# US 2013/0253124 A1 · Propylene polymer composition having superior hexane extractables/impact balance

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2013/0253124 A1
- Document ID: US20130253124A1
- Status: Published application
- Kind: A1
- Application number: 13/704,089
- Filed: 2011-06-15
- Published: 2013-09-26
- Earliest claimed: 2010-06-16
- Assignees: Borealis AG
- Inventors: Klaus Bernreiter; Petar Doshev; Gregory Potter; Martina Sandholzer
- Web page: https://patentgrep.com/patent/US20130253124A1

## CPC

- C08L 23/12: Polypropene
- C08L 19/00: Compositions of rubbers not provided for in groups C08L7/00 - C08L17/00
- C08L 23/10: Homopolymers or copolymers of propene
- C08L 23/16: Ethylene-propylene or ethylene-propylene-diene copolymers
- C09D 119/00: Coating compositions based on rubbers, not provided for in groups C09D107/00 - C09D117/00
- C09D 123/12: Polypropene
- C08L: COMPOSITIONS OF MACROMOLECULAR COMPOUNDS (compositions based on polymerisable monomers C08F, C08G; artificial filaments or fibres D01F; textile treating compositions D06)
- C09D: COATING COMPOSITIONS, e.g. PAINTS, VARNISHES OR LACQUERS; FILLING PASTES; CHEMICAL PAINT OR INK REMOVERS; INKS; CORRECTING FLUIDS; WOODSTAINS; PASTES OR SOLIDS FOR COLOURING OR PRINTING; USE OF MATERIALS THEREFOR (cosmetics A61K; processes for applying liquids or other fluent materials to surfaces, in general, B05D; staining wood B27K5/02; glazes or vitreous enamels C03C; natural resins, French polish, drying-oils, driers, turpentine, per se, C09F; polishing compositions other than French polish, ski waxes C09G; adhesives or use of materials as adhesives C09J; materials for sealing or packing joints or covers C09K3/10; materials for stopping leaks C09K3/12; processes for the electrolytic or electrophoretic production of coatings C25D)

## Abstract

Heterophasic polypropylene copolymers having an MFR (2.16 kg, 230° C.) of 15 to 200 g/10 min, determined according to ISO 1133 comprising a propylene homo- or copolymer matrix with an MFR (2.16 kg, 230° C.) of 80 to 500 g/10 min, determined according to ISO 1133 (A) and an ethylene or C4-C10-alpha-olefin propylene rubber phase (B) dispersed within the matrix, wherein the heterophasic polypropylene resin has a fraction soluble in p-xylene at 25° C. (XCS), having an intrinsic viscosity of 2.85 to 4.00 dl/g, determined according to DIN EN ISO 1628-1 and -3 and being composed of propylene monomer units in an amount of 70 wt % to 90 wt %, with optimum balance of impact resistance and low amount of hexane extractables; a process for their preparation and their use.

## Claims

### Claim at position 1

1-13. (canceled)

### Claim at position 2

14: Heterophasic polypropylene copolymers having an MFR2 (2.16 kg, 230° C.) of 15 to 200 g/10 min, determined according to ISO 1133 comprising a propylene homo- or copolymer matrix (A) with an MFR2 (2.16 kg, 230° C.) of 80 to 500 g/10 min, determined according to ISO 1133 and an ethylene or C4-C10-alpha-olefin propylene rubber phase (B) dispersed within the matrix,
wherein the heterophasic polypropylene resin has a fraction soluble in p-xylene at 25° C. (XCS), having an intrinsic viscosity of 2.85 to 4.00 dl/g, determined according to DIN EN ISO 1628-1 and -3 and being composed of propylene monomer units in an amount of 70 wt % to 90 wt %.

### Claim at position 3 (depends on 14)

15: Heterophasic polypropylene copolymers according to claim 14 wherein the propylene matrix (A) is a propylene homopolymer with an MFR2 (2.16 kg, 230° C.) of 90 to 400 g/10 min, determined according to ISO 1133 (A).

### Claim at position 4 (depends on 14)

16: Heterophasic polypropylene copolymers according to claim 14 wherein the rubber phase (B) is an ethylene/propylene copolymer.

### Claim at position 5 (depends on 14)

17: Heterophasic polypropylene copolymers according to claim 14, which comprises:
a) 75 wt % to 95 wt % of the propylene matrix (A) based on the total amount of the heterophasic propylene copolymer and
b) 5 to 25 wt % of the ethylene or C4-C10-alpha-olefin propylene rubber phase (B) based on the total amount of the heterophasic propylene copolymer.

### Claim at position 6 (depends on 14)

18: Heterophasic polypropylene copolymers according to claim 14, wherein the propylene matrix (A) and the ethylene or C4-C10-alpha-olefin propylene rubber phase (B) contribute to at least 85 wt % to the composition and up to 15 wt % may be on or more additives selected from the group consisting of alpha-nucleating agents, antioxidants, stabilizers, acid scavengers, lubricants, mould release agents, flame retardants, pigments, dyes, fillers and plasticizers.

### Claim at position 7 (depends on 14)

19: Heterophasic polypropylene copolymers according to claim 14, wherein the composition has a Charpy notched impact strength at +23° C. of at least 4.0 kJ/m2, up to 80 kJ/m2, and a Charpy notched impact strength at −20° C. of at least 2.0 kJ/m2 up to 50 kJ/m2, determined according to ISO 179-1 eA:2000.

### Claim at position 8 (depends on 14)

20: Heterophasic polypropylene copolymers according to claim 14, wherein the composition has a flexural modulus of at least 600 MPa up to 2500 MPa determined according to ISO 178.

### Claim at position 9 (depends on 14)

21: Heterophasic polypropylene copolymers according to claim 14, wherein the composition has a fraction extractable in hexane (FDA 177, 1520) of less than 5.0 wt %.

### Claim at position 10 (depends on 14)

22: Process for the preparation of heterophasic polypropylene copolymers according to claim 14, comprising the steps of:
producing a polypropylene polymer matrix (A) in the presence of a catalyst system, comprising a Ziegler-Natta procatalyst (i), an external donor (iii) and optionally the cocatalyst (ii) in a first slurry reactor and optionally in a second slurry reactor or in a 1st gas phase reactor (GPR), yielding a first polymerisation product;
transferring the first polymerisation product into a 1st GPR or a 2nd GPR, if the matrix is produced in a slurry/GPR combination;
producing an ethylene/propylene-copolymer in the polymer matrix in the presence of the catalyst system in said 1st or 2nd GPR;
optionally transferring the 1st or 2nd GPR product into a 2nd respectively 3rd GPR and producing a second ethylene/propylene-copolymer in the polymer matrix in the presence of the catalyst system in said 2nd or 3rd GPR, said 1st and 2nd ethylene/propylene mixtures may have the same or different composition ratios; and
recovering the polymer product for further processing.

### Claim at position 11 (depends on 22)

23: Process according to claim 22 wherein the catalyst system used comprises:
i) a Ziegler-Natta procatalyst which contains a trans-esterification product of a lower alcohol and a phthalic ester;
(ii) optionally an organometallic cocatalyst; and
(iii) an external donor represented by formula (I) or (II)
Si(OCH2CH3)3(NR1R2) (I)
or
R3nR4mSi(OR5)z (II)
wherein R1 and R2 can be the same or different and represent a hydrocarbon group having 1 to 12 carbon atoms,
R3 and R4 are identical or different hydrocarbon residues having 1 to 12 carbon atoms,
R5 is methyl or ethyl,
z is 2 or 3,
m is 0 or 1,
n is 0 or 1,
with the proviso that n+m+z=4.

### Claim at position 12 (depends on 14)

24: Use of heterophasic polypropylene copolymers according to claim 14, for the production of molded articles or films.

### Claim at position 13 (depends on 24)

25: Use according to claim 24 for producing thin wall packaging articles, household electrical materials, automotive applications, car interiors and exteriors, for food and medical packaging or as one component for lamination and coating films.

### Claim at position 14 (depends on 24)

26: Use according to claim 24 for advanced packaging applications or cooking applications, which require a fraction extractable in hexane (FDA (CFR) §177.1520) of less than 2.6 wt %.