# US 2013/0253209 A1 · Process for the start-up of an epoxidation process

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2013/0253209 A1
- Document ID: US20130253209A1
- Status: Published application
- Kind: A1
- Application number: 13/613,896
- Filed: 2012-09-13
- Published: 2013-09-26
- Earliest claimed: 2011-09-22
- Assignees: Shell Oil Company
- Inventors: Randall Clayton YEATES
- Web page: https://patentgrep.com/patent/US20130253209A1

## CPC

- C07D 301/10: with catalysts containing silver or gold
- Y02P 20/141: Feedstock
- Y02P 20/52: using catalysts, e.g. selective catalysts
- C07D: HETEROCYCLIC COMPOUNDS (macromolecular compounds C08)
- Y02P: CLIMATE CHANGE MITIGATION TECHNOLOGIES IN THE PRODUCTION OR PROCESSING OF GOODS

## Abstract

The present disclosure provides processes for the start-up of an ethylene epoxidation process comprising: a. contacting a high selectivity epoxidation catalyst with a feed comprising ethylene, oxygen and an organic chloride for a period of time such that vinyl chloride is produced and capable of being detected in a reactor outlet stream or a recycle gas loop; b. increasing the temperature of the high selectivity epoxidation catalyst to at least about 220° C.; c. subsequently reducing the level of organic chloride in the feed over a period of from about 12 to about 36 hours so as to increase the temperature of the catalyst to a temperature of from about 250° C. to about 265° C.; and d. subsequently adjusting the level of organic chloride in the feed to a value sufficient to produce ethylene oxide at a substantially optimum selectivity at a temperature of from about 250° C. to about 265° C.

## Claims

### Claim 1

A process for the start-up of an ethylene epoxidation process comprising:
a. contacting a high selectivity epoxidation catalyst with a feed comprising ethylene, oxygen and an organic chloride for a period of time such that vinyl chloride is produced and capable of being detected in a reactor outlet stream or a recycle gas loop;
b. increasing the temperature of the high selectivity epoxidation catalyst to at least about 220° C.;
c. subsequently reducing the level of organic chloride in the feed over a period of from about 12 to about 36 hours so as to increase the temperature of the catalyst to a temperature of from about 250° C. to about 265° C.; and
d. subsequently adjusting the level of organic chloride in the feed to a value sufficient to produce ethylene oxide at a substantially optimum selectivity at a temperature of from about 250° C. to about 265° C.

### Claim 2 (depends on 1)

The process of claim 1 wherein at least 1×10−5 mole-% of vinyl chloride is detected in the reactor outlet stream or the recycle gas loop.

### Claim 3 (depends on 1)

The process of claim 1 wherein the feed in step (a) comprises organic chloride in a quantity of from about 1 to about 12 millimolar equivalent of chloride per kilogram of catalyst.

### Claim 4 (depends on 3)

The process of claim 3 wherein the feed in step (c) comprises organic chloride in a quantity of from about 25 to about 75 weight percent of the quantity of organic chloride present in the feed in step (a).

### Claim 5 (depends on 3)

The process of claim 3 wherein the level of organic chloride added to the feed in step (c) is zero.

### Claim 6 (depends on 1)

The process of claim 1 wherein the organic chloride is selected from the group consisting of methyl chloride, ethyl chloride, ethylene dichloride, vinyl chloride and mixtures thereof.

### Claim 7 (depends on 6)

The process of claim 6 further comprising:
e. subsequently heating the high selectivity epoxidation catalyst to a temperature of from about 250° C. to about 275° C. for a period of time between about 12 to about 150 hours.

### Claim 8 (depends on 1)

The process of claim 1 wherein the high selectivity epoxidation catalyst comprises a carrier that comprises silver, a rhenium promoter, a first co-promoter, and a second co-promoter; wherein: the quantity of the rhenium promoter is greater than about 1 mmole/kg, relative to the weight of the catalyst; the first co-promoter is selected from sulfur, phosphorus, boron, and mixtures thereof; and the second co-promoter is selected from tungsten, molybdenum, chromium, and mixtures thereof.

### Claim 9 (depends on 8)

The process of claim 8 wherein the total quantity of the first co-promoter and the second co-promoter is at most 10 mmole/kg, relative to the weight of the catalyst; and wherein the carrier has one or more properties selected from the group consisting of: a monomodal, bimodal or multimodal pore size distribution, a maximum pore diameter range of from about 0.01 μm to about 200 μm, a specific surface area of from about 0.03 m2/g to about 10 m2/g, a pore volume of from about 0.2 cm3/g to about 0.7 cm3/g, a median pore diameter of from about 0.1 μm to about 100 μm, and a water absorption of from about 10% to about 80%.

### Claim 10 (depends on 1)

The process of claim 1 wherein the feed further comprises carbon dioxide in amount of less than about 2%.