# US 2013/0256122 A1 · Electrochemically functional membranes

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2013/0256122 A1
- Document ID: US20130256122A1
- Status: Published application
- Kind: A1
- Application number: 13/819,369
- Filed: 2011-08-31
- Published: 2013-10-03
- Earliest claimed: 2010-08-31
- Assignees: President and Fellows of Harvard College
- Inventors: Shriram Ramanathan; Daniel V. Harburg; Masaru Tsuchiya; Alexander C. Johnson
- Web page: https://patentgrep.com/patent/US20130256122A1

## CPC

- C25B 13/02: characterised by shape or form
- H01M 4/9066: {of metal-ceramic composites or mixtures, e.g. cermets}
- H01M 8/02: Details (electrodes H01M4/86 - H01M4/98)
- H01M 8/0247: characterised by the form (characterised by a channel configuration H01M8/0258)
- H01M 8/1253: the electrolyte containing zirconium oxide
- H01M 8/1286: Fuel cells applied on a support, e.g. miniature fuel cells deposited on silica supports
- H01M 2008/1293: {Fuel cells with solid oxide electrolytes}
- Y02E 60/50: Fuel cells
- Y02P 70/50: Manufacturing or production processes characterised by the final manufactured product
- C25B: ELECTROLYTIC OR ELECTROPHORETIC PROCESSES FOR THE PRODUCTION OF COMPOUNDS OR NON-METALS; APPARATUS THEREFOR (anodic or cathodic protection C23F13/00; single-crystal growth C30B)
- H01M: PROCESSES OR MEANS, e.g. BATTERIES, FOR THE DIRECT CONVERSION OF CHEMICAL ENERGY INTO ELECTRICAL ENERGY
- Y02E: REDUCTION OF GREENHOUSE GAS [GHG] EMISSIONS, RELATED TO ENERGY GENERATION, TRANSMISSION OR DISTRIBUTION
- Y02P: CLIMATE CHANGE MITIGATION TECHNOLOGIES IN THE PRODUCTION OR PROCESSING OF GOODS

## Abstract

A system includes an electrochemically functional membrane, and a support structure constructed and arranged so as to support the membrane while leaving within the membrane a chemically active area having an area utilization of at least about 50%. In some embodiments, the support structure may include a plurality of grids that are sized and shaped so that the contact area between the grids and the membrane is reduced to less than about 40%. In some embodiments, the support structure may include aerogels, for example PVA-reinforced CNT aerogels having a conductivity that is increased by pyrolysis. The system may be a gas separation system; a gas production system; a gas purification system; or an energy generation system such as an SOFC.

## Claims

### Claim 1

A system comprising:
an electrochemically functional membrane; and
a support structure constructed and arranged so as to support the membrane while leaving within the membrane a chemically active area having an area utilization of at least about 50%;
wherein the support structure comprises at least one of:
a plurality of grids that are sized and shaped so as to reduce the contact area between the grids and the membrane to less than about 40%; and
one or more aerogels.

### Claim 2 (depends on 1)

The system of claim 1, wherein the system is one of:
a gas separation system; a gas production system; a gas purification system; and
an energy generation system.

### Claim 3 (depends on 2)

The system of claim 2, further comprising a substrate, and an electrode layer deposited on each side of the membrane.

### Claim 4 (depends on 1)

The system of claim 1, wherein the grids comprise plated metallic grids, and wherein the energy generation system comprises an SOFC.

### Claim 5 (depends on 4)

The system of claim 4, wherein the grids are constructed by:
depositing the membrane and a cathode layer on a substrate;
etching metallic grids by DC-sputtering on the surface of the cathode layer; and
forming a back-side pattern by reactive ion etching and wet etching of the substrate.

### Claim 6 (depends on 5)

The system of claim 5, wherein the grids comprise nickel and have a line width of about 5-10 μm and a pitch of 25-50 μm; and wherein the membrane is a LSCF/yttrium-stabilized zirconium/platinum membrane having a thickness of about 200 μm.

### Claim 7 (depends on 4)

The system of claim 4, wherein shapes of the grids comprise one of: a hexagon; and a circle.

### Claim 8 (depends on 4)

The system of claim 4, wherein the grids comprise Pt or Ag, and have a thickness of about 1 micrometers.

### Claim 9 (depends on 8)

The system of claim 8, wherein the membrane is a 8 mol % yttrium doped zirconium membrane having a thickness of about 50 to about 150 nm, and wherein the area utilization of the membrane is more than 85%.

### Claim 10 (depends on 1)

The system of claim 1, wherein the aerogels comprise a silica aerogel reinforced with carbon fibers.

### Claim 11 (depends on 10)

The system of claim 10, wherein the silica aerogel is created in flow channels etched into the underside of a silicon chip bonded to the top of the membrane.

### Claim 12 (depends on 1)

The system of claim 1, wherein the aerogels comprise a PVA (polyvinyl alcohol)-reinforced CNT (carbon nanotube) aerogel having a conductivity that is increased by pyrolysis.

### Claim 13 (depends on 12)

The system of claim 12, wherein the PVA-reinforced CNT aerogel is fabricated by:
suspending CNTs in water to form a gel;
performing PVA infiltration by covering the gel with a water/PVA solution;
replacing the water with alcohol and then with CO2;
super critically removing the CO2; and
pyrolyzing the gel by heating it to a temperature between about 400 and 1000° C.

### Claim 14

A system comprising:
a substrate;
an electrochemically functional membrane deposited on the substrate;
a cathode layer deposited on the membrane; and
a plurality of supporting grids etched on the surface of the cathode layer according to a grid pattern;
wherein the grids are shaped and sized so as to support the membrane while reducing the contact area between the grids and the membrane to less than about 15%, thereby leaving within the membrane a chemically active area having an area utilization of at least about 60%.

### Claim 15 (depends on 14)

The system of claim 14, wherein the grid pattern ends outside the active area of the membrane so that current collected in the grid can flow down to the substrate.

### Claim 16 (depends on 14)

The system of claim 14, wherein the substrate is a Si substrate coated with an insulating layer; and wherein the insulating layer is patterned with the grid pattern.

### Claim 17 (depends on 16)

The system of claim 16, wherein the plurality of grids comprise a current collector grid etched on the patterned insulating layer.

### Claim 18 (depends on 14)

The system of claim 14, wherein the membrane is a nanostructured electrolyte membrane comprising yttrium doped zirconia; and wherein the cathode layer comprises LSCF.

### Claim 19 (depends on 14)

The system of claim 14, wherein the substrate has a back-side pattern etched thereon by reactive ion etching and wet etching.

### Claim 20 (depends on 14)

The system of claim 14, wherein the grids comprise one of: a metal, and a semiconductor material; and wherein the shapes of the grids comprise one of: a hexagon; and a circle.

### Claim 21

A method of fabricating grids for supporting an electrochemically functional membrane in a device, the method comprising:
depositing a layer of the electrochemically functional membrane on a silicon wafer that is coated both sides with silicon nitride;
sputtering a layer of metal onto the surface of the wafer, and patterning the layer of matter into a grid pattern using photolithography;
patterning the nitride from the back side, and etching the wafer through; and
removing the silicon nitride from the back side of the wafer,
wherein the grid pattern shapes a plurality of grids so as to decrease the contact area between each grid and the membrane to less than about 40% of the total area of the membrane.

### Claim 22 (depends on 21)

The method of claim 21, wherein the grid comprises a current collector grid for the device.

### Claim 23

A method of increasing the active area of an electrochemically functional membrane, the method comprising:
depositing the membrane on a substrate;
covering the membrane with a high porosity material; and
removing the substrate.

### Claim 24 (depends on 23)

The method of claim 23, wherein the high porosity material comprises silica aerogel reinforced with carbon fibers.

### Claim 25 (depends on 24)

The method of claim 24, wherein the aerogel is created in flow channels etched into the underside of a silicon chip bonded to the top of the membrane.

### Claim 26

A method of fabricating a PVA (polyvinyl alcohol) reinforced CNT (carbon nanotube) aerogel for supporting an electrochemically functional membrane in a system, the method comprising:
suspending CNTs in water to form a gel;
performing PVA infiltration by covering the gel with a water/PVA solution;
replacing the water with alcohol and then with CO2;
super critically removing the CO2; and
pyrolyzing the gel by heating it to a temperature between about 400 and 1000° C.