C09G: POLISHING COMPOSITIONS (French polish C09F11/00); SKI WAXES
- B24B: MACHINES, DEVICES, OR PROCESSES FOR GRINDING OR POLISHING (grinding of gear teeth B23F, of screw-threads B23G1/36; by electro-erosion B23H; abrasive or related blasting B24C; tools for grinding, buffing or sharpening B24D; polishing compositions C09G1/00; abrasives C09K3/14; electrolytic etching or polishing C25F3/00; grinding arrangements for use on assembled railway tracks E01B31/17); DRESSING OR CONDITIONING OF ABRADING SURFACES; FEEDING OF GRINDING, POLISHING, OR LAPPING AGENTS
- H10P: GENERIC PROCESSES OR APPARATUS FOR THE MANUFACTURE OR TREATMENT OF DEVICES COVERED BY CLASS H10

## Abstract

Provided is a polishing composition containing abrasive grains, at least one type of alcohol compound selected from the group consisting of aliphatic alcohols with 2 to 6 carbon atoms and glycol ethers with 3 to 10 carbon atoms, at least one type of basic compound selected from the group consisting of quaternary ammonium salts and alkali metal salts, and water. The average primary particle diameter of the abrasive grains is 5 to 50 nm. The content of the alcohol compound in the polishing composition is 0.01 to 1% by mass. The polishing composition is mainly used in an application of polishing a semiconductor substrate surface.

## Claims

### Claim 1

A polishing composition comprising:
abrasive grains;
at least one type of alcohol compound selected from the group consisting of aliphatic alcohols with 2 to 6 carbon atoms and glycol ethers with 3 to 10 carbon atoms;
at least one type of basic compound selected from the group consisting of quaternary ammonium salts and alkali metal salts; and
water, wherein
the abrasive grains have an average primary particle diameter of 5 to 50 nm, and
the alcohol compound is contained in the polishing composition in an amount of 0.01 to 1% by mass.

### Claim 2 (depends on 1)

The polishing composition according to claim 1, wherein the basic compound is at least one type of compound selected from the group consisting of hydroxides of quaternary ammonium, carbonates of quaternary ammonium, bicarbonates of quaternary ammonium, hydroxides of alkali metals, carbonates of alkali metals, and bicarbonates of alkali metals.

### Claim 3 (depends on 1)

The polishing composition according to claim 1, wherein the basic compound is at least one type of compound selected from the group consisting of tetramethylammonium hydroxide, tetramethylammonium carbonate, tetramethylammonium bicarbonate, potassium hydroxide, potassium carbonate, and potassium bicarbonate.

### Claim 4 (depends on 1)

The polishing composition according to claim 1, wherein the abrasive grains have a cocoon shape or have a spherical shape with a plurality of protrusions on its surface.

### Claim 5 (depends on 1)

The polishing composition according to claim 1, further comprising a chelating agent.

### Claim 6

A polishing composition kit comprising a first component and a second component that are mixed mutually to obtain a polishing composition, wherein
the first component contains abrasive grains, at least one type of basic compound selected from the group consisting of quaternary ammonium salts and alkali metal salts, and water,
the second component contains at least one type of alcohol compound selected from the group consisting of aliphatic alcohols with 2 to 6 carbon atoms and glycol ethers with 3 to 10 carbon atoms,
the abrasive grains have an average primary particle diameter of 5 to 50 nm, and
the alcohol compound is contained in the polishing composition in an amount of 0.01 to 1% by mass.

### Claim 7

A method for polishing a semiconductor substrate surface using a polishing composition, wherein
the polishing composition contains:
abrasive grains;
at least one type of alcohol compound selected from the group consisting of aliphatic alcohols with 2 to 6 carbon atoms and glycol ethers with 3 to 10 carbon atoms;
at least one type of basic compound selected from the group consisting of quaternary ammonium salts and alkali metal salts; and
water,
the abrasive grains have an average primary particle diameter of 5 to 50 nm, and
the alcohol compound is contained in the polishing composition in an amount of 0.01 to 1% by mass.

### Claim 8 (depends on 7)

The method according to claim 7, wherein the polishing of the semiconductor substrate surface is performed using a polishing machine and while supplying the polishing composition to the substrate surface, and whereas the abrasive grains and the basic compound are supplied to the substrate surface continuously from a start of polishing of the substrate surface and thereafter, the alcohol compound is supplied to the substrate surface only after the start of polishing of the substrate surface.

### Claim 9 (depends on 7)

The method according to claim 7, wherein the polishing composition is put into cyclical use.

### Claim 10 (depends on 9)

The method according to claim 9, wherein in putting the polishing composition into cyclical use, a reduced amount of at least any one of the abrasive grains, the alcohol compound, and the basic compound in the polishing composition is replenished.