# US 2013/0256580 A1 · Ferroelectric thin film-forming sol-gel solution

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2013/0256580 A1
- Document ID: US20130256580A1
- Status: Published application
- Kind: A1
- Application number: 13/829,125
- Filed: 2013-03-14
- Published: 2013-10-03
- Earliest claimed: 2012-03-30
- Assignees: Mitsubishi Materials Corporation
- Applicants: Mitsubishi Materials Corporation
- Inventors: Toshihiro Doi; Hideaki Sakurai; Toshiaki Watanabe; Nobuyuki Soyama
- Web page: https://patentgrep.com/patent/US20130256580A1

## CPC

- H10N 30/8554: {Lead-zirconium titanate [PZT] based}
- C23C 18/1216: {Metal oxides (C23C18/1212 takes precedence)}
- C23C 18/1254: {Sol or sol-gel processing}
- C23C 18/1283: {Control of temperature, e.g. gradual temperature increase, modulation of temperature}
- C23C 18/1291: {by heating of the substrate}
- H10N: ELECTRIC SOLID-STATE DEVICES NOT OTHERWISE PROVIDED FOR
- C23C: COATING METALLIC MATERIAL; COATING MATERIAL WITH METALLIC MATERIAL; SURFACE TREATMENT OF METALLIC MATERIAL BY DIFFUSION INTO THE SURFACE, BY CHEMICAL CONVERSION OR SUBSTITUTION; COATING BY VACUUM EVAPORATION, BY SPUTTERING, BY ION IMPLANTATION OR BY CHEMICAL VAPOUR DEPOSITION, IN GENERAL (making metal-coated products by extrusion B21C23/22; covering with metal by connecting pre-existing layers to articles, see the relevant places, e.g. B21D39/00, B23K; metallising of glass C03C; metallising mortars, concrete, artificial stone, ceramics or natural stone C04B41/00; enamelling of, or applying a vitreous layer to, metals C23D; treating metal surfaces or coating of metals by electrolysis or electrophoresis C25D; single-crystal film growth C30B; by metallising textiles D06M11/83; decorating textiles by locally metallising D06Q1/04)

## Abstract

When a ferroelectric thin film-forming sol-gel solution contains a PZT-based compound, a viscosity-adjusting macromolecular compound including polyvinylpyrrolidone, and an organic dopant including a formamide-based solvent, the PZT-based compound is included at 17 mass % or more in terms of an oxide, the molar ratio of the polyvinylpyrrolidone to the PZT-based compound is PZT-based compound:polyvinylpyrrolidone=1:0.1 to 0.5 in terms of a monomer, and the formamide-based solvent is included at 3 mass % to 13 mass % of the sol-gel solution, it is possible to form a thick layer by coating the sol-gel solution once, the production efficiency improves, and crack-free and dense film formation even after calcination and firing becomes possible.

## Claims

### Claim 1

A ferroelectric thin film-forming sol-gel solution comprising:
a PZT-based compound;
a viscosity-adjusting macromolecular compound including polyvinylpyrrolidone; and
an organic dopant including a formamide-based solvent,
wherein the PZT-based compound is included at 17 mass % or more in terms of an oxide, a molar ratio of the polyvinylpyrrolidone to the PZT-based compound is PZT-based compound:polyvinylpyrrolidone=1:0.1 to 0.5 in terms of a monomer, and the formamide-based solvent is included at 3 mass % to 13 mass % of the sol-gel solution.

### Claim 2 (depends on 1)

The ferroelectric thin film-forming sol-gel solution according to claim 1,
wherein the formamide-based solvent is formamide, N-methylformamide or N,N-dimethylformamide.

### Claim 3 (depends on 1)

The ferroelectric thin film-forming sol-gel solution according to claim 1,
wherein a k value of the polyvinylpyrrolidone is in a range of 30 to 90.

### Claim 4 (depends on 1)

A method of forming a ferroelectric thin film using the ferroelectric thin film-forming sol-gel solution according to claim 1.

### Claim 5 (depends on 2)

A method of forming a ferroelectric thin film using the ferroelectric thin film-forming sol-gel solution according to claim 2.

### Claim 6 (depends on 3)

A method of forming a ferroelectric thin film using the ferroelectric thin film-forming sol-gel solution according to claim 3.