# US 2013/0256845 A1 · Semiconductor Device and Method for Manufacturing the Same

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2013/0256845 A1
- Document ID: US20130256845A1
- Status: Published application
- Kind: A1
- Application number: 13/512,330
- Filed: 2012-04-09
- Published: 2013-10-03
- Earliest claimed: 2012-03-29
- Assignees: The Institute of Microelectronics Chinese Academy of Science
- Inventors: Haizhou Yin; Wei Jiang
- Web page: https://patentgrep.com/patent/US20130256845A1

## CPC

- H10W 10/014: {using trench refilling with dielectric materials, e.g. shallow trench isolations}
- H10W 10/17: formed using trench refilling with dielectric materials, e.g. shallow trench isolations
- H10D 30/601: {having lightly-doped drain or source extensions, e.g. LDD IGFETs or DDD IGFETs (lightly doped source or drain extensions for TFTs H10D30/6715)}
- H10W 10/0145: {of trenches having shapes other than rectangular or V-shape (H10W10/0143 takes precedence)}
- H10W: GENERIC PACKAGES, INTERCONNECTIONS, CONNECTORS OR OTHER CONSTRUCTIONAL DETAILS OF DEVICES COVERED BY CLASS H10
- H10D: INORGANIC ELECTRIC SEMICONDUCTOR DEVICES

## Abstract

The present invention discloses a semiconductor device, which comprises: a substrate, and a shallow trench isolation in the substrate, characterized in that, the semiconductor device further comprises a stress release layer between the substrate and the shallow trench isolation. In the semiconductor device and the method for manufacturing the same according to the present invention, the stresses accumulated during the formation of the STI can be released by interposing the stress release layer made of a softer material between the substrate and the STI, thereby reducing the leakage current of the substrate of the device and improving the device reliability.

## Claims

### Claim 1

A semiconductor device, comprising: a substrate, and a shallow trench isolation in the substrate, wherein the semiconductor device further comprises a stress release layer between the substrate and the shallow trench isolation.

### Claim 2 (depends on 1)

The semiconductor device according to claim 1, wherein the stress release layer comprises one of BSG and BPSG.

### Claim 3 (depends on 1)

The semiconductor device according to claim 1, wherein the thickness of the stress release layer is about 10-15 nm.

### Claim 4 (depends on 1)

The semiconductor device according to claim 1, wherein the semiconductor device further comprises a liner between the stress release layer and the substrate.

### Claim 5 (depends on 4)

The semiconductor device according to claim 4, wherein the liner includes at least a first liner of oxide and a second liner of nitride.

### Claim 6 (depends on 1)

The semiconductor device according to claim 1, wherein a semiconductor device structure is formed in an active region surrounded by the shallow trench isolation.

### Claim 7

A method for manufacturing a semiconductor device, comprising:
forming a shallow trench in a substrate;
forming a stress release layer in the shallow trench;
filling the shallow trench with an insulating material to form a shallow trench isolation; and
performing an annealing step to enable rheidity of the stress release layer so as to release stresses.

### Claim 8 (depends on 7)

The method for manufacturing a semiconductor device according to claim 7, wherein the stress release layer comprises one of BSG and BPSG.

### Claim 9 (depends on 7)

The method for manufacturing a semiconductor device according to claim 7, wherein the thickness of the stress release layer is about 10-15 nm.

### Claim 10 (depends on 7)

The method for manufacturing a semiconductor device according to claim 7, wherein after forming the shallow trench and before forming the stress release layer, the method further comprises forming a liner in the shallow trench.

### Claim 11 (depends on 10)

The method for manufacturing a semiconductor device according to claim 10, wherein the liner includes at least a first liner of oxide and a second liner of nitride.

### Claim 12 (depends on 7)

The method for manufacturing a semiconductor device according to claim 7, wherein the annealing is performed at a temperature higher than 600° C.

### Claim 13 (depends on 7)

The method for manufacturing a semiconductor device according to claim 7, wherein forming a shallow trench in the substrate comprises:
forming a hard mask layer on the substrate;
photoetching/etching the hard mask layer to form a hard mask layer pattern which has an opening exposing the substrate; and
etching the substrate exposed in the opening with the hard mask layer pattern as a mask to form a shallow trench, the bottom surface of which is lower than the upper surface of the substrate.

### Claim 14 (depends on 13)

The method for manufacturing a semiconductor device according to claim 13, wherein the hard mask layer includes at least a first hard mask layer of oxide and a second hard mask layer of nitride.

### Claim 15 (depends on 7)

The method for manufacturing a semiconductor device according to claim 7, wherein after performing an annealing, the method further comprises forming a semiconductor device structure in an active region surrounded by the shallow trench isolation.