# US 2013/0260310 A1 · Toner process using acoustic mixer

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2013/0260310 A1
- Document ID: US20130260310A1
- Status: Published application
- Kind: A1
- Application number: 13/434,565
- Filed: 2012-03-29
- Published: 2013-10-03
- Earliest claimed: 2012-03-29
- Assignees: Xerox Corporation
- Inventors: Yulin Wang; Kimberly Nosella; David Kurceba; Santiago Faucher
- Web page: https://patentgrep.com/patent/US20130260310A1

## CPC

- G03G 9/08795: {characterised by their chemical properties, e.g. acidity, molecular weight, sensitivity to reactants}
- G03G 9/0804: {whereby the components are brought together in a liquid dispersing medium}
- G03G 9/08755: {Polyesters}
- G03G 9/08797: {characterised by their physical properties, e.g. viscosity, solubility, melting temperature, softening temperature, glass transition temperature}
- G03G 9/09364: {obtained by reactions only involving carbon-to-carbon unsaturated bonds}
- G03G 9/09371: {obtained otherwise than by reactions only involving carbon-to-carbon unsaturated bonds}
- G03G 9/09392: {Preparation thereof}
- G03G: ELECTROGRAPHY; ELECTROPHOTOGRAPHY; MAGNETOGRAPHY

## Abstract

A process for making emulsion aggregation (EA) toners is provided. In embodiments, the process comprises aggregating a mixture comprising a latex resin, and at least one colorant in a reactor to form aggregated toner particles, adding a shell resin to form a shell over the aggregated toner particles, coalescing the aggregated toner particles, and recovering the toner particles.

## Claims

### Claim 1

A method for making a toner particles comprising:
a) mixing a composition comprising an amorphous resin emulsion, an optional crystalline resin emulsion, an optional wax emulsion, at least one colorant emulsion to form a composite emulsion.
b) adding an aggregating agent to the composite emulsion directly without homogenizing the aggregating agent to form a toner slurry of preaggregated particles by subjecting the composite emulsion and aggregating agent to acoustic mixing at a g force of from about 50 g force to about 100 g force;
c) aggregating the particles; and optionally,
d) forming a shell on the particles to form an emulsion aggregated toner.

### Claim 2 (depends on 1)

The process of claim 1, wherein step (b) is performed at a resonant frequency of from about 15 Hz to about 2000 Hz.

### Claim 3 (depends on 1)

The process of claim 1, wherein step (b) is performed with or without milling media.

### Claim 4 (depends on 3)

The process of claim 3, wherein the milling media comprises a size of from about 0.5 mm to 10 mm.

### Claim 5 (depends on 3)

The process of claim 3, wherein the milling media comprises a material selected from the group consisting of glass, steel, ceramic and mixtures thereof.

### Claim 6 (depends on 1)

The process of claim 1, wherein acoustic mixing occurs for a period of time of from about 5 minutes to about 10 minutes.

### Claim 7 (depends on 1)

The process of claim 1, wherein acoustic mixing occurs at a temperature of from about 0° C. to about 50° C.

### Claim 8 (depends on 1)

The process of claim 1, wherein the toner slurry has a solids content of from about 5 to about 30 percent solids by total weight of the toner slurry.

### Claim 9 (depends on 8)

The process of claim 8, wherein the toner slurry has a solids content of from about 10 to about 20 percent solids by total weight of the toner slurry.

### Claim 10 (depends on 1)

The process of claim 1, wherein the amorphous resin is selected from the group consisting of polyester, a polyamide, a polyimide, a polystyrene-acrylate, a polystyrene-methacrylate, a polystyrene-butadiene, or a polyester-imide, and mixtures thereof.

### Claim 11 (depends on 1)

The process of claim 1, wherein the optional crystalline resin is selected from the group consisting of polyester, a polyamide, a polyimide, a polyethylene, a polypropylene, a polybutylene, a polyisobutyrate, an ethylene-propylene copolymer, or an ethylene-vinyl acetate copolymer, and mixtures thereof.

### Claim 12 (depends on 1)

The process of claim 1, wherein the mixture further comprises a component selected from the group consisting of surfactants, functional monomers, initiators, surface additives, charge control agents, chain transfer agents, and combinations thereof.

### Claim 13 (depends on 1)

The process of claim 1, wherein the aggregating agent is selected from the group consisting of polyaluminum chloride, polyaluminum sulfa silicate, aluminum chloride, aluminum nitrite, aluminum sulfate, potassium aluminum sulfate, calcium acetate, calcium chloride, calcium nitrite, calcium oxylate, calcium sulfate, magnesium acetate, magnesium nitrate, magnesium sulfate, zinc acetate, zinc nitrate, zinc sulfate, and combinations thereof.

### Claim 14 (depends on 1)

The process of claim 1, wherein the colorant is selected from the group consisting of carbon black, cyan, yellow, magenta, red, orange, brown, green, blue, violet, and combinations thereof.

### Claim 15

A method for making toner particles comprising:
a) mixing a composition comprising an amorphous resin emulsion, an optional crystalline resin emulsion, an optional wax emulsion, at least one colorant emulsion to form a composite emulsion;
b) adding an aggregating agent to the composite emulsion directly without homogenizing the aggregating agent to form a toner slurry of preaggregated particles by subjecting the composite emulsion and aggregating agent to acoustic mixing at a g force of from about 50 g force to about 100 g force;
c) aggregating the particles; and optionally,
d) forming a shell on the particles to form an emulsion aggregated toner, wherein no heat is generated during the method for making toner particles.

### Claim 16 (depends on 15)

The process of claim 15, wherein the amorphous resin is linear in structure and the optional crystalline resin is a polyester. the linear amorphous resin having the following formula:
wherein m for linear amorphous resin A is about from about 2 to about 10, and m for linear amorphous resin B is about from about 2 to about 10.

### Claim 17 (depends on 15)

The process of claim 15, wherein the crystalline polyester resin has the following
wherein b is from about 5 to about 2000 and d is from about 5 to about 2000.

### Claim 18

A method for making a toner particles comprising:
a) mixing a composition comprising a linear amorphous resin emulsion, an optional crystalline polyester resin emulsion, an optional wax emulsion, at least one colorant emulsion to form a composite emulsion;
b) adding an aggregating agent to the composite emulsion directly without homogenizing the aggregating agent to form a toner slurry of preaggregated particles by subjecting the composite emulsion and aggregating agent to acoustic mixing at a g force of about 90 g force;
c) aggregating the particles; and optionally,
d) forming a shell on the particles to form an emulsion aggregated toner.

### Claim 19 (depends on 18)

The process of claim 18, wherein the linear amorphous resin has the following formula:
wherein m for linear amorphous resin A was about is about from about 2 to about 10, and m for linear amorphous resin B was about is about from about 2 to about 10.

### Claim 20 (depends on 18)

The process of claim 18, wherein the crystalline polyester resin has the following
wherein b is from about 5 to about 2000 and d was from about 5 to about 2000.