# US 2013/0253092 A1 · Glass fiber reinforced polycarbonate molding compositions

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2013/0253092 A1
- Document ID: US20130253092A1
- Status: Published application
- Kind: A1
- Application number: 13/875,696
- Filed: 2013-05-02
- Published: 2013-09-26
- Earliest claimed: 2007-08-16
- Assignees: Bayer MaterialScience AG
- Applicants: Bayer Materialscience AG
- Inventors: Andreas Seidel; Michael Erkelenz; Eckhard Wenz
- Web page: https://patentgrep.com/patent/US20130253092A1

## CPC

- C08L 69/00: Compositions of polycarbonates; Compositions of derivatives of polycarbonates
- C08L 69/005: {Polyester-carbonates}
- C08K 9/08: Ingredients agglomerated by treatment with a binding agent
- C08L 25/12: with unsaturated nitriles
- C08L: COMPOSITIONS OF MACROMOLECULAR COMPOUNDS (compositions based on polymerisable monomers C08F, C08G; artificial filaments or fibres D01F; textile treating compositions D06)
- C08K: Use of inorganic or non-macromolecular organic substances as compounding ingredients (paints, inks, varnishes, dyes, polishes, adhesives C09)

## Abstract

The invention relates to glass fiber reinforced polycarbonate compositions and molding compositions of the present investor and distinguished by high rigidity, high flowabillty, high processing stability, good chemical resistance and good aging resistance vis-à-vis the effects of light and heat compared with the prior art. The present invention also relates to the use of the compositions for the production of shaded articles and to shaped articles comprising the compositions according to the invention.

## Claims

### Claim 1

A composition comprising
A) 10 to 85 parts by weight of a polycarbonate, and/or a polyester carbonate,
B) 10 to 50 parts by weight of a rubber-free vinyl copolymer of
B.1 70 to 80 wt. %, based on the total weight of component B, of styrene and
B.2 20 to 30 wt. %, based on the total weight of component B, of acrylonitrile
C) 5 to 50 parts by weight of sized glass fiber with
C.1 a glass fibers comprising at least one component selected from the group consisting of continuous strands, long glass fiber and chopped glass strands,
C.2 a size, and
C.3 optionally an adhesion promoter,
wherein the size C.2 consists essentially of
C.2.1 50 to 100 wt. %, based on the total weight of C.2, of an epoxy polymer comprising an epoxy resin made from,
C.2.1.1 epichlorohydrin and
C.2.1.2 bisphenol A as bis functional alcohol, and
C.2.2 0 to 50 wt. %, based on the total weight of C.2, of at least one polymer selected from the group consisting of the polyurethanes, polyolefins, acrylate-containing polymers, styrene-containing polymers and polyamides,
and wherein the sized glass fiber has a carbon content of 0.1 to 1 wt. %,
D) 0 to 2 parts by weight of a rubber-modified graft polymer which is substantially free from double bonds and is selected from the group consisting of acrylate rubber, silicone rubber and silicone-acrylate composite rubber, and
E) 0 to 10 parts by weight of a polymer additive, the composition being free from rubber-modified polymers which differ from component D).

### Claim 2 (depends on 1)

The composition of claim 1, wherein the ESC thereof is at least 8 hours.

### Claim 3 (depends on 1)

The composition of claim 1, wherein:
A) is a polycarbonate present in an amount of from about 43 to about 62 parts by weight;
B) is present in an amount of from about 25 to about 30 parts by weight;
C) is present in an amount of from about 10 to about 20 parts by weight:;
D) is present in an amount of from about 0 to about 0.5 parts by weight; and
E) is present in an amount of from about 0 to about 0.6 parts by weight.

### Claim 4 (depends on 1)

The composition of claim 1, having:
a modulus of elasticity of from about 5070 to about 10178 mPa:
a melt viscosity (260° C.) is ≦233 Pas; and
ESC of at least 8 hours.

### Claim 5 (depends on 1)

The composition of claim 1, wherein:
A) is a linear polycarbonate based on Bisphenol A with a weight-average molecular weight of 25,000-32,000 g/mol;
B) is SAN copolymer with an acrylonitrile content of 23 wt % and a weight-average molecular weight of about 130,000 g/mole, or ABS polymer with an acrylonitrile content:butadiene:styrene ratio of 20:28:52 wt %, produced by emulsion polymerization;
C) is chopped glass strands with an average diameter of 13 μm and a size made of epoxy resin produced from epichlorohydrin and bisphenol A;
D) is styrene-acrylonitrile grafted acrylate-silicone composite rubber, produced by emulsion polymerization; and
E) is pentacrythritol tetrastearate, phosphite stabilizer, or a combination thereof.

### Claim 6 (depends on 1)

The composition of claim 1, consisting of the recited components.

### Claim 7 (depends on 3)

The composition of claim 3, consisting of the recited components.

### Claim 8 (depends on 1)

The composition of claim 1, wherein the modulus of elasticity is ≧ about 5070 mPa and the impact resistance (aK260° C.) is ≧ about 38.