# US 2013/0253097 A1 · Polymer made from maleic acid, allyl ether, and vinyl acetate and the preparation and use of said polymer

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2013/0253097 A1
- Document ID: US20130253097A1
- Status: Published application
- Kind: A1
- Application number: 13/990,584
- Filed: 2011-12-20
- Published: 2013-09-26
- Earliest claimed: 2010-12-24
- Assignees: Sika Technology AG
- Inventors: Ueli Sulser; Lukas Frunz; Joerg Zimmermann
- Web page: https://patentgrep.com/patent/US20130253097A1

## CPC

- C08F 216/1433: {Monomers containing side chains of polyethylene oxide groups}
- C04B 24/267: {containing polyether side chains}
- C04B 24/2688: {Copolymers containing at least three different monomers}
- C08F 22/02: Acids; Metal salts or ammonium salts thereof {, e.g. maleic acid or itaconic acid}
- C08F 220/285: {and containing a polyether chain in the alcohol moiety}
- C08F 222/06: Maleic anhydride
- C04B 2103/006: {Comb polymers}
- C04B 2103/408: {Dispersants}
- C08F: MACROMOLECULAR COMPOUNDS OBTAINED BY REACTIONS ONLY INVOLVING CARBON-TO-CARBON UNSATURATED BONDS
- C04B: LIME, MAGNESIA; SLAG; CEMENTS; COMPOSITIONS THEREOF, e.g. MORTARS, CONCRETE OR LIKE BUILDING MATERIALS; ARTIFICIAL STONE {(roofing granules E04D7/005)}; CERAMICS (devitrified glass-ceramics C03C10/00); REFRACTORIES; TREATMENT OF NATURAL STONE

## Abstract

The invention relates to comb polymers made from maleic acid or derivatives thereof, allyl ethers, and vinyl acetate, and the preparation thereof by free-radical polymerization at a reaction temperature of 10° C. to 50° C. The invention relates further to the use of such comb polymers to improve the workability of hydraulically setting compositions.

## Claims

### Claim 1

A polymer P comprising:
e. m mol % of at least one structural unit A of the formula (I);
f. n mol % of at least one structural unit B of the formula (II);
g. o mol % of at least one structural unit C of the formula (III);
and optionally
h. p mol % of at least one further structural unit D;
where R1 and R2 in this respect independently of one another each stand for COO−M or COOR4,
R3 stands for H or CH3,
R4 stands for
R5 stands for an alkylene group having 1 to 6 C atoms,
R6 stands for H, an alkyl group, preferably having 1 to 20 C atoms, an alkylaryl group, preferably having 7 to 20 C atoms;
wherein substituent A independently of one another stands for a C2 to C4 alkylene group, the subscript q represents a value of 2 to 300, and the subscript r represents a value of 0 to 1;
wherein M=cation, preferably H+, an alkali metal ion, alkaline earth metal ion, a bivalent or trivalent metal ion, NH4+, or an organic ammonium, particularly preferably H+, Na+, Ca++/2, Mg++/2, NH4+, or an organic ammonium;
wherein m, n, o, p independently of one another are numbers, whereby the sum m+n+o+p=100, and m>0, n>0, o>0 and p>0; and
wherein
m=20-85
n=10-50
o=5-50
p=0-20.

### Claim 2 (depends on 1)

The polymer P according to claim 1, characterized in that the polymer P has an average molecular weight Mn of 15,000-50,000 g/mol.

### Claim 3 (depends on 1)

The polymer P according to claim 1, characterized in that the polymer P has a ratio m/(n+o+p) of 0.5-2.5.

### Claim 4 (depends on 1)

The polymer P according to claim 1, characterized in that the polymer P has a ratio m/o of 2.5-4.

### Claim 5 (depends on 1)

The polymer P according to claim 1, characterized in that the polymer P has a ratio m/o of 1.5-3.

### Claim 6 (depends on 1)

A method for preparing a polymer P according to claim 1.

### Claim 7 (depends on 6)

The method according to claim 6, comprising the step of the free-radical polymerization of:
i) m′ mol % of at least one compound A′, which is a maleic anhydride or a compound of the formula (IV);
ii) n′ mol % of at least one compound B′ of the formula (V);
iii) o′ mol % of at least one compound C′ of the formula (VI);
and optionally
iv) p′ mol % of at least one further compound D′;
where R1 and R2 in this respect independently of one another each stand for COO−M or COOR4
where R3 stands for H or CH3
where R4 stands for
R5 stands for an alkylene group having 1 to 6 C atoms,
R6 stands for H, an alkyl group, preferably having 1 to 20 C atoms, an alkylaryl group, preferably having 7 to 20 C atoms;
wherein substituent A independently of one another stands for a C2 to C4 alkylene group, the subscript q represents a value of 2 to 300, and the subscript r represents a value of 0 to 1;
wherein M=cation, preferably H+, an alkali metal ion, alkaline earth metal ion, a bivalent or trivalent metal ion, NH4+, or an organic ammonium, particularly preferably H+, Na+, Ca++/2, Mg++/2, NH4+, or an organic ammonium;
wherein m, n′, o, p′ independently of one another are numbers, whereby the sum m′+n′+o′+p′=100, and m′>0, n′>0, o′>0 and p′≧0; and
wherein
m′=20-85
n′=10-50
o′=5-50
p′=0-20;
in the presence of an initiator for free-radical polymerizations at a reaction temperature of 10° C. to 50° C., preferably of 15° C. to 35° C.

### Claim 8 (depends on 7)

The method according to claim 7, characterized in that the initiator for free-radical polymerizations is a redox system-based initiator.

### Claim 9 (depends on 8)

The method according to claim 8, characterized in that the redox system-based initiator comprises a reducing agent and a radical former, whereby the reducing agent is selected from the group consisting of sodium hydroxymethanesulfinate (rongalite), alkali metal sulfites, metabisulfites, ascorbic acid, and ketoenols, and the radical former is a peroxide compound.

### Claim 10 (depends on 7)

The method according to claim 7, characterized in that the ratio m′/(n′+o′+p) is between 0.5 and 2.5.

### Claim 11 (depends on 7)

The method according to claim 7 characterized in that the free-radical polymerization is carried out at a pH of 2-4.

### Claim 12 (depends on 1)

Use of at least one polymer P according to claim 1 to improve the workability of hydraulically setting compositions.

### Claim 13 (depends on 12)

The use according to claim 12, characterized in that the flow table spread of the hydraulically setting composition, measured according to EN 1015-3, declines by less than 10% after 30 minutes.

### Claim 14 (depends on 1)

A hydraulically setting composition containing at least one polymer P according to claim 1.

### Claim 15 (depends on 1)

A method for preparing a hydraulically setting composition with extended workability, whereby a hydraulically setting binder, water, and a polymer P according to claim 1 are combined.