# US 2013/0256933 A1 · Microporous polyethylene membrane, its production method and battery separator

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2013/0256933 A1
- Document ID: US20130256933A1
- Status: Published application
- Kind: A1
- Application number: 13/902,259
- Filed: 2013-05-24
- Published: 2013-10-03
- Earliest claimed: 2005-08-04
- Assignees: Toray Battery Separator Film Co., Ltd.
- Applicants: Toray Battery Separator Film Co., Ltd.
- Inventors: Kotaro TAKITA; Shintaro KIKUCHI; Kazuhiro YAMADA; Teiji NAKAMURA; Koichi KONO
- Web page: https://patentgrep.com/patent/US20130256933A1

## CPC

- B29C 48/08: flexible, e.g. films
- B01D 67/0074: {from melts}
- B01D 69/02: characterised by their properties
- B01D 71/261: {Polyethylene}
- B01D 71/262: {Polypropylene}
- B29C 48/0018: {combined with shaping by orienting, stretching or shrinking, e.g. film blowing (B29C48/0017 takes precedence)}
- B29C 48/9135: {of flat articles, e.g. using specially adapted supporting means}
- B29C 48/914: {Cooling drums}
- H01G 9/02: Diaphragms; Separators
- H01M 50/406: Moulding; Embossing; Cutting
- H01M 50/417: Polyolefins
- B01D 2323/08: Specific temperatures applied
- B01D 2323/12: Specific ratios of components used
- B01D 2325/0233: with clearly distinguishable layers
- B01D 2325/0283: Pore size
- B01D 2325/341: At least two polymers of same structure but different molecular weight
- B29C 48/305: having a wide opening, e.g. for forming sheets
- B29C 48/917: {by applying pressurised gas to the surface of the flat article}
- B29K 2023/06: {PE, i.e. polyethylene}
- B29K 2105/04: cellular or porous
- H01M 10/052: Li-accumulators
- H01M 50/489: Separators, membranes, diaphragms or spacing elements inside the cells, characterised by their physical properties, e.g. swelling degree, hydrophilicity or shut down properties
- H01M 50/491: Porosity
- Y02E 60/10: Energy storage using batteries
- Y10T 428/2495: Thickness [relative or absolute]
- Y10T 428/249978: Voids specified as micro
- B29C: SHAPING OR JOINING OF PLASTICS; SHAPING OF MATERIAL IN A PLASTIC STATE, NOT OTHERWISE PROVIDED FOR; AFTER-TREATMENT OF THE SHAPED PRODUCTS, e.g. REPAIRING (making preforms B29B11/00; making laminated products by combining previously unconnected layers which become one product whose layers will remain together B32B37/00 - B32B41/00)
- B01D: SEPARATION (separating solids from solids by wet methods B03B, B03D; by pneumatic jigs or tables B03B; by other dry methods B07; magnetic or electrostatic separation of solid materials from solid materials or fluids, separation by high-voltage electric fields B03C; centrifuges, vortex apparatus B04; presses per se for squeezing-out liquid from liquid-containing material B30B9/02; treatment of water C02F, e.g. softening by ion-exchange C02F1/42; {arrangements of air intake cleaners in gas turbine plants F02C7/05} ; arrangements or mounting of filters in air-conditioning, air-humidification or ventilation F24F13/28)
- H01G: CAPACITORS; CAPACITORS, RECTIFIERS, DETECTORS, SWITCHING DEVICES, LIGHT-SENSITIVE OR TEMPERATURE-SENSITIVE DEVICES OF THE ELECTROLYTIC TYPE (selection of specified materials as dielectric H01B3/00; capacitors having potential barriers H10D1/62, H10K10/10)
- H01M: PROCESSES OR MEANS, e.g. BATTERIES, FOR THE DIRECT CONVERSION OF CHEMICAL ENERGY INTO ELECTRICAL ENERGY
- B29K: INDEXING SCHEME ASSOCIATED WITH SUBCLASSES B29B, B29C OR B29D, RELATING TO MOULDING MATERIALS OR TO MATERIALS FOR {MOULDS, } REINFORCEMENTS, FILLERS OR PREFORMED PARTS, e.g. INSERTS
- Y02E: REDUCTION OF GREENHOUSE GAS [GHG] EMISSIONS, RELATED TO ENERGY GENERATION, TRANSMISSION OR DISTRIBUTION
- Y10T: TECHNICAL SUBJECTS COVERED BY FORMER US CLASSIFICATION

## Abstract

A microporous polyethylene membrane made of a polyethylene resin comprising 15% or less by mass of ultra-high-molecular-weight polyethylene having a mass-average molecular weight of 1×106 or more, which is constituted by a dense-structure layer having an average pore diameter of 0.01 to 0.05 μm, and a coarse-structure layer formed on at least one surface and having an average pore diameter 1.2-fold to 5.0-fold of that of the dense-structure layer, has a high electrolytic solution absorption speed with thickness and air permeability little changing when compressed. Such a microporous polyethylene membrane is produced by extruding a melt blend of the above polyethylene resin and a membrane-forming solvent through a die, cooling the resultant extrudate with a temperature distribution in a thickness direction to provide a gel-like sheet, stretching the gel-like sheet at a temperature from the crystal dispersion temperature of the polyethylene resin +10° C. to the crystal dispersion temperature +30° C., removing the membrane-forming solvent, and stretching the membrane again to 1.05-fold to 1.45-fold.

## Claims

### Claim 1

A method for producing a microporous polyethylene membrane comprising the steps of extruding a melt blend of a polyethylene resin comprising 15% or less by mass of ultra-high-molecular-weight polyethylene having a mass-average molecular weight of 1×106 or more and a membrane-forming solvent through a die, cooling the resultant extrudate with a temperature distribution in a thickness direction to provide a gel-like sheet, stretching the gel-like sheet at a temperature from the crystal dispersion temperature of the polyethylene resin +10° C. to the crystal dispersion temperature +30° C. in at least one direction, removing the membrane-forming solvent, and stretching the resultant membrane again to 1.05-fold to 1.45-fold in at least one direction.

### Claim 2 (depends on 1)

The method for producing a microporous polyethylene membrane according to claim 1, wherein the gel-like sheet is formed by rapidly cooling one surface of the extrudate while slowly cooling another surface of the extrudate.

### Claim 3 (depends on 2)

The method for producing a microporous polyethylene membrane according to claim 2, wherein the gel-like sheet is formed by rapidly cooling one surface of the extrudate by a cooling roll controlled at a temperature from the crystallization temperature of the polyethylene resin −115° C. to the crystallization temperature −25° C. for a contact time of 1 to 30 seconds, while slowly cooling another surface of the extrudate by exposure to the air at room temperature.

### Claim 4 (depends on 1)

The method for producing a microporous polyethylene membrane according to claim 1, wherein after the stretched gel-like sheet is heat-set, the membrane-forming solvent is removed.

### Claim 5 (depends on 1)

The method for producing a microporous polyethylene membrane according to claim 1, wherein the stretched gel-like sheet, and/or a microporous membrane from which the membrane-forming solvent is removed are brought into contact with a heated solvent.