# US 2013/0260245 A1 · Electrode material and method for producing the same

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2013/0260245 A1
- Document ID: US20130260245A1
- Status: Published application
- Kind: A1
- Application number: 13/993,403
- Filed: 2011-11-28
- Published: 2013-10-03
- Earliest claimed: 2010-12-17
- Assignees: Sumitomo Osaka Cement Co., Ltd.
- Inventors: Takao Kitagawa; Hirofumi Yasumiishi; Masaru Uehara
- Web page: https://patentgrep.com/patent/US20130260245A1

## CPC

- H01M 4/625: {Carbon or graphite}
- C01B 32/05: Preparation or purification of carbon not covered by groups C01B32/15, C01B32/20, C01B32/25, C01B32/30
- H01M 4/131: Electrodes based on mixed oxides or hydroxides, or on mixtures of oxides or hydroxides, e.g. LiCoOx
- H01M 4/366: {as layered products}
- H01M 4/485: of mixed oxides or hydroxides for inserting or intercalating light metals, e.g. LiTi2O4 or LiTi2OxFy (H01M4/505, H01M4/525 take precedence)
- H01M 4/505: of mixed oxides or hydroxides containing manganese for inserting or intercalating light metals, e.g. LiMn2O4 or LiMn2OxFy
- H01M 4/525: of mixed oxides or hydroxides containing iron, cobalt or nickel for inserting or intercalating light metals, e.g. LiNiO2, LiCoO2 or LiCoOxFy
- H01M 4/5825: {Oxygenated metallic salts or polyanionic structures, e.g. borates, phosphates, silicates, olivines}
- H01M 2004/021: {Physical characteristics, e.g. porosity, surface area}
- Y02E 60/10: Energy storage using batteries
- Y02P 70/50: Manufacturing or production processes characterised by the final manufactured product
- H01M: PROCESSES OR MEANS, e.g. BATTERIES, FOR THE DIRECT CONVERSION OF CHEMICAL ENERGY INTO ELECTRICAL ENERGY
- C01B: NON-METALLIC ELEMENTS; COMPOUNDS THEREOF; {METALLOIDS OR COMPOUNDS THEREOF NOT COVERED BY SUBCLASS C01C}
- Y02E: REDUCTION OF GREENHOUSE GAS [GHG] EMISSIONS, RELATED TO ENERGY GENERATION, TRANSMISSION OR DISTRIBUTION
- Y02P: CLIMATE CHANGE MITIGATION TECHNOLOGIES IN THE PRODUCTION OR PROCESSING OF GOODS

## Abstract

The present invention provides an electrode material in which unevenness in a supporting amount of a carbonaceous film is less when using an electrode-active material having a carbonaceous film on a surface thereof as the electrode material, and which is capable of improving conductivity, and a method for producing the electrode material. The electrode material includes an aggregate formed by aggregating an electrode-active material in which a carbonaceous film is formed on a surface. In the electrode material, an average particle size of the aggregate is 0.5 to 100 μm, a volume density of the aggregate is 50 to 80 vol % of a volume density in a case in which the aggregate is a solid, and 80% or more of the surface of the electrode-active material is covered with the carbonaceous film. Alternatively, the electrode material includes an aggregate formed by aggregating electrode-active material particles in which a carbonaceous film is formed on a surface. In the electrode material, an average particle size of the aggregate is 0.5 to 100 μm, a pore size (D50) when an accumulated volume percentage of a pore size distribution of the aggregate is 50% is 0.1 to 0.2 μm, and porosity of the aggregate is 15 to 50 vol % with respect to a volume in a case in which the aggregate is a solid.

## Claims

### Claim 1

An electrode material, comprising:
an aggregate formed by aggregating electrode-active material particles having a carbonaceous film formed on a surface,
wherein an average particle size of the aggregate is 0.5 to 100 μm, and
a volume density of the aggregate is 50 to 80 vol % of the volume density in a case in which the aggregate is a solid.

### Claim 2 (depends on 1)

The electrode material according to claim 1,
wherein 80% or more of the surface of the electrode-active material is covered with the carbonaceous film.

### Claim 3 (depends on 1)

The electrode material according to claim 1,
wherein the aggregate is a shell-like aggregate having a void at the inside, and
a ratio of an average film thickness of the carbonaceous film in an outer peripheral portion and an inner peripheral portion of an outer shell of the shell-like aggregate (a thickness of the carbonaceous film in the inner peripheral portion/a thickness of the carbonaceous film in the outer peripheral portion) is 0.7 to 1.3.

### Claim 4 (depends on 1)

The electrode material according to claim 1,
wherein an amount of carbon in the carbonaceous film is 0.6 to 10 parts by mass on the basis of 100 parts by mass of the electrode-active material.

### Claim 5 (depends on 1)

The electrode material according to claim 1, wherein a tap density of the aggregate is 1.0 to 1.5 g/cm3.

### Claim 6 (depends on 1)

The electrode material according to claim 1,
wherein the electrode-active material contains one kind selected from the group consisting of lithium cobaltate, lithium nickelate, lithium manganate, lithium titanate, and LixAyDzPO4 (provided that, A is one or more kinds selected from the group consisting from Co, Mn, Ni, Fe, Cu, and Cr, D is one or more kinds selected from the group consisting of Mg, Ca, S, Sr, Ba, Ti, Zn, B, Al, Ga, In, Si, Ge, Sc, Y, and rare-earth elements, 0<x<2, 0<y<1.5, and 0≦z<1.5) as a main component.

### Claim 7

A method for producing an electrode material, comprising:
drying slurry which contains an electrode-active material or a precursor of the electrode-active material, and an organic compound, and in which a ratio (D90/D10) of D90 to D10 of a particle size distribution of the electrode-active material or the precursor of the electrode-active material is 5 to 30; and
baking the resultant dried product that is obtained at 500° C. to 1,000° C. in a non-oxidizing atmosphere.

### Claim 8

An electrode material, comprising:
an aggregate formed by aggregating electrode-active material particles having a carbonaceous film formed on a surface,
wherein an average particle size of the aggregate is 0.5 to 100 μm,
a pore size (D50) when an accumulated volume percentage of a pore size distribution of the aggregate is 50% is 0.1 to 0.2 μm, and
porosity of the aggregate is 15 to 50 vol % with respect to a volume in a case in which the aggregate is a solid.

### Claim 9 (depends on 8)

The electrode material according to claim 8,
wherein 80% or more of the surface of the electrode-active material is covered with the carbonaceous film.

### Claim 10 (depends on 8)

The electrode material according to claim 8,
wherein the aggregate is a shell-like aggregate having a void at the inside, and
a ratio of an average film thickness of the carbonaceous film in an outer peripheral portion and an inner peripheral portion of an outer shell of the shell-like aggregate (a thickness of the carbonaceous film in the inner peripheral portion/a thickness of the carbonaceous film in the outer peripheral portion) is 0.7 to 1.3.

### Claim 11 (depends on 8)

The electrode material according to claim 8,
wherein an amount of carbon in the carbonaceous film is 0.6 to 10 parts by mass on the basis of 100 parts by mass of the electrode-active material.

### Claim 12 (depends on 8)

The electrode material according to claim 8,
wherein a tap density of the aggregate is 1.0 to 1.5 g/cm3.

### Claim 13 (depends on 8)

The electrode material according to claim 8,
wherein the electrode-active material contains one kind selected from the group consisting of lithium cobaltate, lithium nickelate, lithium manganate, lithium titanate, and LixAyDzPO4 (provided that, A is one or more kinds selected from the group consisting from Co, Mn, Ni, Fe, Cu, and Cr, D is one or more kinds selected from the group consisting of Mg, Ca, S, Sr, Ba, Ti, Zn, B, Al, Ga, In, Si, Ge, Sc, Y, and rare-earth elements, 0<x<2, 0<y<1.5, and 0≦z<1.5) as a main component.

### Claim 14

A method for producing an electrode material, comprising:
drying slurry which contains an electrode-active material or a precursor of the electrode-active material, and an organic compound, and in which a ratio (D90/D10) of a particle size (D90) when an accumulated volume percentage of a particle size distribution of the electrode-active material or the precursor of the electrode-active material is 90% to a particle size (D10) when the accumulated volume percentage is 10% is 5 to 30; and
baking the resultant dried product that is obtained at 500° C. to 1,000° C. in a non-oxidizing atmosphere.