# US 2013/0258480 A1 · Precursor sol of aluminum oxide and method for manufacturing the same, method for manufacturing optical member, optical member, and optical system

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2013/0258480 A1
- Document ID: US20130258480A1
- Status: Published application
- Kind: A1
- Application number: 13/830,061
- Filed: 2013-03-14
- Published: 2013-10-03
- Earliest claimed: 2012-03-29
- Assignees: Canon Kabushiki Kaisha
- Applicants: Canon Kabushiki Kaisha
- Inventors: Kenji Makino; Tomonari Nakayama; Keiko Abe; Katsuaki Kuge; Hijiri Hasegawa
- Web page: https://patentgrep.com/patent/US20130258480A1

## CPC

- G02B 1/118: having sub-optical wavelength surface structures designed to provide an enhanced transmittance, e.g. moth-eye structures
- C09D 1/00: Coating compositions, e.g. paints, varnishes or lacquers, based on inorganic substances
- C09D 5/006: {Anti-reflective coatings}
- G02B 1/11: Anti-reflection coatings
- G02B 1/113: using inorganic layer materials only
- C01F 7/02: Aluminium oxide; Aluminium hydroxide; Aluminates
- G02B: OPTICAL ELEMENTS, SYSTEMS OR APPARATUS
- C09D: COATING COMPOSITIONS, e.g. PAINTS, VARNISHES OR LACQUERS; FILLING PASTES; CHEMICAL PAINT OR INK REMOVERS; INKS; CORRECTING FLUIDS; WOODSTAINS; PASTES OR SOLIDS FOR COLOURING OR PRINTING; USE OF MATERIALS THEREFOR (cosmetics A61K; processes for applying liquids or other fluent materials to surfaces, in general, B05D; staining wood B27K5/02; glazes or vitreous enamels C03C; natural resins, French polish, drying-oils, driers, turpentine, per se, C09F; polishing compositions other than French polish, ski waxes C09G; adhesives or use of materials as adhesives C09J; materials for sealing or packing joints or covers C09K3/10; materials for stopping leaks C09K3/12; processes for the electrolytic or electrophoretic production of coatings C25D)
- C01F: COMPOUNDS OF THE METALS BERYLLIUM, MAGNESIUM, ALUMINIUM, CALCIUM, STRONTIUM, BARIUM, RADIUM, THORIUM, OR OF THE RARE-EARTH METALS (metal hydrides {monoborane, diborane or addition complexes thereof} C01B6/00; salts of oxyacids of halogens C01B11/00; peroxides, salts of peroxyacids C01B15/00; sulfides or polysulfides of magnesium, calcium, strontium, or barium C01B17/42; thiosulfates, dithionites, polythionates C01B17/64; compounds containing selenium or tellurium C01B19/00; binary compounds of nitrogen with metals C01B21/06; azides C01B21/08; {compounds other than ammonia or cyanogen containing nitrogen and non-metals and optionally metals C01B21/082; amides or imides of silicon C01B21/087}; metal {imides or} amides C01B21/092, {C01B21/0923}; nitrites C01B21/50; {compounds of noble gases C01B23/0005}; phosphides C01B25/08; salts of oxyacids of phosphorus C01B25/16; carbides C01B32/90; compounds containing silicon C01B33/00; compounds containing boron C01B35/00; compounds having molecular sieve properties but not having base-exchange properties C01B37/00; compounds having molecular sieve and base-exchange properties, e.g. crystalline zeolites, C01B39/00; cyanides C01C3/08; salts of cyanic acid C01C3/14; salts of cyanamide C01C3/16; thiocyanates C01C3/20; {double sulfates of magnesium with sodium or potassium C01D5/12; with other alkali metals C01D15/00, C01D17/00})

## Abstract

A precursor sol of aluminum oxide includes particles containing a hydrolysate and/or a condensate of an aluminum compound, a solvent, and an organo aluminum compound. When a pulsed-NMR T2 relaxation curve of nuclide 1H of the precursor sol of aluminum oxide includes two components with different T2 relaxation times and the component with the longer T2 relaxation time has an abundance level of CL (%) and the component with the shorter T2 relaxation time has an abundance level of CS (%), the relative proportion RCS (%) defined by [{CS/(CS+CL)}×100] is in the range of 23.5% to 50.0%, both inclusive.

## Claims

### Claim 1

A precursor sol of aluminum oxide including particles containing a hydrolysate and/or a condensate of an aluminum compound, a solvent, and an organo aluminum compound represented by general formula (1), wherein when a pulsed-NMR T2 relaxation curve of nuclide 1H of the precursor sol of aluminum oxide includes two components with different T2 relaxation times and the component with the longer T2 relaxation time has an abundance level of CL (%) and the component with the shorter T2 relaxation time has an abundance level of CS (%), a relative proportion RCS (%) of CS determined by equation (1) is in a range of 23.5% to 50.0%, both inclusive:
where R1 and R2 denote an alkyl, perfluoroalkyl, or allyl group of one to six carbon atoms, R3 denotes a hydrogen atom, a halogen atom, or an alkyl, perfluoroalkyl, allyl, or aryl group of one to six carbon atoms, and n denotes an integer of 1 to 3, both inclusive.
R
cs
=
C
S
C
S
+
C
L
×
100
(
1
)

### Claim 2 (depends on 1)

The precursor sol of aluminum oxide according to claim 1, wherein the particles containing a hydrolysate and/or a condensate of an aluminum compound have an average particle size of 7.5 nm to 35 nm, both inclusive.

### Claim 3

A method for manufacturing a precursor sol of aluminum oxide including particles containing a hydrolysate and/or a condensate of an aluminum compound, a solvent, and an organo aluminum compound represented by general formula (1), comprising
(A) adding and mixing some amount of a β-diketone and either an aluminum alkoxide or an aluminum salt in the solvent to produce an aluminum compound solution,
(B) adding and mixing some amount of water with or without a catalyst in the solution obtained in (A) to form a condensate of the aluminum alkoxide or aluminum salt and the organo aluminum compound represented by general formula (1), and
(C) heating the solution obtained in (B) to a temperature of 60° C. to 150° C., both inclusive, to obtain the precursor sol of aluminum oxide, wherein
the amount of the β-diketone, the amount of the water added with or without a catalyst, or the temperature of heating the solution obtained in (B) is adjusted so that when a pulsed-NMR T2 relaxation curve of nuclide 1H of the precursor sol of aluminum oxide includes two components with different T2 relaxation times and the component with the longer T2 relaxation time has an abundance level of CL (%) and the component with the shorter T2 relaxation time has an abundance level of CS (%), a relative proportion RCS (%) of CS determined by equation (1) is in a range of 23.5% to 50.0%, both inclusive:
where R1 and R2 denote an alkyl, perfluoroalkyl, or allyl group of one to six carbon atoms, R3 denotes a hydrogen atom, a halogen atom, or an alkyl, perfluoroalkyl, allyl, or aryl group of one to six carbon atoms, and n denotes an integer of 1 to 3, both inclusive.
R
cs
=
C
S
C
S
+
C
L
×
100
(
1
)

### Claim 4 (depends on 3)

The method for manufacturing a precursor sol of aluminum oxide according to claim 3, wherein the β-diketone is a compound represented by general formula (2):
R1COCHR3COR2 General formula (2)
where R1 and R2 denote an alkyl, perfluoroalkyl, or allyl group of one to six carbon atoms, and R3 denotes a hydrogen atom, a halogen atom, or an alkyl, perfluoroalkyl, allyl, or aryl group of one to six carbon atoms.

### Claim 5 (depends on 4)

The method for manufacturing a precursor sol of aluminum oxide according to claim 4, wherein the temperature of heating the solution obtained in (B) is in a range of 75° C. to 130° C., both inclusive.

### Claim 6 (depends on 5)

The method for manufacturing a precursor sol of aluminum oxide according to claim 5, wherein the β-diketone is 3-methyl-2,4-pentanedione.

### Claim 7 (depends on 6)

The method for manufacturing a precursor sol of aluminum oxide according to claim 6, wherein the amount of the water added with or without a catalyst is in a range of 1.65 mol to less than 2 mol per mol of the aluminum compound.

### Claim 8 (depends on 4)

The method for manufacturing a precursor sol of aluminum oxide according to claim 4, wherein the β-diketone is acetylacetone.

### Claim 9 (depends on 4)

The method for manufacturing a precursor sol of aluminum oxide according to claim 4, wherein the β-diketone is 3-ethyl-2,4-pentanedione.

### Claim 10 (depends on 3)

The method for manufacturing a precursor sol of aluminum oxide according to claim 3, wherein the solvent is a monohydric alcohol of five to eight carbon atoms.

### Claim 11 (depends on 1)

A method for manufacturing an optical member, comprising (a) supplying the precursor sol of aluminum oxide according to claim 1 to at least either side of a base, (b) drying and/or baking the precursor sol of aluminum oxide supplied to the base to form an aluminum oxide film, and (c) bringing the aluminum oxide film into contact with hot water or steam at 60° C. to 100° C., both inclusive, to make a crystalline matter containing aluminum oxide separate out, thereby forming a textured structure containing aluminum oxide crystals.

### Claim 12 (depends on 11)

The method for manufacturing an optical member according to claim 11, wherein the precursor sol of aluminum oxide is supplied to the base by spin coating.

### Claim 13 (depends on 11)

The method for manufacturing an optical member according to claim 11, wherein the aluminum oxide film has a thickness of 160 nm to 300 nm, both inclusive.

### Claim 14 (depends on 11)

An optical member produced by the method for manufacturing an optical member according to claim 11.

### Claim 15 (depends on 14)

The optical member according to claim 14, wherein the textured structure is an aluminum oxide nanostructure and exhibits an apparent refractive index varying in the thickness direction while always being less than the specific refractive index of aluminum oxide.

### Claim 16 (depends on 14)

An optical system comprising the optical member according to claim 14.