# US 2013/0253182 A1 · Polymer film, and optically-compensatory film, polarizer and liquid-crystal display device comprising the same

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2013/0253182 A1
- Document ID: US20130253182A1
- Status: Published application
- Kind: A1
- Application number: 13/890,398
- Filed: 2013-05-09
- Published: 2013-09-26
- Earliest claimed: 2004-08-09
- Assignees: FUJIFILM Corporation
- Applicants: FUJIFILM Corporation
- Inventors: Tadashi OMATSU; Hajime Nakayama; Akihiro Matsufuji; Osamu Takahashi; Shigeaki Nimura; Yousuke Nishiura
- Web page: https://patentgrep.com/patent/US20130253182A1

## CPC

- G02B 1/08: made of polarising materials
- C08J 7/12: Chemical modification
- G02B 5/3016: {involving passive liquid crystal elements (optical properties of liquid crystals G02F1/0063; polarising elements associated with active liquid crystal devices G02F1/133528)}
- C08J 2301/10: Esters of organic acids
- C09K 2323/031: Polarizer or dye
- Y10T 428/31: Surface property or characteristic of web, sheet or block
- G02B: OPTICAL ELEMENTS, SYSTEMS OR APPARATUS
- C08J: WORKING-UP; GENERAL PROCESSES OF COMPOUNDING; AFTER-TREATMENT NOT COVERED BY SUBCLASSES C08B, C08C, C08F, C08G or C08H (working, e.g. shaping, of plastics B29)
- C09K: MATERIALS FOR MISCELLANEOUS APPLICATIONS, NOT PROVIDED FOR ELSEWHERE
- Y10T: TECHNICAL SUBJECTS COVERED BY FORMER US CLASSIFICATION

## Abstract

A polymer film that has an in-plane retardation Re(λ) and a thickness-direction retardation Rth(λ) satisfying formula (i) and (ii), and that further has a surface energy of at least one surface is from 50 mN/m to 80 mN/m: 0≦Re(630)≦10, and |Rth(630)|≦25; (i) and |Re(400)−Re(700)|≦10, and |Rth(400)−Rth(700)|≦35. (ii) in the formulae, Re(λ) and Rth(λ) are measurement values at the wavelength of λ nm, and an optically-compensatory film, an optical material such as a polarizer and a liquid-crystal display device using the polymer film.

## Claims

### Claim 1

A polymer film that has an in-plane retardation Re(λ) and a thickness-direction retardation Rth(λ) (where λ indicates a wavelength (nm)) satisfying formulae (i) and (ii), and that further has a surface energy of at least one surface is from 50 mN/m to 80 mN/m:
0≦Re(630)≦1.7 nm, and |Rth(630)|≦15.0; (i)
and
|Re(400)−Re(700)|≦2 nm, and |Rth(400)−Rth(700)|≦20 nm, (ii)
wherein a polymer material to form the film comprises a cellulose acylate.

### Claim 2 (depends on 1)

The polymer film according to claim 1,
wherein an in-plane distribution of the surface energy of the polymer film, ΔE is 10 or less.

### Claim 3 (depends on 1)

The polymer film according to claim 1,
wherein at least one surface of the polymer film is surface-treated, and a surface energy of the surface-treated surface is from 30 mN/m to 50 mN/m before a surface treatment, and a surface energy of the surface-treated surface is from 50 mN/m to 80 mN/m after the surface treatment.

### Claim 4 (depends on 1)

The polymer film according to claim 1,
wherein an in-plane distribution of Re(λ) and Rth(λ), ΔRe(λ) and ΔRth(λ) satisfy formula (iii) and (iv):
ΔRe(λ)≦5; (iii)
and
ΔRth(λ)≦10. (iv)

### Claim 5 (depends on 3)

The polymer film according to claim 3,
wherein a Re and Rth change before and after the surface treatment satisfy formula (v) and (vi):
|Re−Re′|≦10; (v)
and
|Rth−Rth′|≦20, (vi)
wherein Re indicates an in-plane retardation (nm) of the film before the surface treatment;
Re′ indicates an in-plane retardation (nm) of the film after the surface treatment;
Rth indicates a thickness-direction retardation (nm) of the film before the surface treatment; and
Rth′ indicates a thickness-direction retardation (nm) of the film after the surface treatment.

### Claim 6 (depends on 1)

The polymer film according to claim 1, which comprises at least one compound capable of lowering an optical anisotropy,
wherein an amount of the at least one compound capable of lowering an optical anisotropy is from 0.01 to 20% by mass of the cellulose acylate.

### Claim 7 (depends on 6)

The polymer film according to claim 6, which comprises the at least one compound capable of lowering an optical anisotropy that satisfies formula (vii) within a range satisfying formula (viii):
(RthA−Rth0)/A≦−1.0, (vii)
0.01≦A≦30, (viii)
wherein RthA indicates Rth (nm) of a film containing A % by mass of the at least one compound;
Rth0 indicates Rth (nm) of a film not containing the at least one compound; and
A indicates a mass % of the at least one compound relative to a mass of a starting polymer for a film as 100.

### Claim 8 (depends on 1)

The polymer film according to claim 1, which comprises at least one compound capable of lowering |Re(400)−Re(700)| and |Rth(400)−Rth(700)|.

### Claim 9 (depends on 3)

The polymer film according to claim 3,
wherein the surface treatment is an alkali saponification.

### Claim 10 (depends on 6)

The polymer film according to claim 6,
wherein a degree of dissolution of the at least one compound capable of lowering an optical anisotropy in an alkali solution in an alkali saponification treatment of the polymer film is 20% by mass or less.

### Claim 11 (depends on 9)

The polymer film according to claim 9,
wherein an absorbance at 450 nm of an alkali solution after the alkali saponification treatment of the film surface is 0.1 or less.

### Claim 12 (depends on 6)

The polymer film according to claim 6,
wherein a pKa of the at least one compound capable of lowering an optical anisotropy is 14 or more.

### Claim 13 (depends on 3)

The polymer film according to claim 3,
wherein the surface treatment is a plasma treatment.

### Claim 14 (depends on 3)

The polymer film according to claim 3,
wherein the surface treatment is a corona treatment.

### Claim 15 (depends on 1)

The polymer film according to claim 1,
wherein an acyl substituent in the cellulose acylate is substantially an acetyl group alone, a total degree of substitution is from 2.80 to 2.99, and a mean degree of polymerization of the polymer is from 180 to 550.

### Claim 16 (depends on 1)

The polymer film according to claim 1,
wherein an acyl substituent in the cellulose acylate comprises substantially at least two of acetyl group/propionyl group/butanoyl group, and a total degree of acyl substitution of the cellulose acylate is from 2.50 to 3.00.

### Claim 17 (depends on 1)

An optically-compensatory film, which comprises an optically-anisotropic layer formed on a polymer film according to claim 1, and wherein the optically-anisotropic layer satisfies formula (ix):
Re=0 to 200 (nm), and |Rth|=0 to 400 (nm). (ix)

### Claim 18 (depends on 1)

A polarizer which comprises, as a protective film for a polarizing element, at least one sheet of a polymer film according to claim 1.

### Claim 19 (depends on 1)

A liquid-crystal display device, which comprises a polymer film according to claim 1.

### Claim 20 (depends on 1)

A VA or IPS liquid-crystal display device, which comprises a polymer film according to claim 1.