# US 2013/0255074 A1 · Method for manufacturing lithium ion secondary battery

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2013/0255074 A1
- Document ID: US20130255074A1
- Status: Published application
- Kind: A1
- Application number: 13/991,186
- Filed: 2010-12-06
- Published: 2013-10-03
- Earliest claimed: 2010-12-06
- Assignees: Toyota Jidosha Kabushiki Kaisha
- Inventors: Yozo Uchida; Nobuyuki Yamazaki; Tomohide Sumi; Tomohiko Ishida
- Web page: https://patentgrep.com/patent/US20130255074A1

## CPC

- H01M 4/622: {being polymers}
- H01M 4/0404: {by coating on electrode collectors}
- H01M 4/139: Processes of manufacture
- H01M 4/1393: of electrodes based on carbonaceous material, e.g. graphite-intercalation compounds or CFx
- H01M 4/587: for inserting or intercalating light metals
- H01M 4/621: {Binders}
- Y02E 60/10: Energy storage using batteries
- Y02P 70/50: Manufacturing or production processes characterised by the final manufactured product
- Y10T 29/49115: including coating or impregnating
- H01M: PROCESSES OR MEANS, e.g. BATTERIES, FOR THE DIRECT CONVERSION OF CHEMICAL ENERGY INTO ELECTRICAL ENERGY
- Y02E: REDUCTION OF GREENHOUSE GAS [GHG] EMISSIONS, RELATED TO ENERGY GENERATION, TRANSMISSION OR DISTRIBUTION
- Y02P: CLIMATE CHANGE MITIGATION TECHNOLOGIES IN THE PRODUCTION OR PROCESSING OF GOODS
- Y10T: TECHNICAL SUBJECTS COVERED BY FORMER US CLASSIFICATION

## Abstract

The method for manufacturing a lithium ion secondary battery includes a binder coating step (18), a mixture supplying step (20), a magnetic field applying step (22), and a convection generating step (24). The binder coating step (18) is a step of coating a slurry-form binder (18a) on a metal foil (12a) (collector). The mixture supplying step (20) is a step of supplying a negative electrode mixture containing graphite so as to be superposed on the slurry-form binder (18a) coated on the metal foil (12a) in the binder coating step (18). The magnetic field applying step (22) is a step of applying a magnetic field having magnetic lines of force pointing in the direction orthogonal to the metal foil (12a), to the negative electrode mixture (20a) coated on the metal foil (12a) in the mixture supplying step (20). Further, the convection generating step (24) is a step of generating convection in the negative electrode mixture (20a) by applying heat to the negative electrode mixture (20a) to which a magnetic field has been applied in the magnetic field applying step (22).

## Claims

### Claim 1

A method for manufacturing a lithium ion secondary battery, comprising:
a binder coating step of coating a slurry-form binder containing a binding agent on a collector;
a mixture supplying step of supplying a negative electrode mixture containing graphite, so as to be superposed on the slurry-form binder having been coated on the collector in the binder coating step;
a magnetic field applying step of applying a magnetic field having magnetic lines of force pointing in a direction orthogonal to a plane of the collector having been supplied with the negative electrode mixture, to the negative electrode mixture having been supplied to the collector in the mixture supplying step; and
a convection generating step of generating convection in the negative electrode mixture by applying heat to the negative electrode mixture to which the magnetic field has been applied in the magnetic field applying step.

### Claim 2 (depends on 1)

The method for manufacturing a lithium ion secondary battery according to claim 1, wherein the graphite has a layered structure including hexagonal platelet-shaped crystals stacked one on another in such a manner as to form a plurality of layers.

### Claim 3 (depends on 1)

The method for manufacturing a lithium ion secondary battery according to claim 1, wherein the graphite has a flat flake shape.

### Claim 4 (depends on 1)

The method for manufacturing a lithium ion secondary battery according to claim 1, wherein the binding agent is SBR.

### Claim 5 (depends on 1)

The method for manufacturing a lithium ion secondary battery according to claim 1, wherein the slurry-form binder to be coated in the binder coating step has a viscosity (Adv) satisfying 50 mPa·sec≦Adv≦2000 mPa·sec.

### Claim 6 (depends on 1)

The method for manufacturing a lithium ion secondary battery according to claim 1, wherein the slurry-form binder to be coated in the binder coating step has a solid content concentration (Ads) satisfying 5 wt %≦Ads≦20 wt %.

### Claim 7 (depends on 1)

The method for manufacturing a lithium ion secondary battery according to claim 1, wherein the slurry-form binder to be coated in the binder coating step has a thickness (At) satisfying 1.0 μm≦At≦10.0 μm.

### Claim 8 (depends on 1)

The method for manufacturing a lithium ion secondary battery according to claim 1, wherein in the binder coating step, the slurry-form binder is coated on the collector by gravure printing.

### Claim 9 (depends on 1)

The method for manufacturing a lithium ion secondary battery according to claim 1, wherein the negative electrode mixture to be supplied in the mixture supplying step is free from a binding agent.

### Claim 10 (depends on 1)

The method for manufacturing a lithium ion secondary battery according to claim 1, wherein the negative electrode mixture to be supplied in the mixture supplying step has a viscosity (Bdv) satisfying 500 mPa·sec≦Bdv≦5000 mPa·sec.

### Claim 11 (depends on 1)

The method for manufacturing a lithium ion secondary battery according to claim 1, wherein the negative electrode mixture to be supplied in the mixture supplying step has a solid content concentration (Bds) satisfying 40 wt %≦Bds≦60 wt %.

### Claim 12 (depends on 1)

The method for manufacturing a lithium ion secondary battery according to claim 1, wherein the magnetic field applying step and the convection generating step are performed at the same timing, thereby to apply a magnetic field having magnetic lines of force pointing in a direction orthogonal to the collector, to the negative electrode mixture having been coated on the collector in the mixture supplying step, and to generate convention by applying heat to the negative electrode mixture.

### Claim at position 13

-15. (canceled)